# US 2016/0260772 A1 · Semiconductor device and method of manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0260772 A1
- Document ID: US20160260772A1
- Status: Published application
- Kind: A1
- Application number: 15/047,746
- Filed: 2016-02-19
- Published: 2016-09-08
- Earliest claimed: 2015-03-06
- Assignees: Renesas Electronics Corporation
- Applicants: Renesas Electronics Corporation
- Inventors: Tatsuya USAMI; Yukio MIURA
- Web page: https://patentgrep.com/patent/US20160260772A1

## CPC

- H10N 50/10: Magnetoresistive devices
- H10B 61/22: {of the field-effect transistor [FET] type}
- H10N 50/01: Manufacture or treatment
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

To provide a magnetoresistance effect element configuring MRAM by dry etching and thereby processing a stacked film including magnetic layers, in order to prevent a leakage current from flowing between the magnetic layers, that is, magnetic free layer and magnetic pinned layer which configure a magnetic tunnel junction (MTJ) via a metal deposit that has attached to the side wall of the MTJ. After formation of the magnetoresistance effect element by dry etching, plasma treatment is performed in a gas atmosphere containing carbon and oxygen to remove a metal deposit attached to the magnetoresistance effect element. By this plasma treatment, oxide films are formed on the side walls of the magnetic free layer and the magnetic pinned layer, respectively.

## Claims

### Claim 1

A method of manufacturing a semiconductor device equipped with a memory cell including a magnetoresistance effect element, comprising the steps of:
(a) stacking a first magnetic layer, an oxidized magnetic layer, and a second magnetic layer successively to form a stacked film;
(b) processing the first magnetic layer, the oxidized magnetic layer, and the second magnetic layer by first anisotropic etching to form the magnetoresistance effect element having the stacked film; and
(c) subjecting the magnetoresistance effect element to plasma treatment in an atmosphere of a gas containing carbon and oxygen.

### Claim 2 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein in the step (b), a conductor substance configuring a portion of the first magnetic layer or the second magnetic layer is etched by the first anisotropic etching and then attaches to a surface of the magnetoresistance effect element obtained by being processed by the first anisotropic etching; and
wherein in the step (c), the plasma treatment is performed to remove the conductor substance that has attached to the surface of the magnetoresistance effect element.

### Claim 3 (depends on 2)

The method of manufacturing a semiconductor device according to claim 2,
wherein in the step (c), the conductor substance that has attached to the surface of the magnetoresistance effect element reacts with the gas to form a carbonyl compound, and the carbonyl compound is sublimed to remove the conductor substance.

### Claim 4 (depends on 3)

The method of manufacturing a semiconductor device according to claim 3,
wherein in the step (c), a temperature in a plasma apparatus in which the plasma treatment is performed is set at 104° C. or more.

### Claim 5 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein in the step (c), the plasma treatment is performed to oxidize a side wall of the first magnetic layer to form a first oxidized insulating film and oxidize a side wall of the second magnetic layer to form a second oxidized insulating film.

### Claim 6 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein in the step (b), a conductor substance configuring a portion of the first magnetic layer or the second magnetic layer is etched by the first anisotropic etching and then attaches to a surface of the magnetoresistance effect element processed by the first anisotropic etching, and
wherein in the step (c), the plasma treatment is performed to oxidize the conductor substance that has attached to the surface of the magnetoresistance effect element.

### Claim 7 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein the first magnetic layer or the second magnetic layer contains cobalt or iron.

### Claim 8 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein the gas contains a carbon oxide gas.

### Claim 9 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein the gas contains an O2 gas.

### Claim 10 (depends on 3)

The method of manufacturing a semiconductor device according to claim 3,
wherein the step (b) comprises the sub-steps of:
(b1) processing the first magnetic layer by second anisotropic etching; and
(b2) processing the second magnetic layer by third anisotropic etching,
wherein the oxidized magnetic layer is processed in the step (b1) or the step (b2),
wherein the step (b1) and the step (b2) are carried out to form the magnetoresistance effect element,
wherein a width of the first magnetic layer configuring the magnetoresistance effect element is greater than a width of the second magnetic layer configuring the magnetoresistance effect element, in a direction perpendicular to a stacking direction of the stacked film.

### Claim 11

A semiconductor device, comprising:
a first magnetic layer;
an oxidized magnetic layer formed over the first magnetic layer;
a second magnetic layer formed on the oxidized magnetic layer;
a first oxidized insulating film covering a side wall of the first magnetic layer; and
a second oxidized insulating film covering a side wall of the second magnetic layer.

### Claim 12 (depends on 11)

The semiconductor device according to claim 11;
wherein the first oxidized insulating film contains an oxide of a composition of the first magnetic layer and the second oxidized insulating film contains an oxide of a composition of the second magnetic layer.

### Claim 13 (depends on 11)

The semiconductor device according to claim 11,
wherein the first magnetic layer and the second magnetic layer contain cobalt or iron and the first oxidized insulating film and the second oxidized insulating film contain cobalt oxide or iron oxide.

### Claim 14 (depends on 11)

The semiconductor device according to claim 11,
wherein a width of the first magnetic layer is greater than a width of the second magnetic layer in a direction perpendicular to a stacking direction of the first magnetic layer, the oxidized magnetic layer, and the second magnetic layer.

### Claim 15 (depends on 14)

The semiconductor device according to claim 14,
wherein the first magnetic layer is, at an upper surface at both end portions thereof, not covered with the second magnetic layer but covered with the oxidized magnetic layer.