# US 2016/0260769 A1 · Fabricating method of back-illuminated image sensor with dishing depression surface

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0260769 A1
- Document ID: US20160260769A1
- Status: Published application
- Kind: A1
- Application number: 15/153,702
- Filed: 2016-05-12
- Published: 2016-09-08
- Earliest claimed: 2012-06-14
- Assignees: United Microelectronics Corp.
- Applicants: United Microelectronics Corporation
- Inventors: TSENG-FEI WEN
- Web page: https://patentgrep.com/patent/US20160260769A1

## CPC

- H10F 39/024: {of coatings or optical elements}
- H10F 39/014: {of CMOS image sensors}
- H10F 39/028: {performed after manufacture of the image sensors, e.g. annealing, gettering of impurities, short-circuit elimination or recrystallisation}
- H10F 39/199: {Back-illuminated image sensors}
- H10F 39/807: {Pixel isolation structures}
- H10F 71/128: {Annealing}
- H10F 77/413: {directly associated or integrated with the devices, e.g. back reflectors (directly associated or integrated with photovoltaic cells H10F77/42)}
- H10F 39/8053: {Colour filters}
- H10F 39/8063: {Microlenses}
- H10F 77/40: Optical elements or arrangements (surface textures H10F77/70)
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION

## Abstract

A fabricating method of a back-illuminated image sensor includes the following steps. First, a silicon wafer having a first surface and a second surface is provided, wherein a number of trench isolations are formed in the first surface, and at least one image sensing member is formed between the trench isolations. Then, a first chemical mechanical polishing (CMP) process is performed to the second surface using the trench isolations as a polishing stop layer to thin the silicon wafer. Because the polishing rate of the silicon material in the silicon wafer is different with that of the isolation material of the trench isolations in the first CMP process, at least one dishing depression is formed in the second surface of the silicon wafer. Finally, a microlens is formed above the dishing depression, and a surface of the microlens facing the dishing depression is a curved surface.

## Claims

### Claim 1

A fabricating method of a back-illuminated image sensor, comprising:
providing a silicon wafer, comprising a first surface and a second surface, wherein a plurality of trench isolations are formed in the first surface, and at least one image sensing member is formed between the plurality of trench isolations;
performing a first chemical mechanical polishing (CMP) process to the second surface using the trench isolations as a polishing stop layer to thin the silicon wafer, wherein a polishing rate of a silicon material of the silicon wafer is different with a polishing rate of an isolation material of the trench isolations, and at least one right-side up dishing depression is formed in the second surface of the silicon wafer; and
forming a microlens above the right-side up dishing depression, wherein a surface of the microlens facing the right-side up dishing depression is a smoothly curving surface.

### Claim 2 (depends on 1)

The fabricating method of a back-illuminated image sensor of claim 1, further comprising a thinning process that reduces a thickness of the silicon wafer to a predetermined value, and then the CMP process is performed.

### Claim 3 (depends on 2)

The fabricating method of a back-illuminated image sensor of claim 2, wherein the thinning process comprises a second CMP process and an etching process.

### Claim 4 (depends on 2)

The fabricating method of a back-illuminated image sensor of claim 2, wherein the predetermined values is not less than 3 micrometers.

### Claim 5 (depends on 1)

The fabricating method of a back-illuminated image sensor of claim 1, wherein the polishing rate of the silicon material is greater than the polishing rate of the isolation material.

### Claim 6 (depends on 5)

The fabricating method of a back-illuminated image sensor of claim 5, wherein a ratio of the polishing rate of the silicon material to the polishing rate of the isolation material is greater than 200.

### Claim 7 (depends on 1)

The fabricating method of a back-illuminated image sensor of claim 1, prior to forming the microlens above the right-side up dishing depressions, further comprising:
performing an ion implantation and an annealing process to the second surface of the silicon wafer; and
forming an anti-reflection layer on the second surface.

### Claim 8 (depends on 1)

The fabricating method of a back-illuminated image sensor of claim 1, further comprising:
forming a first plane layer on the microlens; and
forming a color filer on the first plane layer.

### Claim 9 (depends on 8)

The fabricating method of a back-illuminated image sensor of claim 8, further comprising:
forming a second plane layer on the color filter; and
forming a second microlens on the second plane layer.

### Claim 10 (depends on 1)

The fabricating method of a back-illuminated image sensor of claim 1, upon forming the microlens above the right-side up dishing depression, wherein an edge of the surface of the microlens is directly next to an end of one of the trench isolations.

### Claim 11 (depends on 1)

The fabricating method of a back-illuminated image sensor of claim 1, upon forming the microlens above the right-side up dishing depression, wherein an edge of the right-side up dishing depression touches an end of one of the trench isolations.