# US 2016/0326036 A1 · Terpolymerized corrosion and scale inhibitor used in circulating cooling water of central air conditioning and its preparation method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0326036 A1
- Document ID: US20160326036A1
- Status: Published application
- Kind: A1
- Application number: 15/109,261
- Filed: 2014-12-29
- Published: 2016-11-10
- Earliest claimed: 2014-01-03
- Assignees: Guangzhou Special Pressure Equipment Inspection and Research Institute
- Applicants: Guangzhou Special Pressure Equipment Inspection and Research Institute
- Inventors: Bo Yang; Maodong Li; Zhigang Chen; Weiwen Ye; Hua Li; Junming Zhao; Hui Zhang; Jinmei Lin; Wen Yu; Ming Zeng; Zongjie Yin; Juan Liu
- Web page: https://patentgrep.com/patent/US20160326036A1

## CPC

- C02F 5/105: {combined with inorganic substances}
- C02F 5/083: {Mineral agents}
- C02F 5/12: containing nitrogen (C02F5/14 takes precedence)
- C02F 5/125: {combined with inorganic substances}
- C02F 5/145: {combined with inorganic substances}
- C09K 15/328: {containing boron, silicon, selenium or tellurium}
- C23F 11/08: in other liquids
- C23F 14/02: by chemical means
- C02F 2101/10: Inorganic compounds
- C02F 2303/08: Corrosion inhibition
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25

## Abstract

A terpolymerized corrosion and scale inhibitor used in circulating cooling water of central air conditioning, containing tourmaline, polyaspartic acid, polyepoxysuccinic acid, polymaleic acid, etidronic acid, zinc salt, and the like, wherein the content of the tourmaline is 5-500 g/t (calculated based on solid form); the content of polyaspartic acid, polyepoxysuccinic acid, polymaleic acid and etidronic acid is 2-60 g/t (calculated based on liquid form); and the content of the zinc salt is 0.2-0.8 g/t (calculated based on solid form), is provided. Also disclosed is a method of preparing the terpolymerized corrosion and scale inhibitor used in circulating cooling water of central air conditioning.

## Claims

### Claim at position 1

1-9. (canceled)

### Claim 10

A terpolymerized corrosion and scale inhibitor used in circulating cooling water of central air conditioning, comprising: tourmaline, a copolymer and zinc salt, wherein the copolymer is a polymer of any three or four of polyaspartic acid, polyepoxysuccinic acid, polymaleic acid and etidronic acid; wherein a content of tourmaline is 5-500 g/t calculated based on solid form, a content of the copolymer is 2-60 g/t calculated based on liquid form; and a content of the zinc salt is 0.2-0.8 g/t calculated based on solid form.

### Claim 11 (depends on 10)

The terpolymerized corrosion and scale inhibitor used in circulating cooling water of central air conditioning according to claim 10, wherein the tourmaline is at least one of dravite, schorlite, elbaite, manganese tourmaline, and uvite.

### Claim 12 (depends on 10)

The terpolymerized corrosion and scale inhibitor used in circulating cooling water of central air conditioning according to claim 10, wherein the zinc salt is any one or a mixture of zinc sulfate and zinc chloride.

### Claim 13 (depends on 10)

The terpolymerized corrosion and scale inhibitor used in circulating cooling water of central air conditioning according to claim 10, wherein the terpolymerized corrosion and scale inhibitor further comprises 0.2-2 g/t calculated based on solid form of benzotriazole.

### Claim 14 (depends on 10)

The terpolymerized corrosion and scale inhibitor used in circulating cooling water of central air conditioning according to claim 10, wherein the content of the copolymer is 6-16 g/t calculated based on liquid form.

### Claim 15 (depends on 10)

The terpolymerized corrosion and scale inhibitor used in circulating cooling water of central air conditioning according to claim 10, wherein a concentration rate of the circulating cooling water of central air conditioning is 3-12.

### Claim 16 (depends on 10)

A preparation method of the terpolymerized corrosion and scale inhibitor used in circulating cooling water of central air conditioning according to the claim 10, wherein the preparation method comprises the following steps:
1) dissolving 2-60 g of the polymer of any three or four of polyaspartic acid, polyepoxysuccinic acid, polymaleic acid and etidronic acid into 1000 ml of deionized water, and adding 0.2-0.8 g of the zinc salt;
2) heating to 55-75° C., and performing a heat preservation reaction on the polymer solution for 4-6 hours under the condition of stirring, and then cooling, thereby obtaining a terpolymerized mother liquor; and
3) in 1 L of the circulating cooling water of central air conditioning, firstly feeding 6-600 mg of the tourmaline directly or through a recyclable tourmaline dosing device, and subsequently adding 1 mg of the terpolymerized mother liquor directly.

### Claim 17 (depends on 16)

The preparation method of the terpolymerized corrosion and scale inhibitor used in circulating cooling water of central air conditioning according to claim 16, wherein in step 1), 0.2-2 g of benzotriazole is added into the corrosion and scale inhibitor for copper-containing devices.

### Claim 18 (depends on 16)

The preparation method of the terpolymerized corrosion and scale inhibitor used in circulating cooling water of central air conditioning according to claim 16, wherein in step 2), the optimal temperature is 65° C., and the optimal reaction time is 5 hours.