# US 2016/0348212 A1 · A method for separating the mixture of zirconium oxide/hafnium oxide by pyrometallurgy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0348212 A1
- Document ID: US20160348212A1
- Status: Published application
- Kind: A1
- Application number: 15/102,255
- Filed: 2014-09-29
- Published: 2016-12-01
- Earliest claimed: 2013-12-12
- Inventors: Xingfeng Zhu
- Web page: https://patentgrep.com/patent/US20160348212A1

## CPC

- C22B 34/14: Obtaining zirconium or hafnium {(treatment or purification of solutions by liquid-liquid extraction, by ion exchange or by adsorption C22B3/00, C01G25/003, C01G27/003)}
- C01G 25/04: Halides
- C01G 27/04: Halides
- C22B 5/00: General methods of reducing to metals
- C22B 7/002: {by treating with halogens, sulfur or compounds thereof; by carburising, by treating with hydrogen (hydriding)}
- C22B 9/02: Refining by liquating, filtering, centrifuging, distilling, or supersonic wave action {including acoustic waves; (C22B9/003, C22B9/006, C22B9/05, C22B9/22 take precedence)}
- C22B 15/0073: {containing nitrogen}
- C22B 15/008: {with non-acid solutions containing salts of alkali or alkaline earth metals}
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for separating zirconium oxide/hafnium oxide by pyrometallurgy. The mixture of zirconium oxide/hafnium oxide, carbon and pure bromine react one hour at 650° C., then added to molten salt mixture for rectifying separation, and then maintained two hours at rectifying tower bottom below 357° C., to get the non-target substance; and then maintained five hours at 357° C. to collect the target substance zirconium tetrabromide; the residue in the reactor is retained, then rectification separation is performed in the same device, heated to 400° C. to retain more than five hours, to get hafnium tetrabromide, then the zirconium tetrabromide and hafnium tetrabromide are substituted by magnesium to get the pure zirconium and pure hafnium.

## Claims

### Claim 1

A method for separating zirconium oxide and hafnium oxide from a mixture of zirconium oxide and hafnium oxide comprises the following steps:
mixing the mixture of zirconium oxide and hafnium oxide, carbon and pure bromine, reacting one hour at 650° C. which results in a mixture of zirconium tetrabromide and hafnium tetrabromide;
adding the mixture of zirconium tetrabromide and hafnium tetrabromide into molten salt for rectification separation, and maintaining the rectification for two hours at 200-357° C. which yields a non-target substance at the top of the rectification tower, wherein the molten salt is the molten mixture of potassium fluorine and aluminum potassium sulfate with a weight ratio of 1.2-1.6:1;
maintaining for additional five hours at 357° C.-360° C., collecting the target substance zirconium tetrabromide from the top of the rectification tower;
performing the rectification separation in the rectification tower, heat up to 400-403° C. and maintaining for five hours, and then collecting the hafnium tetrabromide from the top of the rectification tower.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the temperature for collecting the zirconium tetrabromide is 357° C.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the temperature for collecting the hafnium tetrabromide is 400° C.

### Claim 4 (depends on 1)

The method according to claim 1, wherein it further comprises: performing a magnetism replacement for the zirconium tetrabromide which yields a pure zirconium.

### Claim 5 (depends on 1)

The method according to claim 1, wherein it further comprises: performing a magnetism replacement for the hafnium tetrabromide which yields a pure hafnium.