# US 2016/0260611 A1 · Method of controlling solid phase diffusion of boron dopants to form ultra-shallow doping regions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0260611 A1
- Document ID: US20160260611A1
- Status: Published application
- Kind: A1
- Application number: 15/055,920
- Filed: 2016-02-29
- Published: 2016-09-08
- Earliest claimed: 2015-03-03
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Steven P. Consiglio; Robert D. Clark; David L. O'Meara
- Web page: https://patentgrep.com/patent/US20160260611A1

## CPC

- H10P 32/171: {being group IV material}
- H10P 32/1408: {from or through or into an external applied layer, e.g. photoresist or nitride layers}
- H10P 32/1412: {through the applied layer}
- H10D 30/0241: {doping of vertical sidewalls, e.g. using tilted or multi-angled implants}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/68: Organic materials, e.g. photoresists
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method is provided for forming an ultra-shallow boron doping region in a semiconductor device. The method includes depositing a diffusion filter layer on a substrate, the diffusion filter containing a boron nitride layer, a boron oxynitride layer, a silicon nitride layer, or a silicon oxynitride layer, and depositing a boron dopant layer on the diffusion filter layer, the boron dopant layer containing boron oxide, boron oxynitride, or a combination thereof, with the proviso that the diffusion filter layer and the boron dopant layer do not contain the same material. The method further includes heat-treating the substrate to form the ultra-shallow boron dopant region in the substrate by controlled diffusion of boron from the boron dopant layer through the diffusion filter layer and into the substrate.

## Claims

### Claim 1

A method of forming an ultra-shallow boron doping region in a semiconductor device, the method comprising:
depositing a diffusion filter layer on a substrate, the diffusion filter layer containing a boron nitride layer, a boron oxynitride layer, a silicon nitride layer, or a silicon oxynitride layer;
depositing a boron dopant layer on the diffusion filter layer, the boron dopant layer containing boron oxide, boron oxynitride, or a combination thereof, with the proviso that the diffusion filter layer and the boron dopant layer do not contain the same material; and
heat-treating the substrate to form the ultra-shallow boron dopant region in the substrate by controlled diffusion of boron from the boron dopant layer through the diffusion filter layer and into the substrate.

### Claim 2 (depends on 1)

The method of claim 1, further comprising prior to the heat-treating, depositing a cap layer on the boron dopant layer.

### Claim 3 (depends on 2)

The method of claim 2, wherein the cap layer contains a boron nitride layer.

### Claim 4 (depends on 1)

The method of claim 1, further comprising removing the diffusion filter layer and the boron dopant layer from the substrate.

### Claim 5 (depends on 1)

The method of claim 1, wherein the heat-treating is performed in an inert atmosphere.

### Claim 6 (depends on 1)

The method of claim 1, wherein the heat-treating is performed at a substrate temperature greater than 800° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the heat-treating is performed at a substrate temperature of 900° C., or greater.

### Claim 8 (depends on 1)

The method of claim 1, wherein the substrate contains a raised feature or a recessed feature, and the diffusion filter layer and the boron dopant layer are conformally deposited on the raised feature or in the recessed feature.

### Claim 9 (depends on 1)

The method of claim 1, wherein the diffusion filter layer, the boron dopant layer, or both the diffusion filter layer and the boron dopant layer are deposited by atomic layer deposition (ALD).

### Claim 10 (depends on 9)

The method of claim 9, wherein the diffusion filter layer and the boron dopant layer are deposited using alternating gaseous exposures of a boron amide precursor and a reactant gas.

### Claim 11 (depends on 10)

The method of claim 10, wherein the boron dopant layer contains boron oxide and the reactant gas includes H2O, O2, or O3, or a combination of two or more thereof.

### Claim 12 (depends on 10)

The method of claim 10, wherein the boron dopant layer contains boron oxynitride and the reactant gas includes a) H2O, O2, or O3, and NH3, or b) NO, NO2, or N2O, and optionally one or more of H2O, 02, O3, and NH3.

### Claim 13 (depends on 9)

The method of claim 9, wherein the diffusion filter layer and the boron dopant layer are deposited using alternating gaseous exposures of an organoboron precursor and a reactant gas.

### Claim 14 (depends on 13)

The method of claim 13, wherein the boron dopant layer contains boron oxide and the reactant gas includes H2O, O2, or O3, or a combination of two or more thereof.

### Claim 15 (depends on 1)

The method of claim 1, wherein the boron dopant layer contains boron oxynitride and the reactant gas includes a) H2O, O2, or O3, and NH3, or b) NO, NO2, or N2O, and optionally one or more of H2O, O2, O3, and NH3.

### Claim 16 (depends on 9)

The method of claim 9, wherein the diffusion filter layer is deposited using alternating gaseous exposures of a boron amide precursor and a reactant gas containing NH3.

### Claim 17 (depends on 9)

The method of claim 9, wherein the diffusion filter layer is deposited using alternating gaseous exposures of organoboron precursor and a reactant gas containing NH3.

### Claim 18 (depends on 1)

The method of claim 1, wherein the diffusion filter layer and the boron dopant layer are deposited in the same process chamber, and wherein the substrate is maintained at the same substrate temperature during deposition of the diffusion filter layer and the boron dopant layer.

### Claim 19

A method of forming an ultra-shallow boron doping region in a semiconductor device, the method comprising:
depositing a diffusion filter layer on a substrate, the diffusion filter containing a boron nitride layer;
depositing a boron dopant layer on the diffusion filter layer, the boron dopant layer containing boron oxide;
depositing a cap layer on the boron dopant layer;
heat-treating the substrate in an inert atmosphere to form the ultra-shallow boron dopant region in the substrate by controlled diffusion of boron from the boron dopant layer through the diffusion filter layer and into the substrate; and
removing the diffusion filter layer and the boron dopant layer from the substrate.

### Claim 20

A method of forming an ultra-shallow boron doping region in a semiconductor device, the method comprising:
depositing a diffusion filter layer on a substrate, the diffusion filter containing a boron nitride layer;
depositing a boron dopant layer on the diffusion filter layer, the boron dopant layer containing boron oxynitride;
depositing a cap layer on the boron dopant layer;
heat-treating the substrate in an inert atmosphere to form the ultra-shallow boron dopant region in the substrate by controlled diffusion of boron from the boron dopant layer through the diffusion filter layer and into the substrate; and
removing the diffusion filter layer and the boron dopant layer from the substrate.