# US 2016/0260981 A1 · Electrodeposited copper foil, and electrical component and battery comprising same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0260981 A1
- Document ID: US20160260981A1
- Status: Published application
- Kind: A1
- Application number: 15/030,447
- Filed: 2014-11-10
- Published: 2016-09-08
- Earliest claimed: 2013-11-08
- Assignees: Iljin Materials Co., Ltd.
- Applicants: Iljin Materials Co., Ltd.
- Inventors: Sun Hyoung LEE; Tae Jin JO; Seul Ki PARK; Ki Deok SONG
- Web page: https://patentgrep.com/patent/US20160260981A1

## CPC

- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H05K 1/09: Use of materials for the {conductive, e.g. } metallic pattern
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H05K 2201/0355: Metal foils
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Disclosed is an electrodeposited copper foil, in which a center line roughness average Ra (μm), a maximum height Rmax (μm), and a ten-point height average Rz (μm) of a matte side satisfy an Equation below, 1.5≦(Rmax−Rz)/Ra≦6.5. The electrodeposited copper foil according to the present invention maintains low roughness and high strength, and exhibits a high elongation rate, and particularly, has excellent glossiness, so that the electrodeposited copper foil may be used in a current collector of a medium and large lithigum ion secondary battery and a semiconductor packaging substrate for Tape Automated Bonding (TAB) used in a Tape Carrier Package (TCP).

## Claims

### Claim 1

An electrodeposited copper foil, in which a center line roughness average Ra (μm), a maximum height Rmax (μm), and a ten-point height average Rz (μm) of a matte side satisfy an Equation below, 1.5≦(Rmax−Rz)/Ra≦6.5.

### Claim 2 (depends on 1)

The electrodeposited copper foil of claim 1, wherein tensile strength of the electrodeposited copper foil before a heat treatment is 40 kgf/mm2 to 70 kgf/mm2.

### Claim 3 (depends on 1)

The electrodeposited copper foil of claim 1, wherein tensile strength of the electrodeposited copper foil after a heat treatment is 40 kgf/mm2 to 70 kgf/mm2.

### Claim 4 (depends on 1)

The electrodeposited copper foil of claim 1, wherein tensile strength of the electrodeposited copper foil after a heat treatment for one hour at 180° C. is 40 kgf/mm2 to 70 kgf/mm2.

### Claim 5 (depends on 3)

The electrodeposited copper foil of claim 3, wherein tensile strength of the electrodeposited copper foil after the heat treatment is 85% to 99% of tensile strength of the electrodeposited copper foil before the heat treatment.

### Claim 6 (depends on 1)

The electrodeposited copper foil of claim 1, wherein an elongation rate before a heat treatment is 2% to 15%.

### Claim 7 (depends on 1)

The electrodeposited copper foil of claim 1, wherein an elongation rate after a heat treatment is 4% to 15%.

### Claim 8 (depends on 1)

The electrodeposited copper foil of claim 1, wherein an elongation rate after a heat treatment for one hour at 180° C. is 4% to 15%.

### Claim 9 (depends on 3)

The electrodeposited copper foil of claim 3, wherein an elongation rate after a heat treatment is one time to 4.5 times of an elongation rate before the heat treatment.

### Claim 10 (depends on 1)

The electrodeposited copper foil of claim 1, wherein a corner curl angle of the electrodeposited copper foil is 0° to 45°.

### Claim 11 (depends on 1)

The electrodeposited copper foil of claim 1, wherein a corner curl height of the electrodeposited copper foil is 0 mm to 40 mm.

### Claim 12 (depends on 1)

The electrodeposited copper foil of claim 1, wherein the electrodeposited copper foil has a thickness of 2 μm to 10 μm.

### Claim 13

(canceled)

### Claim 14

(canceled)

### Claim 15

A battery including an electrodeposited copper foil, wherein a center line roughness average Ra (μm), a maximum height Rmax (μm), and a ten-point height average Rz (μm) of a matte side of the electrodeposited copper foil satisfy an Equation below, 1.5≦(Rmax−Rz)/Ra≦6.5.

