# US 2016/0258077 A1 · Copper electroplating method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0258077 A1
- Document ID: US20160258077A1
- Status: Published application
- Kind: A1
- Application number: 15/031,317
- Filed: 2014-10-09
- Published: 2016-09-08
- Earliest claimed: 2013-10-22
- Assignees: Atotech Deutschland GmbH
- Applicants: Atotech Deutschland GmbH
- Inventors: Andreas MACIOßEK; Olivier MANN; Pamela CEBULLA
- Web page: https://patentgrep.com/patent/US20160258077A1

## CPC

- C25D 5/18: Electroplating using modulated, pulsed or reversing current
- C25D 3/38: of copper
- C25D 5/02: Electroplating of selected surface areas
- C25D 5/022: {using masking means}
- C25D 5/56: of plastics
- C25D 7/123: {Semiconductors first coated with a seed layer or a conductive layer}
- C25D 17/001: {Apparatus specially adapted for electrolytic coating of wafers, e.g. semiconductors or solar cells}
- C25D 17/10: Electrodes {, e.g. composition, counter electrode}
- C25D 21/18: of electrolytes (C25D21/22 takes precedence)
- H05K 2201/09509: Blind vias, i.e. vias having one side closed
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

The method for copper electroplating according to the present invention comprises an aqueous acidic copper plating bath containing a leveler additive which forms copper trenches having a cross-sectional round shape under direct current plating conditions, and at least one reverse current pulse cycle consisting of one forward current pulse and one reverse current pulse wherein the fraction of the reverse charge to the forward charge applied to the substrate in said at least one current pulse cycle ranges between 0.1 to 5%. The method is particularly suitable for simultaneously filling blind micro vias and plating trenches with a rectangular cross-sectional shape.

## Claims

### Claim 1

A method for copper electroplating comprising, in this order, the steps of
(i) providing a substrate comprising blind micro vias and a patterned resist layer having openings for trench formation and an aqueous acidic copper electrolyte comprising a leveler additive wherein the leveler additive is selected from the group consisting of ureylene polymers, aminocarboxylic acids functionalized with polyalkylene glycol residues, aminocarboxylic acids functionalized with polyalkylene imine residues, aminocarboxylic acids functionalized with polyvinyl alcohol residues, peptides functionalized with polyalkylene glycol residues, peptides functionalized with polyalkylene imine residues and peptides functionalized with polyvinyl alcohol residues,
(ii) operating said substrate as a cathode which is in contact with at least one anode and contacting said substrate with said aqueous acidic copper electrolyte, and,
(iii) applying to the substrate an electrical current, comprising at least one current pulse cycle consisting of one forward current pulse and one reverse current pulse and wherein the fraction of reverse charge to the forward charge applied to said substrate in said at least one current pulse cycle ranges from 0.1 to 5%,
wherein
the duration of the forward current pulse in said at least one current pulse cycle ranges from 10 to 1000 ms,
the duration of the reverse current pulse in said at least one current pulse cycle ranges from 0.05 to 1 ms, and
the current density of the reverse current pulse in said at least one current cycle ranges from 20 to 100 A/dm2,
wherein the applying fills the blind micro vias with copper and forms copper trenches having a rectangular cross-sectional shape.

### Claim 2 (depends on 1)

The method for copper electroplating according to claim 1 wherein the fraction of the reverse charge to the forward charge applied to the substrate in said at least one current pulse cycle ranges from 0.5 to 4%.

### Claim 3 (depends on 1)

The method for copper electroplating according to claim 1 wherein the fraction of the reverse charge to the forward charge applied to the substrate in said at least one current pulse cycle ranges from 1 to 3%.

### Claim 4 (depends on 1)

The method for copper electroplating according to claim 1 wherein the at least one anode is an inert anode.

### Claim 5 (depends on 1)

The method for copper electroplating according to claim 1 wherein the aqueous acidic copper electrolyte further comprises a metal ion redox system.

### Claim 6 (depends on 5)

The method for copper electroplating according to claim 5 wherein the metal ion redox system consists of ferrous and ferric ions.

### Claim 7 (depends on 6)

The method for copper electroplating according to claim 6 wherein the concentration of ferric ions ranges from 0.1 to 4.0 g/l.

### Claim 8 (depends on 5)

The method for copper electroplating according to claim 5 wherein the at least one anode is an inert anode.

### Claim 9

(canceled)

### Claim 10 (depends on 1)

The method for copper electroplating according to claim 1 wherein the concentration of the leveler additive ranges from 0.01 to 200 mg/l.

### Claim 11

(canceled)

### Claim 12 (depends on 1)

The method for copper electroplating according to claim 1 wherein the current density of the forward current pulse in said at least one current pulse cycle ranges from 0.5 to 10 A/dm2.

### Claim 13

(canceled)

### Claim 14

(canceled)

### Claim 15 (depends on 2)

The method for copper electroplating according to claim 2 wherein the fraction of the reverse charge to the forward charge applied to the substrate in said at least one current pulse cycle ranges from 1 to 3%.

### Claim 16 (depends on 6)

The method for copper electroplating according to claim 6 wherein the at least one anode is an inert anode.

### Claim 17 (depends on 7)

The method for copper electroplating according to claim 7 wherein the at least one anode is an inert anode.

### Claim 18 (depends on 2)

The method for copper electroplating according to claim 2 wherein the aqueous acidic copper electrolyte further comprises a metal ion redox system.

### Claim 19 (depends on 3)

The method for copper electroplating according to claim 3 wherein the aqueous acidic copper electrolyte further comprises a metal ion redox system.

### Claim 20 (depends on 4)

The method for copper electroplating according to claim 4 wherein the aqueous acidic copper electrolyte further comprises a metal ion redox system.