# US 2016/0260818 A1 · Semiconductor device and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0260818 A1
- Document ID: US20160260818A1
- Status: Published application
- Kind: A1
- Application number: 15/074,014
- Filed: 2016-03-18
- Published: 2016-09-08
- Earliest claimed: 2013-04-12
- Assignees: Sumitomo Electric Device Innovations, Inc.
- Applicants: Sumitomo Electric Device Innovations, Inc.
- Inventors: Masahiro Nishi
- Web page: https://patentgrep.com/patent/US20160260818A1

## CPC

- H10D 30/015: {of FETs having heterojunction interface channels or heterojunction gate electrodes, e.g. HEMT}
- H10D 30/4755: {having wide bandgap charge-carrier supplying layers, e.g. modulation doped HEMTs such as n-AlGaAs/GaAs HEMTs}
- H10D 62/824: comprising only Group III-V materials heterojunctions, e.g. GaN/AlGaN heterojunctions
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10D 64/0125: {characterised by the sectional shape, e.g. T or inverted T}
- H10D 64/256: {for lateral devices wherein the source or drain electrodes are recessed in semiconductor bodies (source or drain electrodes of TFTs H10D30/673)}
- H10P 50/242: {of Group IV materials}
- H10P 50/692: {characterised by their composition, e.g. multilayer masks or materials}
- H10P 50/693: {characterised by their size, orientation, disposition, behaviour or shape, in horizontal or vertical plane}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor device includes a semiconductor layer formed on a substrate, an electrode contact window that includes a recess formed on a surface of the semiconductor layer, an inner wall having a slope, and a source electrode, a drain electrode, and a gate electrode formed on the semiconductor layer, in which the drain electrode is in contact with the slope of the inner wall.

## Claims

### Claim at position 1

1-17. (canceled)

### Claim 18

A method of manufacturing a semiconductor device, the method comprising:
forming a semiconductor layer on a substrate;
forming a first resist on the semiconductor layer;
forming a second resist on the first resist;
forming a first opening pattern of the first resist and a second opening pattern of the second resist, the first opening pattern and the second opening pattern being overlapped with each other;
performing isotropic etching on the semiconductor layer through the first opening pattern and the second opening pattern; and
forming an electrode on a surface of the semiconductor layer which is exposed from the first opening pattern and the second opening pattern.

### Claim 19 (depends on 18)

The method according to claim 18,
wherein the performing of the isotropic etching comprises forming a recess on the surface, the recess having a slanted slope, and
wherein the forming of the electrode comprises forming the electrode on the recess.

### Claim 20 (depends on 19)

The method according to claim 19,
wherein the semiconductor layer is formed by an electron transit layer on the substrate, an electron supply layer on the electron transit layer, and a cap layer on the electron supply layer, and
wherein a bottom of the recess is formed at a surface of the electron supply layer.

### Claim 21 (depends on 20)

The method according to claim 20,
wherein the electron transit layer includes GaN, the electron supply layer includes AlGaN or InAlN, and the cap layer includes GaN.

### Claim 22 (depends on 20)

The method according to claim 20,
wherein the electrode is formed so as to be in contact with the bottom and the slanted slope of the recess in the forming of the electrode.

### Claim 23 (depends on 18)

The method according to claim 18,
wherein the electrode is a source electrode or a drain electrode.

### Claim 24 (depends on 18)

The method according to claim 18,
wherein a size of the first opening is greater than that of the second opening.

### Claim 25 (depends on 18)

The method according to claim 18,
wherein the performing of the isotropic etching is conducted after performing anisotropic etching on the semiconductor layer through the first opening pattern and the second opening pattern.

### Claim 26 (depends on 25)

The method according to claim 25,
wherein any of Cl2, BCl3, and SiCl4 is used for the isotropic etching and the anisotropic etching.

### Claim 27 (depends on 25)

The method according to claim 25,
wherein the isotropic etching is wet etching, and
wherein potassium hydroxide or sodium hydroxide is used for the wet etching.
