# US 2016/0258041 A1 · Die-castable nickel based superalloy composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0258041 A1
- Document ID: US20160258041A1
- Status: Published application
- Kind: A1
- Application number: 14/822,066
- Filed: 2015-08-10
- Published: 2016-09-08
- Earliest claimed: 2014-08-11
- Assignees: United Technologies Corporation
- Applicants: United Technologies Corporation
- Inventors: Awadh B. Pandey
- Web page: https://patentgrep.com/patent/US20160258041A1

## CPC

- C22C 19/055: {with the maximum Cr content being at least 20% but less than 30%}
- B22D 21/005: {with high melting point, e.g. Be 1280 degrees C, Ti 1725 degrees C}
- B22D 25/02: by its peculiarity of shape; of works of art {(cylinders, pistons B22D15/02)}
- C22C 19/03: based on nickel
- C22C 19/056: {with the maximum Cr content being at least 10% but less than 20%}
- F01D 5/28: Selecting particular materials; {Particular measures relating thereto;} Measures against erosion or corrosion
- F05D 2220/32: in gas turbines
- F05D 2230/21: by casting
- F05D 2240/30: Characteristics of rotor blades, i.e. of any element transforming dynamic fluid energy to or from rotational energy and being attached to a rotor
- F05D 2260/221: Improvement of heat transfer
- F05D 2300/175: Superalloys
- F05D 2300/177: Ni - Si alloys
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS

## Abstract

A die-cast nickel based superalloy including 3-7 wt % Tungsten (W), 3-7 wt % Tantalum (Ta), and 0.5-3.0 wt % Aluminum (Al).

## Claims

### Claim 1

A die-cast nickel based superalloy comprising:
3-7 wt % Tungsten (W), 3-7 wt % Tantalum (Ta), and 0.5-3.0 wt % Aluminum (Al).

### Claim 2 (depends on 1)

The die-cast nickel based superalloy as recited in claim 1, wherein said 3-7 wt % Tungsten (W) includes 4.5-5.5 wt % Tungsten (W).

### Claim 3 (depends on 1)

The die-cast nickel based superalloy as recited in claim 1, wherein said 4.5-5.5 wt % Tantalum (Ta) includes 3-7 wt % Tantalum (Ta).

### Claim 4 (depends on 1)

The die-cast nickel based superalloy as recited in claim 1, further comprising: 0.15-0.2 wt % Carbon (C).

### Claim 5 (depends on 1)

The die-cast nickel based superalloy as recited in claim 1, further comprising: 8.0-11.0 wt % Chromium (Cr).

### Claim 6 (depends on 1)

The die-cast nickel based superalloy as recited in claim 1, further comprising: 13.0-17.0 wt % Cobalt (Co).

### Claim 7 (depends on 1)

The die-cast nickel based superalloy as recited in claim 1, further comprising: 2.0-4.0 wt % Molybdenum (Mo)

### Claim 8 (depends on 1)

The die-cast nickel based superalloy as recited in claim 1, further comprising: 3.0-5.0 wt % Titanium (Ti).

### Claim 9 (depends on 1)

The die-cast nickel based superalloy as recited in claim 1, further comprising: 0.15-0.2 wt % Carbon (C), 0-0.2 wt % Manganese (Mn), 0-0.2 wt % Silicon (Si), 0-0.015 wt % Phosphorus (P), 0-0.015 wt % Sulfur (S), 8.0-11.0 wt % Chromium (Cr), 13.0-17.0 wt % Cobalt (Co), 2.0-4.0 wt % Molybdenum (Mo), 3.0-5.0 wt % Titanium (Ti), 0.01-0.02 wt % Boron (B), 0.7-1.2 wt % Vanadium (V), 0.03-0.09 Zirconium (Zr), 0-0.30 wt % Iron (Fe), and the balance Nickel (Ni) plus incidental impurities.

