# US 2016/0260679 A1 · Hybrid interconnect for low temperature attach

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0260679 A1
- Document ID: US20160260679A1
- Status: Published application
- Kind: A1
- Application number: 14/430,131
- Filed: 2014-03-27
- Published: 2016-09-08
- Earliest claimed: 2014-03-27
- Assignees: Intel Corporation
- Applicants: Intel Corporation
- Inventors: Kabirkumar J. Mirpuri; Hongjin Jiang; Tyler N. Osborn; Rajen S. Sidhu; Ibrahim Bekar; Susheel G. Jadhav
- Web page: https://patentgrep.com/patent/US20160260679A1

## CPC

- H10W 70/098: {Applying pastes or inks, e.g. screen printing (H10W70/095 takes precedence)}
- H10W 90/701: {characterised by the relative positions of pads or connectors relative to package parts}
- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10W 72/072: {of bump connectors}
- H10W 72/073: {of die-attach connectors}
- H10W 72/232: {Plan-view shape, i.e. in top view}
- H10W 72/244: {relative to underlying supporting features, e.g. bond pads, RDLs or vias}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/29: Bond pads specially adapted therefor
- H10W 72/344: {relative to underlying supporting features, e.g. bond pads, RDLs or vias}
- H10W 72/352: {comprising metals or metalloids, e.g. solders}
- H10W 72/90: Bond pads, in general
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/953: {not comprising solid metals or solid metalloids, e.g. polymers, ceramics or liquids}
- H10W 74/15: on active surfaces of flip-chip devices, e.g. underfills
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Apparatuses, processes, and systems related to an interconnect with an increased z-height and decreased reflow temperature are described herein. In embodiments, an interconnect may include a solder ball and a solder paste to couple the solder ball to a substrate. The solder ball and/or solder paste may be comprised of an alloy with a relatively low melting point and an alloy with a relatively high melting point.

## Claims

### Claim 1

An apparatus comprising:
a substrate having a pad disposed on the substrate;
a solder ball coupled with the pad, the solder ball including an alloy of tin, silver, and copper; and
a solder paste generally positioned between the pad and the solder ball, the solder paste including the alloy and a low-temperature solder (LTS) with a melting point that is less than or equal to a melting point of the alloy.

### Claim 2 (depends on 1)

The apparatus of claim 1, wherein the pad comprises copper and has a surface finish of nickel, palladium, gold, copper, or an organic solderability preservative.

### Claim 3 (depends on 1)

The apparatus of claim 1, wherein the alloy is a lead-free alloy.

### Claim 4 (depends on 1)

The apparatus of claim 1, wherein the LTS comprises indium or bismuth.

### Claim 5 (depends on 1)

The apparatus of claim 1, wherein the solder paste comprises approximately equal amounts of the alloy and the LTS.

### Claim 6 (depends on 1)

The apparatus of claim 1, further comprising:
a mold compound coupled with the substrate and generally disposed laterally adjacent to, and generally surrounding, the solder ball and the solder paste.

### Claim 7 (depends on 1)

The apparatus of claim 1, further comprising an inter-metallic compound (IMC) disposed between the solder paste and the substrate.

### Claim 8 (depends on 7)

The apparatus of claim 7, wherein the IMC comprises nickel, copper, tin, bismuth, or alloys thereof.

### Claim 9 (depends on 1)

The apparatus of claim 1, wherein the alloy has a melting point between approximately 180° Celsius and approximately 280° Celsius.

### Claim 10 (depends on 9)

The apparatus of claim 9, wherein the solder paste has a melting point greater than or equal to 175° Celsius.

### Claim 11

A method comprising:
depositing a solder paste on a pad of a substrate, the solder paste including a low-temperature solder (LTS) with a melting point that is less than or equal to 217° Celsius and an alloy of tin, silver, and copper;
positioning a solder ball including the alloy on the solder paste such that the solder paste is disposed between the pad and the solder ball; and
performing a reflow process at a temperature above the melting point of the LTS and below a melting point of the alloy.

### Claim 12 (depends on 11)

The method of claim 11, wherein the LTS comprises indium or bismuth.

### Claim 13 (depends on 11)

The method of claim 11, wherein the melting point of the alloy is between approximately 180° Celsius and approximately 280° Celsius.

### Claim 14 (depends on 11)

The method of claim 11, further comprising forming, during the low-temperature reflow process, an inter-metallic compound (IMC) between the solder ball and the pad, and directly adjacent to the pad.

### Claim 15 (depends on 11)

The method of claim 11, wherein the pad comprises copper.

### Claim 16

An apparatus comprising:
a substrate with a first side and a second side, a die mounted on the first side and a pad disposed on the first side of the substrate;
a mold compound coupled with the first side of the substrate, the mold compound having a through-mold via over the pad;
a solder joint positioned within the through-mold via and coupled with the pad, the solder joint comprising:
a solder ball comprised of a lead-free alloy; and
a solder paste generally positioned between the substrate and the solder ball, the solder paste including generally equal amounts of the lead-free alloy and a low-temperature solder (LTS) having a melting point that is less than or equal to 175° Celsius, wherein the solder joint is configured to route electrical signals of the die.

### Claim 17 (depends on 16)

The apparatus of claim 16, wherein the lead-free alloy comprises tin, silver, and copper.

### Claim 18 (depends on 16)

The apparatus of claim 16, wherein the LTS comprises indium or bismuth.

### Claim 19 (depends on 16)

The apparatus of claim 16, wherein the lead-free alloy has a melting point of 217° Celsius.

### Claim 20 (depends on 19)

The apparatus of claim 19, wherein the solder paste has a melting point greater than 175° Celsius.

### Claim 21 (depends on 16)

The apparatus of claim 16, wherein the pad comprises copper with a surface finish of nickel, palladium, gold, copper, or an organic solderability preservative.