### Claim 16 (depends on 15)

The battery of claim 15, wherein tensile strength of the electrodeposited copper foil before a heat treatment is 40 kgf/mm2 to 70 kgf/mm2.

### Claim 17 (depends on 15)

The battery of claim 15, wherein tensile strength of the electrodeposited copper foil after a heat treatment is 40 kgf/mm2 to 70 kgf/mm2.

### Claim 18 (depends on 15)

The battery of claim 15, wherein tensile strength of the electrodeposited copper foil after a heat treatment for one hour at 180° C. is 40 kgf/mm2 to 70 kgf/mm2.

### Claim 19 (depends on 17)

The battery of claim 17, wherein tensile strength of the electrodeposited copper foil after the heat treatment is 85% to 99% of tensile strength of the electrodeposited copper foil before the heat treatment.

### Claim 20 (depends on 15)

The battery of claim 15, wherein an elongation rate before a heat treatment is 2% to 15%.

### Claim 21 (depends on 15)

The battery of claim 15, wherein an elongation rate after a heat treatment is 4% to 15%.

### Claim 22 (depends on 15)

The battery of claim 15, wherein an elongation rate after a heat treatment for one hour at 180° C. is 4% to 15%.

### Claim 23 (depends on 17)

The battery of claim 17, wherein an elongation rate after a heat treatment is one time to 4.5 times of an elongation rate before the heat treatment.

### Claim 24 (depends on 15)

The battery of claim 15, wherein a corner curl angle of the electrodeposited copper foil is 0° to 45°.

### Claim 25 (depends on 15)

The battery of claim 15, wherein a corner curl height of the electrodeposited copper foil is 0 mm to 40 mm.

### Claim 26 (depends on 15)

The battery of claim 15, wherein the electrodeposited copper foil has a thickness of 2 μm to 10 μm.

### Claim 27

An electrical component, comprising:
an insulating base material; and
the electrodeposited copper foil attached onto one surface of the insulating base material, wherein a center line roughness average Ra (μm), a maximum height Rmax (μm), and a ten-point height average Rz (μm) of a matte side of the electrodeposited copper foil satisfy an Equation below, 1.5≦(Rmax−Rz)/Ra≦6.5.

### Claim 28 (depends on 27)

The electrical component of claim 27, wherein tensile strength of the electrodeposited copper foil before a heat treatment is 40 kgf/mm2 to 70 kgf/mm2.

### Claim 29 (depends on 27)

The electrical component of claim 27, wherein tensile strength of the electrodeposited copper foil after a heat treatment is 40 kgf/mm2 to 70 kgf/mm2.

### Claim 30 (depends on 27)

The electrical component of claim 27, wherein tensile strength of the electrodeposited copper foil after a heat treatment for one hour at 180° C. is 40 kgf/mm2 to 70 kgf/mm2.

### Claim 31 (depends on 29)

The electrical component of claim 29, wherein tensile strength of the electrodeposited copper foil after the heat treatment is 85% to 99% of tensile strength of the electrodeposited copper foil before the heat treatment.

### Claim 32 (depends on 27)

The electrical component of claim 27, wherein an elongation rate before a heat treatment is 2% to 15%.

### Claim 33 (depends on 27)

The electrical component of claim 27, wherein an elongation rate after a heat treatment is 4% to 15%.

### Claim 34 (depends on 27)

The electrical component of claim 27, wherein an elongation rate after a heat treatment for one hour at 180° C. is 4% to 15%.

### Claim 35 (depends on 29)

The electrical component of claim 29, wherein an elongation rate after a heat treatment is one time to 4.5 times of an elongation rate before the heat treatment.

### Claim 36 (depends on 27)

The electrical component of claim 27, wherein a corner curl angle of the electrodeposited copper foil is 0° to 45°.

### Claim 37 (depends on 27)

The electrical component of claim 27, wherein a corner curl height of the electrodeposited copper foil is 0 mm to 40 mm.

### Claim 38 (depends on 27)

The electrical component of claim 27, wherein the electrodeposited copper foil has a thickness of 2 μm to 10 μm.