# US 2016/0260968 A1 · "B" AND "O" SITE DOPED AB2O4 SPINEL CATHODE MATERIAL, METHOD OF PREPARING THE SAME, AND RECHARGEABLE LITHIUM AND Li-ION ELECTROCHEMICAL SYSTEMS CONTAINING THE SAME

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0260968 A1
- Document ID: US20160260968A1
- Status: Published application
- Kind: A1
- Application number: 14/636,183
- Filed: 2015-03-03
- Published: 2016-09-08
- Earliest claimed: 2015-03-03
- Assignees: United States Government as represented by the Secretary of the Army
- Applicants: United States Government, as represented by the Secretary of the Army
- Inventors: Terrill B. Atwater; Paula C. Latorre; Ashley L. Ruth
- Web page: https://patentgrep.com/patent/US20160260968A1

## CPC

- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- C01G 49/0072: {containing manganese}
- C01G 51/54: of the type (Mn2O4)-, e.g. Li(CoxMn2-x)O4 or Li(MyCoxMn2-x-y)O4
- C01G 53/54: of the type (Mn2O4)-, e.g. Li(NixMn2-x)O4 or Li(MyNixMn2-x-y)O4
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- C01P 2002/32: spinel-type (AB2O4)
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/40: prism-like
- H01M 4/623: {fluorinated polymers}
- H01M 4/625: {Carbon or graphite}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A process for preparing a stable Group VIII Period 4 element (iron, cobalt, or nickel) “B” site and chlorine “O” site modified lithium manganese-based AB2O4 spinel cathode material is provided. The general formula of the “B” and “O” site modified lithium manganese-based AB2O4 spinel is LixMn2-yMyO4-z(Clz) where M is Fe, Co or Ni. In addition, a Group VIII Period 4 element (iron, cobalt, or nickel) “B” site and chlorine “O” site modified lithium manganese-based AB2O4 spinel cathode material is provided. Furthermore, a lithium or lithium ion rechargeable electrochemical cell is provided, incorporating the Group VIII Period 4 element (iron, cobalt, or nickel) “B” site and chlorine “O” site modified lithium manganese-based AB2O4 spinel cathode material in a positive electrode.

## Claims

### Claim 1

A method of preparing a homogeneously dispersed Group VIII Period 4 element and chlorine-modified lithium manganese based AB2O4 spinel cathode material, the method comprising:
dissolving a chlorine-containing salt, a nitrate of a Group VIII Period 4 element, manganese nitrate, and lithium nitrate to produce an aqueous solution;
mixing the aqueous solution with a chelating agent to produce a mixture;
heating the mixture to produce an ash;
grinding the ash; and
calcining the ground ash for a time period no greater than 5 hours at a temperature of at least 350° C. to produce the homogeneously dispersed Group VIII Period 4 element and chlorine-modified lithium manganese-based AB2O4 spinel cathode material.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the Group VIII Period 4 element is selected from a group consisting of iron, cobalt, and nickel.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the heating step comprises:
heating the mixture at a temperature ranging from 75° C. to 120° C. to produce a gel; and
heating the gel at a temperature ranging from 200° C. to 300° C. to produce an ash.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the chlorine-containing salt is a compound selected from a group consisting of lithium chloride, a chloride of a Group VIII Period 4 element, and manganese chloride.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the chelating agent is a compound selected from a group consisting of glycine, cellulose, citric acid, a cellulose-citric acid mixture, and urea.

### Claim 6 (depends on 1)

The method according to claim 1, further comprising mixing the homogenous mixture with a conductive carbon and a binder.

### Claim 7 (depends on 5)

The method according to claim 5, wherein the conductive carbon is selected from a group consisting of conductive carbon black, graphite, carbon nanofibers, and carbon nanoparticles and the binder is selected from a group consisting of polytetrafluoroethylene, polyvinylidene fluoride, and latex.

### Claim 8

A homogeneously dispersed Group VIII Period 4 element and chlorine-modified lithium manganese-based AB2O4 spinel cathode material prepared by a process comprising:
dissolving a chlorine-containing salt, manganese nitrate, a nitrate of a Group VIII Period 4 element, and lithium nitrate to produce an aqueous solution;
mixing the aqueous solution with a chelating agent;
heating the mixture to produce an ash;
grinding the ash; and
calcining the ground ash for a time period no greater than 5 hours at a temperature of at least 350° C. to produce the homogeneously dispersed Group VIII Period 4 element (iron, cobalt, or nickel) and chlorine-modified lithium manganese-based AB2O4 spinel cathode material.

### Claim 9 (depends on 8)

The cathode material according to claim 8, wherein the heating step comprises:
heating the mixture at a temperature ranging from 75° C. to 120° C. to produce a gel; and
heating the gel at a temperature ranging from 200° C. to 300° C. to produce an ash.

### Claim 10 (depends on 8)

The cathode material according to claim 8, wherein the chlorine-containing salt is a compound selected from a group consisting of lithium chloride, a chloride of a Group VIII Period 4 element, and manganese chloride.

### Claim 11 (depends on 8)

The cathode material according to claim 8, wherein the chelating agent is a compound selected from a group consisting of glycine, cellulose, citric acid, a cellulose-citric acid mixture, and urea.

### Claim 12 (depends on 8)

The cathode material according to claim 8, wherein the process further comprises mixing the homogenous mixture with a conductive carbon and a binder.

### Claim 13 (depends on 12)

The cathode material according to claim 12, wherein the conductive carbon is selected from a group consisting of conductive carbon black, graphite, carbon nanofibers, and carbon nanoparticles.

### Claim 14 (depends on 12)

The cathode material according to claim 12, wherein the binder is selected from a group consisting of polytetrafluoroethylene, polyvinylidene fluoride, and latex.

### Claim 15

A lithium electrochemical cell comprising: an anode; and a cathode comprising a homogeneously dispersed Group VIII Period 4 element and chlorine-modified lithium manganese-based AB2O4 spinel cathode material prepared by a process comprising:
dissolving a chlorine-containing salt, manganese nitrate, a nitrate of a Group VIII Period 4 element, and lithium nitrate to produce an aqueous solution;
mixing the aqueous solution with a chelating agent to produce a mixture;
heating the mixture to produce an ash;
grinding the ash; and
calcining the ground ash for a time period no greater than 5 hours at a temperature of at least 350° C. to produce the homogeneously dispersed Group VIII Period 4 element and chlorine-modified lithium manganese-based AB2O4 spinel cathode material.

### Claim 16 (depends on 15)

The cathode material according to claim 15, wherein the chlorine-containing salt is a compound selected from a group consisting of lithium chloride, a chloride of a Group VIII Period 4 element, and manganese chloride.

### Claim 17 (depends on 15)

The cathode material according to claim 15, wherein the chelating agent is a compound selected from a group consisting of, glycine, cellulose, citric acid, a cellulose-citric acid mixture, and urea.

### Claim 18 (depends on 17)

The lithium electrochemical cell according to claim 17, wherein the cathode material further comprises a conductive carbon and a binder.

### Claim 19 (depends on 18)

The lithium electrochemical cell according to claim 18, wherein the conductive carbon is a compound selected from a group consisting of carbon black, graphite, carbon nanofibers, and carbon nanoparticles.

### Claim 20 (depends on 18)

The lithium electrochemical cell according to claim 18, wherein the binder is a compound selected from the group consisting of polytetrafluoroethylene, polyvinylidene fluoride, and latex.