# US 2016/0260977 A1 · Method for manufacturing a composite

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0260977 A1
- Document ID: US20160260977A1
- Status: Published application
- Kind: A1
- Application number: 15/157,560
- Filed: 2016-05-18
- Published: 2016-09-08
- Earliest claimed: 2013-01-24
- Assignees: National Taiwan University of Science and Technology
- Applicants: National Taiwan University of Science and Technology
- Inventors: Bing Joe Hwang; Yun Sheng Ye; Wei Nien Su
- Web page: https://patentgrep.com/patent/US20160260977A1

## CPC

- H01M 4/625: {Carbon or graphite}
- H01M 4/364: {as mixtures}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/387: {Tin or alloys based on tin}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for manufacturing a composite is disclosed. The method includes steps of (a) providing a powder in a first weight ratio, a graphene oxide in a second weight ratio, a first modifying agent having a negative electric charge, and a second modifying agent having a positive electric charge; (b) reacting the first modifying agent with the powder so that a surface of the powder has the negative electric charge; (c) reacting the second modifying agent with the graphene oxide so that a surface of the graphene oxide has the positive electric charge; and (d) mixing the powder having the negative electric charge and the graphene oxide having the positive electric charge to form a composite.

## Claims

### Claim 1

A powder composite comprising:
a powder having a first surface; and
a graphene having a second surface and mixed with the powder, wherein:
the first surface has a negative electric charge; and
the second surface has a positive electric charge.

### Claim 2 (depends on 1)

A powder composite according to claim 1, wherein the powder is one selected from a group consisting of a silicon powder, a germanium powder, a tin powder and a combination thereof.

### Claim 3 (depends on 1)

A powder composite according to claim 1, wherein the powder ranges between 50 wt % and 90 wt %.

### Claim 4

A method for modifying a powder having a surface, comprising steps of:
(a) providing a modifier having a negative electric charge; and
(b) distributing the modifier on the surface of the powder so that the surface has the negative electric charge.

### Claim 5 (depends on 4)

A method for modifying a powder according to claim 4, wherein the modifier is chemically bonded to the surface.

### Claim 6

A method for modifying a powder, comprising steps of:
(a) providing a modifying agent having a first free radical and a negative electric charge;
(b) providing a powder having a second free radical; and
(c) causing the first free radical to be bound with the second free radical so as to enable the powder to have the negative electric charge.