# US 2016/0260608 A1 · Manufacturing method of semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0260608 A1
- Document ID: US20160260608A1
- Status: Published application
- Kind: A1
- Application number: 15/056,543
- Filed: 2016-02-29
- Published: 2016-09-08
- Earliest claimed: 2015-03-03
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Applicants: Toyota Jidosha Kabushiki Kaisha
- Inventors: Tomoharu Ikeda; Shinichiro Miyahara; Sachiko Aoi
- Web page: https://patentgrep.com/patent/US20160260608A1

## CPC

- H10P 50/00: Etching of wafers, substrates or parts of devices
- H10D 62/8325: {Silicon carbide}
- H10P 14/2904: {Silicon carbide}
- H10P 14/3408: {Silicon carbide}
- H10P 30/2042: {into crystalline silicon carbide}
- H10P 30/21: {of electrically active species}
- H10P 30/28: characterised by an annealing step, e.g. for activation of dopants
- H10P 72/74: {using temporarily an auxiliary support}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10P 32/172: {being crystalline silicon carbide}
- H10P 72/7422: {used to protect an active side of a device or wafer}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A manufacturing method of a semiconductor device is provided by forming a trench in a surface of a SiC substrate, positioning a protective substrate to cover the trench, and annealing the SiC substrate and the protective substrate.

## Claims

### Claim 1

A manufacturing method of a semiconductor device, the method comprising:
forming a trench in a surface of a SiC substrate;
positioning a protective substrate to cover the trench; and
annealing the SiC substrate and the protective substrate.

### Claim 2 (depends on 1)

The manufacturing method according to claim 1, wherein
a melting point of the protective substrate is equal to or higher than 2000 degrees Celsius, and
in the annealing of the SiC substrate and the protective substrate, the SiC substrate is annealed at a temperature equal to or higher than 1700 degrees Celsius.

### Claim 3 (depends on 1)

The manufacturing method according to claim 1, the method further comprising:
forming a protective film on the surface of the SiC substrate after the forming of the trench; and
removing the protective film after the annealing of the SiC substrate and the protective substrate,
wherein
in the positioning of the protective substrate, the protective substrate is positioned on the surface side of the SiC substrate on which the protective film has been formed.

### Claim 4 (depends on 1)

The manufacturing method according to claim 1, the method further comprising:
introducing impurities to the SiC substrate before the annealing of the SiC substrate and the protective substrate.

### Claim 5 (depends on 1)

The manufacturing method according to claim 1, wherein
in the positioning of the protective substrate, the SiC substrate is mounted on the protective substrate.

### Claim 6 (depends on 1)

The manufacturing method according to claim 1, wherein
the protective substrate consists of Carbon or a compound including Carbon.