# US 2016/0260902 A1 · Vapor deposition device, vapor deposition method, and method for producing organic electroluminescence display device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0260902 A1
- Document ID: US20160260902A1
- Status: Published application
- Kind: A1
- Application number: 15/094,902
- Filed: 2016-04-08
- Published: 2016-09-08
- Earliest claimed: 2010-10-19
- Assignees: Sharp Kabushiki Kaisha
- Applicants: Sharp Kabushiki Kaisha
- Inventors: Tohru SONODA; Shinichi KAWATO; Satoshi INOUE
- Web page: https://patentgrep.com/patent/US20160260902A1

## CPC

- C23C 14/042: {using masks}
- C23C 14/12: Organic material
- C23C 14/24: Vacuum evaporation
- C23C 14/50: Substrate holders
- C23C 16/042: {using masks}
- H05B 33/10: Apparatus or processes specially adapted to the manufacture of electroluminescent light sources
- H10K 71/164: {using vacuum deposition}
- H10K 71/166: {using selective deposition, e.g. using a mask}
- H10K 59/12: Active-matrix OLED [AMOLED] displays
- H10K 59/1201: {Manufacture or treatment}
- H10K 59/35: comprising red-green-blue [RGB] subpixels
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H05B: ELECTRIC HEATING; ELECTRIC LIGHT SOURCES NOT OTHERWISE PROVIDED FOR; CIRCUIT ARRANGEMENTS FOR ELECTRIC LIGHT SOURCES, IN GENERAL
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

A vapor deposition device (50) disclosed, a partition wall (26) standing between film formation regions on a film formation substrate (200), includes: a mask unit (80) including a shadow mask (81) and a vapor deposition source (85) fixed in position relative to each other; contacting means for bringing the film formation substrate (200) and the shadow mask (81) into contact with each other at the partition wall (26); and moving means for moving at least a first one of the mask unit (80) and the film formation substrate (200) relative to a second one thereof in a state in which the contact caused by the contacting means is kept.

## Claims

### Claim at position 1

-28. (canceled)

### Claim 29

A method for forming, on a film formation substrate, vapor deposition films each having a predetermined pattern, the method comprising the steps of:
(I) forming a partition wall between film formation regions on the film formation substrate, the partition wall having a cross section in a reverse tapered shape and having a predetermined height;
(II) providing a mask unit so that the mask unit faces the film formation substrate, the mask unit including:
(i) a vapor deposition mask that has a plurality of openings and that is smaller in area than a vapor deposition region of the film formation substrate, wherein the vapor deposition mask includes an engaging section configured to engage with the partition wall, and
(ii) a vapor deposition source that has an emission hole configured to emit a vapor deposition particle, the emission hole being provided so as to face the vapor deposition mask, the vapor deposition mask and the vapor deposition source being separated by a fixed gap, and bringing the vapor deposition mask and the film formation substrate into contact with each other at the partition wall;
(III) sequentially depositing the vapor deposition particle onto the vapor deposition region of the film formation substrate through the opening of the vapor deposition mask while causing at least one of the vapor deposition mask and the film formation substrate to move relative to each other,
the engaging section having a wall surface having a depressed portion in a reverse tapered shape toward the film formation substrate, the depressed portion corresponding to the partition wall in a one-to-one correspondence,
in the step (II), when the depressed portion of the vapor deposition mask is first brought into contact with the partition wall, the depressed portion of the vapor deposition mask having a larger width than a width of the partition wall or the width of the partition wall having a smaller width than the width of the depressed portion of the vapor deposition mask, so that the depressed portion of the vapor deposition mask and the partition wall are not stuck with each other, and
in the step (III), at least one of the vapor deposition mask and the film formation substrate being caused to move relative to each other so that the depressed portion of the vapor deposition mask and the partition wall are stuck with each other and the engaging section engages with the partition wall along a direction of the relative movement of the film formation substrate and the mask unit, and in a state where the depressed portion of the vapor deposition mask and the partition wall are stuck with each other, while at least one of the mask unit and the film formation substrate is caused to move relative to each other, the vapor deposition particle being deposited onto the vapor deposition region of the film formation substrate.