### Claim 10 (depends on 1)

The die-cast nickel based superalloy as recited in claim 1, further comprising: 0.15-0.2 wt % Carbon (C), 0-0.2 wt % Manganese (Mn), 0-0.2 wt % Silicon (Si), 0-0.015 wt % Phosphorus (P), 0-0.015 wt % Sulfur (S), 8.0-11.0 wt % Chromium (Cr), 13.0-17.0 wt % Cobalt (Co), 2.0-4.0 wt % Molybdenum (Mo), 3.0-5.0 wt % Titanium (Ti), 0.01-0.02 wt % Boron (B), 0.7-1.2 wt % Vanadium (V), 0.03-0.09 Zirconium (Zr), 0-0.30 wt % Iron (Fe), 0-0.00003 wt % Bismuth (Bi), 0-0.0005 wt % Lead (Pb), 0-0.00005 wt % Selenium (Se), 0-0.00005 wt % Tellurium (Te), 0-0.00005 wt % Thallium (Tl) and the balance Nickel (Ni) plus incidental impurities.

### Claim 11 (depends on 1)

A gas turbine engine component comprising a die-cast nickel based superalloy as claimed in claim 1.

### Claim 12 (depends on 1)

A gas turbine engine rotor blade comprising a die-cast nickel based superalloy as claimed in claim 1.

### Claim 13 (depends on 1)

A gas turbine engine component comprising a die-cast nickel based superalloy as claimed in claim 1, said die-cast nickel based superalloy die cast at a cooling rate on the order of at least equal 10̂2 degree F. per second.

### Claim 14 (depends on 13)

The die-cast nickel based superalloy as recited in claim 13, wherein an average gran size that is ASTM 3 or smaller.

### Claim 15 (depends on 13)

The die-cast nickel based superalloy as recited in claim 13, wherein a degree of elemental segregation is lower than investment casting.

### Claim 16

A nickel based superalloy consisting of: 0.15-0.2 wt % Carbon (C), 0-0.2 wt % Manganese (Mn), 0-0.2 wt % Silicon (Si), 0-0.015 wt % Phosphorus (P), 0-0.015 wt % Sulfur (S), 8.0-11.0 wt % Chromium (Cr), 13.0-17.0 wt % Cobalt (Co), 2.0-4.0 wt % Molybdenum (Mo), 4.5-5.5 wt % Tungsten (W), 4.5-5.5 wt % Tantalum (Ta), 0.5-3.0 wt % Aluminum (Al), 3.0-5.0 wt % Titanium (Ti), 0.01-0.02 wt % Boron (B), 0.7-1.2 wt % Vanadium (V), 0.03-0.09 Zirconium (Zr), 0-0.30 wt % Iron (Fe), 0-0.00003 wt % Bismuth (Bi), 0-0.0005 wt % Lead (Pb), 0-0.00005 wt % Selenium (Se), 0-0.00005 wt % Tellurium (Te), 0-0.00005 wt % Thallium (Tl) and the balance Nickel (Ni) plus incidental impurities.

### Claim 17 (depends on 14)

A gas turbine engine rotor blade comprising a nickel based superalloy as claimed in claim 14.

### Claim 18 (depends on 8)

A gas turbine engine rotor blade comprising a die-cast nickel based superalloy as claimed in claim 8, said die-cast nickel based superalloy die cast at a cooling rate on the order of at least equal 10̂2 degree F. per second.

### Claim 19

A gas turbine engine rotor blade, comprising:
a die cast nickel based superalloy including a 0.15-0.2 wt % Carbon (C), 0-0.2 wt % Manganese (Mn), 0-0.2 wt % Silicon (Si), 0-0.015 wt % Phosphorus (P), 0-0.015 wt % Sulfur (S), 8.0-11.0 wt % Chromium (Cr), 13.0-17.0 wt % Cobalt (Co), 2.0-4.0 wt % Molybdenum (Mo), 4.5-5.5 wt % Tungsten (W), 4.5-5.5 wt % Tantalum (Ta), 0.5-3.0 wt % Aluminum (Al), 3.0-5.0 wt % Titanium (Ti), 0.01-0.02 wt % Boron (B), 0.7-1.2 wt % Vanadium (V), 0.03-0.09 Zirconium (Zr), 0-0.30 wt % Iron (Fe), 0-0.00003 wt % Bismuth (Bi), 0-0.0005 wt % Lead (Pb), 0-0.00005 wt % Selenium (Se), 0-0.00005 wt % Tellurium (Te), 0-0.00005 wt % Thallium (Tl) and the balance Nickel (Ni) plus incidental impurities.

### Claim 20 (depends on 19)

A gas turbine engine rotor blade as recited in claim 19, said die-cast nickel based superalloy die cast at a cooling rate on the order of at least equal 10̂2 degree F. per second.