# US 2016/0258035 A1 · Method for producing a hot-formed and quench-hardened motor vehicle component formed by internal high-pressure forming

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0258035 A1
- Document ID: US20160258035A1
- Status: Published application
- Kind: A1
- Application number: 15/059,556
- Filed: 2016-03-03
- Published: 2016-09-08
- Earliest claimed: 2015-03-06
- Assignees: Benteler Automobiltechnik GmbH
- Applicants: BENTELER Automobiltechnik GmbH
- Inventors: Rafael Garcia GOMEZ
- Web page: https://patentgrep.com/patent/US20160258035A1

## CPC

- C21D 9/08: for tubular bodies or pipes
- B21D 26/033: Deforming tubular bodies (corrugating tubes by applying fluid pressure B21D15/03, B21D15/10)
- B21D 53/88: other parts for vehicles, e.g. cowlings, mudguards
- B23K 26/262: of longitudinal seams of tubes
- B23K 31/027: {Making tubes by soldering or welding}
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 1/56: characterised by the quenching agents
- C21D 8/10: during manufacturing of tubular bodies
- B23K 2101/006: {Vehicles}
- B23K 2101/045: {Hollow panels}
- B23K 2101/18: Sheet panels
- B23K 2103/04: Steel {or steel} alloys
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B21D: WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS OR PROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL; PUNCHING METAL (working or processing of wire B21F)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

The present invention relates to a method for producing a hot-formed and quench-hardened tubular motor vehicle component (7) by way of internal high-pressure forming, a metallic starting material being at least partially heated to a heating temperature, in particular to a temperature above Ac3, being subjected to internal high-pressure forming in the hot state, and subsequently being quenched, preferably quench-hardened, wherein the internal high-pressure forming is performed as high-speed forming in a time of between 1 and 30 seconds, and the still-hot, formed motor vehicle component (7) is transferred into at least one separate quenching tool (5, 10) and is in particular quench-hardened, the motor vehicle component (7) being braced in a fixed position in the quenching tool (5, 10) and the cycle time of the quenching tool (5,10) corresponding to the cycle time of the internal high-pressure forming.

## Claims

### Claim 1

A method for producing a hot-formed and quench-hardened tubular motor vehicle component by way of internal high-pressure forming, a metallic starting material being at least partially heated to a heating temperature, in particular to a temperature above Ac3, being subjected to internal high-pressure forming in the hot state, and subsequently being quenched, preferably quench-hardened, wherein the internal high-pressure forming is performed as high-speed forming during a time of between 1 and 30 seconds, and the still-hot, formed motor vehicle component is transferred into at least one separate quenching tool and is in particular quench-hardened, the motor vehicle component being braced in a fixed position in the quenching tool and the cycle time of the quenching tool corresponding to the cycle time of the internal high-pressure forming.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the motor vehicle component is quenched in two successive stages, and for this purpose, is transferred initially into a first quenching tool and subsequently into a second quenching tool, each quenching tool -operating with the cycle time of the internal high-pressure forming.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the internal high-pressure forming is performed during a time of between 2 and 15 seconds.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the quenching is performed in a dip bath, and/or wherein the quenching is performed by way of spray cooling and/or injection cooling.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the positive fixing in position in each quenching tool is performed by way of a holding device, the geometric dimension of the holding device having an undersize in relation to the component dimension before the quenching process.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein the internal high-pressure forming tool is cooled and heated, the temperature in the component, being set to between martensite start temperature and Ac3.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the means for fixing in position is in the form of readjustable clamping jaws, and, during the quenching process, the clamping jaws are readjusted in accordance with the shrinkage of the motor vehicle component.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein nozzles of a spray cooling means and/or injection cooling means perform rotating and/or pulsed spraying; such that the motor vehicle component is cooled homogeneously.

### Claim 9 (depends on 1)

The method as claimed in claim 1, wherein a motor vehicle pillar is produced.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein an expected shrinkage curve of the motor vehicle component is calculated or determined experimentally, and the clamping jaws are readjusted in a manner dependent on the shrinkage curve.

### Claim 11 (depends on 1)

The method as claimed in claim 1, wherein linear or punctiform contact against the surface of the produced motor vehicle component is generated by way of the clamping jaws.

### Claim 12 (depends on 1)

The method as claimed in claim 1, wherein a segmented internal high-pressure forming tool with multiple mold segments is used for the hot-forming process, and mold segments are slidingly feedable in particular in a longitudinal direction of the motor vehicle component.