### Claim 30 (depends on 29)

The method according to claim 29, wherein:
the partition wall is provided in a stripe shape along the direction of the relative movement.

### Claim 31 (depends on 30)

The method according to claim 30, wherein:
the partition wall includes a plurality of discontinuous partition walls.

### Claim 32 (depends on 31)

The method according to claim 31, wherein:
the partition wall is provided in such a pattern that no straight line passing through a discontinuous portion of the partition wall passes over a pixel light-emitting region of the film formation substrate, the pixel light-emitting region corresponding to the respective formation regions of the vapor deposition films.

### Claim 33

A method for forming, on a film formation substrate, vapor deposition films each having a predetermined pattern, the method comprising the steps of:
(I) forming a partition wall between film formation regions on the film formation substrate, the partition wall having a cross section in a reverse tapered shape and having a predetermined height;
(II) providing a mask unit so that the mask unit faces the film formation substrate, the mask unit including:
(i) a vapor deposition mask that has a plurality of openings and that is smaller in area than a vapor deposition region of the film formation substrate, wherein the vapor deposition mask includes an engaging section configured to engage with the partition wall, and
(ii) a vapor deposition source that has an emission hole configured to emit a vapor deposition particle, the emission hole being provided so as to face the vapor deposition mask, the vapor deposition mask and the vapor deposition source being separated by a fixed gap, and bringing the vapor deposition mask and the film formation substrate into contact with each other at the partition wall;
(III) sequentially depositing the vapor deposition particle onto the vapor deposition region of the film formation substrate through the opening of the vapor deposition mask while causing at least one of the vapor deposition mask and the film formation substrate to move relative to each other,
the engaging section having a wall surface having a depressed portion in a reverse tapered shape toward the film formation substrate, the depressed portion corresponding to the partition wall in a one-to-one correspondence,
in the step (II), when the depressed portion of the vapor deposition mask is first brought into contact with the partition wall, the depressed portion of the vapor deposition mask having a larger width than a width of the partition wall or the width of the partition wall having a smaller width than the width of the depressed portion of the vapor deposition mask, so that the depressed portion of the vapor deposition mask and the partition wall are not stuck with each other,
in the step (III), at least one of the vapor deposition mask and the film formation substrate being caused to move relative to each other so that the depressed portion of the vapor deposition mask and the partition wall are stuck with each other and the engaging section engages with the partition wall along a direction of the relative movement of the film formation substrate and the mask unit, and in a state where the depressed portion of the vapor deposition mask and the partition wall are stuck with each other, while at least one of the mask unit and the film formation substrate is caused to move relative to each other, the vapor deposition particle being deposited onto the vapor deposition region of the film formation substrate,
a magnet being provided on a first surface of the film formation substrate, the first surface being opposite to a second surface of the film formation substrate which second surface faces the vapor deposition mask,
the magnet including a plurality of magnets provided along a first direction in which at least a first one of the mask unit and the film formation substrate moves relative to a second one thereof,
the magnets each having a stripe shape extending in a second direction that is perpendicular to the first direction and that is parallel to the film formation substrate,
the magnets being provided only at such a position as to correspond to the vapor deposition mask,
in the step (III), the magnets being so controlled that in a case where the film formation substrate is present between the magnets and the vapor deposition mask, (i) only a line of magnets overlapping the film formation substrate generate a magnetic force and (ii) a line of magnets not overlapping the film formation substrate are stopped from generating a magnetic force.

### Claim 34 (depends on 33)

The method according to claim 33, wherein:
the magnet has, on a surface in contact with the film formation substrate, a contact area reducing structure for reducing an area of contact with the film formation substrate.

### Claim 35 (depends on 29)

The method according to claim 29, wherein:
an electrostatic chuck is in contact with a first surface of the film formation substrate, the first surface being opposite to a second surface of the film formation substrate which second surface faces the vapor deposition mask, and that holds the film formation substrate.

