# US 2016/0260894 A1 · Methods of manufacturing a magnetic field sensor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0260894 A1
- Document ID: US20160260894A1
- Status: Published application
- Kind: A1
- Application number: 15/142,721
- Filed: 2016-04-29
- Published: 2016-09-08
- Earliest claimed: 2010-03-31
- Assignees: Everspin Technologies, Inc.
- Applicants: Everspin Technologies, Inc.
- Inventors: Renu WHIG; Phillip MATHER; Kenneth SMITH; Sanjeev AGGARWAL; Jon SLAUGHTER; Nicholas RIZZO
- Web page: https://patentgrep.com/patent/US20160260894A1

## CPC

- H10N 50/01: Manufacture or treatment
- B82Y 25/00: Nanomagnetism, e.g. magnetoimpedance, anisotropic magnetoresistance, giant magnetoresistance or tunneling magnetoresistance
- G01R 33/0052: {Manufacturing aspects; Manufacturing of single devices, i.e. of semiconductor magnetic sensor chips (devices based on galvano-magnetic effect or the like H10N50/85)}
- G01R 33/09: Magnetoresistive devices
- G01R 33/093: {using multilayer structures, e.g. giant magnetoresistance sensors (thin magnetic films H01F10/00)}
- G01R 33/098: {comprising tunnel junctions, e.g. tunnel magnetoresistance sensors}
- H10B 61/00: Magnetic memory devices, e.g. magnetoresistive RAM [MRAM] devices
- H10N 50/10: Magnetoresistive devices
- H10N 50/80: Constructional details
- H10N 59/00: Integrated devices, or assemblies of multiple devices, comprising at least one galvanomagnetic or Hall-effect element covered by groups H10N50/00 - H10N52/00 (MRAM devices H10B61/00)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- G01R: MEASURING ELECTRIC VARIABLES; MEASURING MAGNETIC VARIABLES (indicating correct tuning of resonant circuits H03J3/12)
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A semiconductor process integrates three bridge circuits, each include magnetoresistive sensors coupled as a Wheatstone bridge on a single chip to sense a magnetic field in three orthogonal directions. The process includes various deposition and etch steps forming the magnetoresistive sensors and a plurality of flux guides on one of the three bridge circuits for transferring a “Z” axis magnetic field onto sensors orientated in the XY plane.

## Claims

### Claim at position 1

1-27. (canceled)

### Claim 28

A method of manufacturing an integrated magneto-resistive sensor, the method comprising:
forming a first plurality of magneto-resistive sensor elements over a substrate, wherein forming the first plurality of magneto-resistive sensor elements includes:
forming a reference layer,
forming an intermediate layer on the reference layer, and
forming a sensing layer on the intermediate layer;
forming conductors to electrically connect the first plurality of magneto-resistive sensor elements;
providing an insulating material over the first plurality of magneto-resistive sensor elements; and
forming flux guides over the insulating material, wherein at least one flux guide is associated with at least one magneto-resistive sensor element of the first plurality of magneto-resistive sensor elements, and wherein the at least one flux guide is offset from the at least one magneto-resistive sensor element.

### Claim 29 (depends on 28)

The method of claim 28, wherein:
forming conductors to electrically connect the first plurality of magneto-resistive sensor elements includes forming a first circuit by electrically connecting the magneto-resistive sensor elements of the first plurality of magneto-resistive sensor elements.

### Claim 30 (depends on 29)

The method of claim 29, wherein the first circuit is a bridge circuit, and wherein the method further includes:
connecting the bridge circuit to a voltage source.

### Claim 31 (depends on 28)

The method of claim 28, wherein forming the first plurality of magneto-resistive sensor elements includes electrically connecting the first plurality of magneto-resistive sensor elements to form a first bridge circuit.

### Claim 32 (depends on 28)

The method of claim 28, wherein the formed conductors electrically connect the first plurality of magneto-resistive sensor elements to form a first circuit.

### Claim 33 (depends on 32)

The method of claim 32, wherein the first circuit is a bridge circuit.

### Claim 34 (depends on 28)

The method of claim 28, wherein the at least one flux guide includes at least one of nickel, a nickel alloy, iron, an iron alloy, cobalt, and a cobalt alloy.

### Claim 35 (depends on 28)

The method of claim 28, wherein the at least one flux guide is formed below the at least one magneto-resistive sensor element.

### Claim 36 (depends on 28)

The method of claim 28, wherein the at least one flux guide is formed above the at least one magneto-resistive sensor element.

### Claim 37 (depends on 28)

The method of claim 28, wherein the at least one flux guide is formed above or below the at least one magneto-resistive sensor element.

### Claim 38 (depends on 28)

The method of claim 28, wherein the magneto-resistive sensor elements are magnetic tunnel junction sensor elements.

### Claim 39 (depends on 28)

The method of claim 28, further comprising:
forming a second plurality of magneto-resistive sensor elements over the substrate; and
forming second conductors to electrically connect the second plurality of magneto-resistive sensor elements.

### Claim 40 (depends on 28)

The method of claim 28, further comprising:
connecting the first plurality of magneto-resistive sensor elements in a circuit such that, in operation, the circuit is configured to subtract a resistance of the least one magneto-resistive sensor element from a resistance of another magneto-resistive sensor element.

### Claim 41 (depends on 28)

The method of claim 28, further comprising:
forming a first bridge circuit by electrically connecting the magneto-resistive sensor elements of the first plurality of magneto-resistive sensor elements;
forming a second plurality of magneto-resistive sensor elements over the substrate; and
forming a second bridge circuit by electrically connecting the magneto-resistive sensor elements of the second plurality of magneto-resistive sensor elements.

### Claim 42 (depends on 28)

The method of claim 28, wherein the intermediate layer includes an insulating material.

### Claim 43 (depends on 28)

The method of claim 28, wherein the sensing layer includes a magnetization direction configured to change when exposed to an external magnetic field.