### Claim 13 (depends on 1)

The method as claimed in claim 1, wherein the motor vehicle component is temperature-controlled during the internal high-pressure forming such that, after removal from the internal high-pressure forming tool, said motor vehicle component has a component temperature which, in the quenching tool effects complete quench hardening by microstructure transformation.

### Claim 14

A method for producing a hollow elongate shaped component from a steel material, in particular a motor vehicle pillar, characterized by the following method steps:
providing two sheet-metal blanks, composed in particular of a pre-coated, hardenable steel alloy,
pre-bending at least one sheet-metal blank at a longitudinal edge such that in each case one longitudinal edge of one sheet metal blank is placed in butting contact with the longitudinal edge of the second sheet-metal blank, and an at least partially open hollow profile is provided, in particular a closed hollow profile
thermally joining the longitudinal edges that are in butting contact with one another, in particular by longitudinal seam welding,
performing internal high-pressure forming of the hollow profile.

### Claim 15 (depends on 14)

The method as claimed in claim 14, wherein the hollow profile is austenized before the internal high-pressure forming, and in particular, the pre-coating is fully alloyed.

### Claim 16 (depends on 15)

The method as claimed in claim 15, wherein the internal high-pressure forming is performed in the hot state of the hollow profile, and the component that has been formed by internal high-pressure forming is quench-hardened.

### Claim 17 (depends on 14)

The method as claimed in claim 14, wherein, on the side situated opposite the longitudinally seam-welded side, there is formed a flange region; in particular, in each case one side of the sheet-metal blank is formed as a flange, which flanges overlap in the flange region.

### Claim 18 (depends on 17)

The method as claimed in claim 17, wherein, during the internal high-pressure forming, an enlargement of the cross section at least in sections takes place, with a shortening of at least one flange and/or, by way of ironing of the material, with a reduction in the wall thickness.

### Claim 19 (depends on 14)

The method as claimed in claim 14, wherein the internal high-pressure forming is performed in accordance with a method for producing a hot-formed and quench-hardened tubular motor vehicle component by way of internal high-pressure forming, a metallic starting material being at least partially heated to a heating temperature, in particular to a temperature above Ac3, being subjected to internal high-pressure forming in the hot state, and subsequently being quenched, preferably quench-hardened, wherein the internal high-pressure forming is performed as high-speed forming during a time of between 1 and 30 seconds, and the still-hot, formed motor vehicle component is transferred into at least one separate quenching tool and, is in particular quench-hardened, the motor vehicle component being braced in a fixed position in the quenching tool and the cycle time of the quenching tool corresponding to the cycle time of the internal high-pressure forming.

### Claim 20

A motor vehicle pillar formed from a closed hollow profile with a cross section which varies over its longitudinal extent, the motor vehicle pillar being hot-formed and hardened and having a coating, wherein the hollow profile is formed from two sheet-metal blanks which are connected by way of a longitudinal weld seam which runs so as to be oriented in the direction of longitudinal extent, with two flanges, which protrude in an outwardly oriented direction and which at least partially overlap, being formed in the region of that side of the hollow profile which is situated opposite the longitudinal weld seam.

### Claim 21 (depends on 20)

The motor vehicle pillar as claimed in claim 20, wherein it is produced in accordance with a method for producing a hot-formed and quench-hardened tubular motor vehicle component by way of internal high-pressure forming a metallic starting material being at least partially heated to a heating temperature, in particular to a temperature above Ac3, being subjected to internal high-pressure forming in the hot state, and subsequently being quenched, preferably quench-hardened, wherein the internal high-pressure forming is performed as high-speed forming during a time of between 1 and 30 seconds, and the still-hot, formed motor vehicle component is transferred into at least one separate quenching tool and is in particular quench-hardened, the motor vehicle component being braced in a fixed position in the quenching tool and the cycle time of the quenching tool corresponding to the cycle time of the internal high-pressure forming.

### Claim 22 (depends on 20)

The motor vehicle pillar as claimed in claim 20, wherein it is produced in accordance with a method for producing a hollow elongate shaped component from a steel material, in particular a motor vehicle pillar, wherein the following method steps:
providing two sheet-metal blanks, composed in particular of a pre-coated, hardenable steel alloy,
pre-bending at least one sheet-metal blank at a longitudinal edge such that in each case one longitudinal edge of one sheet metal blank is placed in butting contact with, the longitudinal edge of the second sheet-metal blank, and an at least partially open hollow profile is provided, in particular a closed hollow profile,
thermally joining the longitudinal edges that are in butting contact with one another, in particular by longitudinal seam welding,
performing internal high-pressure forming of the hollow profile.