# US 2016/0318793 A1 · Optical fiber preform

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0318793 A1
- Document ID: US20160318793A1
- Status: Published application
- Kind: A1
- Application number: 15/137,255
- Filed: 2016-04-25
- Published: 2016-11-03
- Earliest claimed: 2015-04-30
- Assignees: Sumitomo Electric Industries, Ltd.
- Applicants: Sumitomo Electric Industries, Ltd.
- Inventors: Yoshiaki TAMURA; Tetsuya HARUNA; Yuki KAWAGUCHI
- Web page: https://patentgrep.com/patent/US20160318793A1

## CPC

- C03C 13/046: {Multicomponent glass compositions}
- C03B 37/01211: {by inserting one or more rods or tubes into a tube}
- C03B 37/01237: {to modify the diameter by heat-polishing, e.g. fire-polishing}
- C03B 37/0124: {Means for reducing the diameter of rods or tubes by drawing, e.g. for preform draw-down}
- C03B 37/014: made entirely or partially by chemical means {, e.g. vapour phase deposition of bulk porous glass either by outside vapour deposition [OVD], or by outside vapour phase oxidation [OVPO] or by vapour axial deposition [VAD] (C03C17/02 takes precedence)}
- C03B 37/01807: {Reactant delivery systems, e.g. reactant deposition burners}
- C03B 37/01861: {Means for changing or stabilising the diameter or form of tubes or rods}
- C03B 2201/12: doped with fluorine (C03B2201/14 takes precedence)
- C03B 2201/20: doped with non-metals other than boron or fluorine
- C03B 2201/50: doped with alkali metals
- C03B 2201/54: doped with beryllium, magnesium or alkaline earth metals
- C03B 2203/22: Radial profile of refractive index, composition or softening point
- C03B 2203/222: Mismatching viscosities or softening points of glass layers
- C03C 2201/12: containing fluorine (C03C2201/14 takes precedence)
- C03C 2201/50: containing alkali metals
- C03C 2201/54: containing beryllium, magnesium or alkaline earth metals
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

An optical fiber preform of the present embodiment comprises a core portion and a cladding each comprised of silica glass. The core portion has a first dopant region including a central axis of the core portion and a second dopant region away from the central axis. The first dopant region contains a first dopant selected from among Na, K, and their compounds, and a concentration of the first dopant is 10 atomic ppm or more but 2,000 atomic ppm or less. The second dopant region contains a second dopant reducing viscosity of the silica glass. The second dopant has, as a characteristic at a temperature of 2,000° C. to 2,300° C., a diffusion coefficient of 1×10−12 cm2/s or higher but lower than that of the first dopant, and a concentration of the second dopant region is 10 atomic ppm or more.

## Claims

### Claim 1

An optical fiber preform comprising:
a core portion comprised of silica glass and extending along a central axis thereof, in a cross-section of the optical fiber preform orthogonal to the central axis, the core portion having
a first dopant region containing a first dopant and including the central axis, the first dopant being selected from among Na, K, and their compounds, a concentration of the first dopant being set at 10 atomic ppm or more but 2,000 atomic ppm or less, and
a second dopant region containing a second dopant for reducing viscosity of the silica glass and surrounding the central axis while being away from the central axis, the second dopant having, as a characteristic at a temperature of 2,000° C. to 2,300° C., a diffusion coefficient of 1×10−12 cm2/s or higher but lower than that of the first dopant, a concentration of the second dopant being set at 10 atomic ppm or more; and
a cladding portion comprised of silica glass and surrounding an outer periphery of the core portion, the cladding portion containing F and having a refractive index lower than that of the core portion.

### Claim 2 (depends on 1)

The optical fiber preform according to claim 1, wherein a ratio (r2/r1) of a radius r2 of the core portion to a distance r1 from the central axis falls within a range from 3 to 9.5, the distance r1 being defined as a distance from the central axis to a position where a concentration peak of the second dopant exists.

### Claim 3 (depends on 1)

The optical fiber preform according to claim 1, wherein the second dopant includes any one selected from among Rb, Cs, Mg, Ca, and Sr.

### Claim 4 (depends on 2)

The optical fiber preform according to claim 2, wherein the second dopant includes any one selected from among Rb, Cs, Mg, Ca, and Sr.

### Claim 5 (depends on 1)

The optical fiber preform according to claim 1, wherein, in the cross-section, the first and second dopant regions overlap each other.

### Claim 6 (depends on 1)

The optical fiber preform according to claim 1, wherein, in the cross-section, an outer periphery of the first dopant region is away from or corresponds to an inner periphery of the second dopant region.