# US 2016/0260602 A1 · Adhesion improvements for oxide-silicon stack

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0260602 A1
- Document ID: US20160260602A1
- Status: Published application
- Kind: A1
- Application number: 14/400,735
- Filed: 2014-10-15
- Published: 2016-09-08
- Earliest claimed: 2013-11-04
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Subbalakshmi SREEKALA; Nagarajan RAJAGOPALAN; Bok Hoen KIM
- Web page: https://patentgrep.com/patent/US20160260602A1

## CPC

- H10P 14/6336: {in the presence of a plasma [PECVD]}
- C23C 16/24: Deposition of silicon only
- C23C 16/402: {Silicon dioxide}
- C23C 16/4408: {by purging residual gases from the reaction chamber or gas lines}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3454: {Amorphous}
- H10P 14/3602: {In-situ cleaning}
- H10P 14/416: {of highly doped semiconductor materials, e.g. polysilicon layers or amorphous silicon layers}
- H10P 14/6504: {In-situ cleaning}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10B 41/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10B 43/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

Embodiments generally relate to methods of controlling hydrogen content in a silicon oxide/amorphous silicon stack. By precleaning the substrate of residues, controlling the delivery of hydrogen during the stack deposition and preventing outgassing of hydrogen from deposited layers during subsequent layer deposition and processing, the effects of delamination can be avoided in the formation of devices, such as 3D NAND devices.

## Claims

### Claim 1

A method comprising:
positioning a substrate in a processing chamber;
energizing a preclean gas into a plasma to create an energized preclean gas;
delivering the energized preclean gas to the substrate;
purging the processing chamber; and
depositing one or more silicon oxide/silicon containing stacks on a substrate in the presence of a vacuum, wherein depositing a silicon oxide/silicon-containing stack comprises:
energizing a first process gas into a first plasma;
depositing a first material layer on the substrate from the first plasma;
energizing a second process gas into a second plasma;
depositing a layer of a second material on the substrate from the second plasma; and
repeating the above steps until a predetermined number of the first material layers and the second material layers have been deposited on the substrate, wherein the first material layer and the second material layer are either a silicon oxide layer or an amorphous silicon layer and wherein the second material layer is different from the first material layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the substrate comprises a carbon-containing residue and the preclean gas is an oxygen-containing gas.

### Claim 3 (depends on 1)

The method of claim 1, wherein the substrate comprises an oxygen-containing residue and the preclean gas is a hydrogen-containing gas.

### Claim 4 (depends on 1)

The method of claim 1, wherein the preclean gas is an inert gas.

### Claim 5 (depends on 1)

The method of claim 1, further comprising:
plasma purging the processing chamber to expose a surface of the first material layer, creating first gas contaminants;
gas purging the processing chamber to remove the first gas contaminants;
plasma purging the processing chamber to expose a surface of the second material layer, creating second gas contaminants; and
gas purging the processing chamber to remove the second gas contaminants.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first material layer and the second material layer are deposited at a temperature between about 500 degrees Celsius and about 650 degrees Celsius.

### Claim 7 (depends on 1)

The method of claim 1, wherein the substrate comprises an inner zone and an outer zone which circumscribes the inner zone, and wherein the temperature of the outer zone is between 5 degrees Celsius and about 20 degrees Celsius higher than the temperature of the inner zone.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first material layer and the second material layer are sequentially annealed at a temperature between about 500 degrees Celsius and about 650 degrees Celsius.

### Claim 9 (depends on 1)

The method of claim 1, wherein the first material layer has a first thickness and the second material layer has a second thickness, and wherein the first thickness is less than the second thickness.

### Claim 10 (depends on 1)

The method of claim 1, wherein the silicon oxide layer has a tensile stress.

### Claim 11 (depends on 1)

The method of claim 1, wherein the amorphous silicon layer comprises boron.

### Claim 12

A method of forming a stack comprising:
energizing a first process gas into a first plasma;
depositing a first material layer on the substrate from the first plasma, the layer of the first material having a first thickness;
plasma purging the PECVD chamber to expose a surface of the first material layer, creating first gas contaminants;
gas purging the PECVD chamber to remove the first gas contaminants;
energizing a second process gas into a second plasma;
depositing a second material layer on the first material layer from the second plasma, the second material layer having a second thickness;
plasma purging the PECVD chamber to expose a surface of the second material layer, creating second gas contaminants;
gas purging the PECVD chamber to remove the second gas contaminants; and
repeating the above steps until a predetermined number of the first material layers and the second material layers have been deposited on the substrate, wherein, during at least one of the above steps, at least a portion of the chamber, the substrate support or combinations thereof is maintained at a temperature of between about 500 degrees Celsius and about 650 degrees Celsius, wherein the first material layer and the second material layer are either a silicon oxide layer or an amorphous silicon layer and wherein the second material layer is different from the first material layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the substrate is maintained at a temperature between 500 degrees Celsius and 650 degrees Celsius during the deposition of the first material layer and the deposition of the second material layer.

### Claim 14 (depends on 12)

The method of claim 12, wherein the substrate comprises an inner zone and an outer zone which circumscribes the inner zone, and wherein the temperature of the outer zone is between 5 degrees Celsius and about 20 degrees Celsius higher than the temperature of the inner zone.

### Claim 15 (depends on 12)

The method of claim 12, wherein the first material layer and the second material layer are sequentially annealed at a temperature between about 500 degrees Celsius and about 650 degrees Celsius.

### Claim 16 (depends on 15)

The method of claim 15, wherein the anneal has a controlled ramp rate.

### Claim 17 (depends on 12)

The method of claim 12, wherein the first material layer has a first thickness and the second material layer has a second thickness, and wherein the first thickness is less than the second thickness.

### Claim 18 (depends on 12)

The method of claim 12, wherein the silicon oxide layer has a tensile stress.

### Claim 19 (depends on 12)

The method of claim 12, wherein the substrate receives a silane soak prior to deposition of the first material layer.

### Claim 20

A method of forming a stack comprising:
energizing a first process gas into a first plasma;
depositing a first material layer on the substrate from the first plasma, the layer of the first material having a first thickness, the substrate being maintained at a temperature between 500 degrees Celsius and 650 degrees Celsius;
plasma purging the PECVD chamber to expose a surface of the first material layer, creating first gas contaminants;
gas purging the PECVD chamber to remove the first gas contaminants;
energizing a second process gas into a second plasma;
depositing a second material layer on the first material layer from the second plasma, the second material layer having a second thickness, the substrate being maintained at a temperature between 500 degrees Celsius and 650 degrees Celsius, wherein the first material layer has a first thickness and the second material layer has a second thickness, and wherein the first thickness is less than the second thickness;
plasma purging the PECVD chamber to expose a surface of the second material layer, creating second gas contaminants;
gas purging the PECVD chamber to remove the second gas contaminants; and
repeating the above steps until a predetermined number of the first material layers and the second material layers have been deposited on the substrate, wherein, during at least one of the above steps, at least a portion of the chamber, the substrate support or combinations thereof is maintained at a temperature of between about 500 degrees Celsius and about 650 degrees Celsius, wherein the first material layer and the second material layer are either a silicon oxide layer or an amorphous silicon layer and wherein the second material layer is different from the first material layer.