# US 2016/0258040 A1 · Titanium alloy, parts made thereof and method of use

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0258040 A1
- Document ID: US20160258040A1
- Status: Published application
- Kind: A1
- Application number: 14/647,622
- Filed: 2015-04-28
- Published: 2016-09-08
- Earliest claimed: 2014-04-28
- Assignees: RTI International Metals, Inc.
- Applicants: Rti International Metals, Inc.
- Inventors: Ronald W. Schutz; Birendra C. Jena
- Web page: https://patentgrep.com/patent/US20160258040A1

## CPC

- C22C 14/00: Alloys based on titanium
- E21B 17/00: Drilling rods or pipes; Flexible drill strings; Kellies; Drill collars; Sucker rods; {Cables;} Casings; Tubings
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS

## Abstract

A titanium alloy, components formed thereof, and methods of use are provided. Embodiments of the alloy may be useful in the energy extraction environment. Components formed of the alloy may include subsea or land-based components associated with oil and gas production and drilling.

## Claims

### Claim 1

A titanium alloy consisting essentially of:
aluminum from 5.0 to 6.0% by weight;
zirconium from 3.75 to 4.75% by weight;
vanadium from 5.2 to 6.2% by weight;
molybdenum from 1.0 to 1.7% by weight;
one of palladium from 0.04 to 0.20% by weight and ruthenium from 0.06 to 0.20% by weight; and
a titanium remainder balance.

### Claim 2 (depends on 1)

The titanium alloy of claim 1 wherein the titanium alloy comprises by weight no more than 0.13% oxygen, 0.05% nitrogen, 0.03% carbon, 0.015% hydrogen, 0.015% boron and 0.25% iron;
the titanium alloy has a molybdenum equivalency in a range of 5.0 to 6.0, wherein the molybdenum equivalency=molybdenum weight % in the alloy+(0.67)(vanadium weight % in the alloy)+(2.5)(iron weight % in the alloy);
the titanium alloy has an aluminum equivalency in a range of 6.5 to 7.5, wherein the aluminum equivalency=aluminum weight % in the alloy+(0.33)(tin weight % in the alloy)+(0.17)(zirconium weight % in the alloy)+(10.0)(oxygen weight % in the alloy);
the titanium alloy has a yield strength of at least 125 ksi at room temperature;
the titanium alloy has a fracture toughness at room temperature in air and seawater of at least 50 ksi √in;
the titanium alloy is fully stress corrosion cracking resistant in 25-33% NaCl brine at a temperature of at least 160° F.; and
an after post-weld heat treatment weld of the titanium alloy has a fracture toughness at room temperature in air of at least 50 ksi √in and an elongation at room temperature of at least 4.0%.

### Claim 3 (depends on 1)

The titanium alloy of claim 1 wherein the titanium alloy has a molybdenum equivalency no more than 6.0; wherein the molybdenum equivalency=molybdenum weight % in the alloy+(0.67)(vanadium weight % in the alloy)+(2.5)(iron weight % in the alloy).

### Claim 4 (depends on 3)

The titanium alloy of claim 3 wherein the molybdenum equivalency is at least 5.0.

### Claim 5 (depends on 4)

The titanium alloy of claim 4 wherein the titanium alloy has an aluminum equivalency no more than 7.5; wherein the aluminum equivalency=aluminum weight % in the alloy+(0.33)(tin weight % in the alloy)+(0.17)(zirconium weight % in the alloy)+(10.0)(oxygen weight % in the alloy).

### Claim 6 (depends on 1)

The titanium alloy of claim 1 wherein the titanium alloy has an aluminum equivalency no more than 7.5; wherein the aluminum equivalency=aluminum weight % in the alloy+(0.33)(tin weight % in the alloy)+(0.17)(zirconium weight % in the alloy)+(10.0)(oxygen weight % in the alloy).

### Claim 7 (depends on 1)

The titanium alloy of claim 1 wherein the titanium alloy comprises by weight no more than 0.13% oxygen, 0.05% nitrogen, 0.03% carbon, 0.015% hydrogen, 0.015% boron and 0.25% iron.

### Claim 8 (depends on 1)

The titanium alloy of claim 1 wherein a total amount of any single element in the titanium alloy other than titanium, aluminum, zirconium, vanadium, molybdenum and the one of palladium and ruthenium is no more than 1.0% by weight.

### Claim 9 (depends on 1)

The titanium alloy of claim 1 wherein the titanium alloy has no local crevice attack after the alloy has been submerged for 60 days in naturally-aerated seawater which has a pH of 3 and is maintained at a temperature of about 500° F. throughout the 60 days.

### Claim 10 (depends on 1)

The titanium alloy of claim 1 wherein the titanium alloy has a yield strength of at least 125 ksi at room temperature and a fracture toughness at room temperature in air and seawater of at least 50 ksi √in.

### Claim 11 (depends on 10)

The titanium alloy of claim 10 wherein an after post-weld heat treatment weld of the titanium alloy has a fracture toughness at room temperature in air of at least 50 ksi √in.

### Claim 12 (depends on 10)

The titanium alloy of claim 10 wherein the titanium alloy has a yield strength of at least 90 ksi at a temperature of 500° F.

### Claim 13 (depends on 10)

The titanium alloy of claim 10 wherein the titanium alloy has a molybdenum equivalency no more than 6.0; wherein the molybdenum equivalency molybdenum weight % in the alloy+(0.67)(vanadium weight % in the alloy)+(2.5)(iron weight % in the alloy); and wherein the titanium alloy has an aluminum equivalency no more than 7.5; wherein the aluminum equivalency aluminum weight % in the alloy+(0.33)(tin weight % in the alloy)+(0.17)(zirconium weight % in the alloy)+(10.0)(oxygen weight % in the alloy).

### Claim 14 (depends on 1)

The titanium alloy of claim 1 wherein an as-welded weld of the titanium alloy has an elongation at room temperature of at least 2.0%.

### Claim 15 (depends on 1)

The titanium alloy of claim 1 wherein a weld of the titanium alloy after post-weld heat treatment has an elongation at room temperature of at least 4.0%.

### Claim 16 (depends on 1)

The titanium alloy of claim 1 wherein the titanium alloy is formed as a tubular component.

### Claim 17 (depends on 1)

The titanium alloy of claim 1 wherein the titanium alloy is formed as a component which comprises at least a portion of one of an offshore pipe, a subsea flow line, a drill pipe, an offshore riser, an oil country tubular goods (OCTG) production tubular, an OCTG well casing, an offshore landing string, an offshore well-workover string and downhole equipment.

### Claim 18 (depends on 1)

The titanium alloy of claim 1 wherein the titanium alloy is formed as a component having an operational position in which the component in contact with aqueous chloride media.

### Claim 19 (depends on 1)

The titanium alloy of claim 1 wherein the titanium alloy is formed as a component having an operational position in which the component is under a pressure of at least 1,200 psi.

### Claim 20

A method comprising the steps of:
providing a component formed of a titanium alloy consisting essentially of, by weight, 5.0 to 6.0% aluminum, 3.75 to 4.75% zirconium, 5.2 to 6.2% vanadium, 1.0 to 1.7% molybdenum, one of 0.04 to 0.20% palladium and 0.06 to 0.20% ruthenium, and a balance titanium; and
operating or maintaining a production and/or extraction system comprising the component while the component is in contact with aqueous chloride media.