### Claim 36 (depends on 35)

The method according to claim 35, wherein:
the electrostatic chuck has, on a surface in contact with the film formation substrate, a contact area reducing structure for reducing an area of contact with the film formation substrate.

### Claim 37 (depends on 34)

The method according to claim 34, wherein:
the contact area reducing structure is a hemispheric protruding structure.

### Claim 38 (depends on 29)

The method according to claim 29, wherein:
the vapor deposition mask is a rectangular vapor deposition mask that has (i) along a short-axis direction thereof, a side shorter than a width of the vapor deposition region along a side facing the short-axis direction of the vapor deposition mask and that has (ii) along a long-axis direction thereof, a side longer than a width of the vapor deposition region along a side facing the long-axis direction of the vapor deposition mask.

### Claim 39 (depends on 29)

The method according to claim 29, wherein a first alignment marker on the film formation substrate and a second alignment marker on the vapor deposition mask, the method further comprising:
aligning the film formation substrate and the vapor deposition mask with use of the first and second alignment markers.

### Claim 40 (depends on 29)

The method according to claim 29, wherein:
the mask unit is provided so that the emission hole faces the opening of the vapor deposition mask in a one-to-one correspondence.

### Claim 41 (depends on 29)

The method according to claim 29, wherein:
the vapor deposition films each having the predetermined pattern are each an organic layer for an organic electroluminescent device.

### Claim 42 (depends on 36)

The method according to claim 36, wherein:
the contact area reducing structure is a hemispheric protruding structure.

### Claim 43

A method for forming, on a film formation substrate, vapor deposition films each having a predetermined pattern, the method comprising the steps of:
(I) forming a plurality of discontinuous partition walls each of which has a cross section in a reverse tapered shape and has a predetermined height and each of which stands between film formation regions on the film formation substrate, the plurality of discontinuous partition walls each being provided in such a pattern that no straight line passing through a discontinuous portion of the partition walls passes over a pixel light-emitting region of the film formation substrate, the pixel light-emitting region corresponding to respective pattern formation regions of the vapor deposition films;
(II) providing a mask unit so that the mask unit faces the film formation substrate, the mask unit including (i) a vapor deposition mask that has a plurality of openings and that is smaller in area than a vapor deposition region of the film formation substrate, wherein the vapor deposition mask includes an engaging section configured to engage with the partition wall, and (ii) a vapor deposition source that has an emission hole configured to emit a vapor deposition particle, the emission hole being provided so as to face the vapor deposition mask, the vapor deposition mask and the vapor deposition source being separated by a fixed gap, and bringing the vapor deposition mask and the film formation substrate into contact with each other at the partition wall;
(III) sequentially depositing the vapor deposition particle onto the vapor deposition region of the film formation substrate through the opening of the vapor deposition mask while causing at least one of the vapor deposition mask and the film formation substrate to move relative to each other,
the engaging section having a wall surface having a depressed portion in a reverse tapered shape toward the film formation substrate, the depressed portion corresponding to the partition wall in a one-to-one correspondence,
in the step (II), when the depressed portion of the vapor deposition mask is first brought into contact with the partition wall, the depressed portion of the vapor deposition mask having a larger width than a width of the partition wall or the width of the partition wall having a smaller width than the width of the depressed portion of the vapor deposition mask, so that the depressed portion of the vapor deposition mask and the partition wall are not stuck with each other, and
in the step (III), at least one of the vapor deposition mask and the film formation substrate being caused to move relative to each other so that the depressed portion of the vapor deposition mask and the partition wall are stuck with each other and the engaging section engages with the partition wall along a direction of the relative movement of the film formation substrate and the mask unit, and in a state where the depressed portion of the vapor deposition mask and the partition wall are stuck with each other, while at least one of the mask unit and the film formation substrate is caused to move relative to each other, the vapor deposition particle being deposited onto the vapor deposition region of the film formation substrate.

### Claim 44 (depends on 43)

The method according to claim 43, wherein:
the vapor deposition films each having the predetermined pattern are each an organic layer for an organic electroluminescent device.