# US 2016/0258860 A1 · Remaining service life evaluation method for metal pipe suffering from creep damage

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0258860 A1
- Document ID: US20160258860A1
- Status: Published application
- Kind: A1
- Application number: 15/023,361
- Filed: 2014-01-24
- Published: 2016-09-08
- Earliest claimed: 2014-01-24
- Assignees: The Chugoku Electric Power Co., Inc.
- Applicants: The Chugoku Electric Power Co., Inc.
- Inventors: Hidetaka Nishida
- Web page: https://patentgrep.com/patent/US20160258860A1

## CPC

- G01N 17/006: {of metals}
- G01N 3/12: Pressure testing
- G01N 17/008: {Monitoring fouling}
- G01N 2203/0071: Creep
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

A remaining service life evaluation method for evaluating a remaining service life of a metal pipe suffering from creep damage on a basis of a master curve that is prepared in advance that includes wrapping a steel strip around an outer peripheral face of the metal pipe under same conditions as those during an internal pressure creep test and evaluating a remaining service life of the metal pipe on a basis of a degree of deterioration of the steel strip.

## Claims

### Claim 1

A remaining service life evaluation method for evaluating a remaining service life of a metal pipe suffering from creep damage on a basis of a master curve that is prepared in advance, the master curve being prepared by performing an internal pressure creep test in a state in which a steel strip, made of a metal material having a thermal expansion coefficient and strength of the metal pipe or greater, is wrapped under tension around an outer peripheral face of a test piece made of the same material and having the same inner and outer diameters as the metal pipe, the master curve indicating a relationship between a degree of deterioration of the steel strip and a remaining service life of the metal pipe, the remaining service life evaluation method comprising:
wrapping a steel strip around an outer peripheral face of the metal pipe under the same conditions as those during the internal pressure creep test; and
evaluating a remaining service life of the metal pipe on a basis of a degree of deterioration of the steel strip.

### Claim 2 (depends on 1)

The remaining service life evaluation method according to claim 1, wherein the steel strip is subjected to heat treatment in advance.

### Claim 3 (depends on 1)

The remaining service life evaluation method according to claim 1, wherein the steel strip includes:
a ring shaped section of a strip shaped thin metal sheet that is curved in a circular cylindrical shape and has a circumferential direction length determined so as to be shorter than a length around the outer peripheral face of the metal pipe;
a pair of flange portions provided extending in an outer peripheral direction from circumferential direction ends of the ring shaped section; and
a connection screw that adjusts a spacing between the flange portions and connects the flange portions with each other.

### Claim 4 (depends on 1)

The remaining service life evaluation method according to claim 1, wherein the steel strip is made of the same metal material as that of the metal pipe.

### Claim 5 (depends on 2)

The remaining service life evaluation method according to claim 2, wherein the steel strip includes:
a ring shaped section of a strip shaped thin metal sheet that is curved in a circular cylindrical shape and has a circumferential direction length determined so as to be shorter than a length around the outer peripheral face of the metal pipe;
a pair of flange portions provided extending in an outer peripheral direction from circumferential direction ends of the ring shaped section; and
a connection screw that adjusts a spacing between the flange portions and connects the flange portions with each other.

### Claim 6 (depends on 2)

The remaining service life evaluation method according to claim 2, wherein the steel strip is made of the same metal material as that of the metal pipe.

### Claim 7 (depends on 3)

The remaining service life evaluation method according to claim 3, wherein the steel strip is made of the same metal material as that of the metal pipe.

### Claim 8 (depends on 5)

The remaining service life evaluation method according to claim 5, wherein the steel strip is made of the same metal material as that of the metal pipe.