# US 2016/0258032 A1 · High-strength hot-rolled steel sheet and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0258032 A1
- Document ID: US20160258032A1
- Status: Published application
- Kind: A1
- Application number: 15/143,965
- Filed: 2016-05-02
- Published: 2016-09-08
- Earliest claimed: 2013-04-15
- Assignees: Jfe Steel Corporation
- Applicants: JFE Steel Corporation
- Inventors: Katsumi Nakajima; Kazuhiko Yamazaki; Chikara Kami
- Web page: https://patentgrep.com/patent/US20160258032A1

## CPC

- C21D 1/20: Isothermal quenching, e.g. bainitic hardening
- B21D 22/022: {by heating the blank or stamping associated with heat treatment (C21D takes precedence)}
- B32B 15/013: {one layer being formed of an iron alloy or steel, another layer being formed of a metal other than iron or aluminium}
- C21D 1/28: Normalising
- C21D 1/84: Controlled slow cooling (cooling-beds for metal rolling B21B43/00)
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0263: {following hot rolling}
- C21D 8/0426: {Hot rolling}
- C21D 8/0463: {following hot rolling}
- C21D 9/46: for sheet metals
- C21D 9/48: deep-drawing sheets
- C22C 18/04: with aluminium as the next major constituent
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C23C 2/022: {by heating}
- C23C 2/024: {by cleaning or etching}
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C23C 2/40: Plates; Strips
- C23F 17/00: Multi-step processes for surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by subclass C21D or C22F or class C25 (coating for obtaining at least two superposed coatings either by methods not provided for in a single one of main groups C23C2/00 - C23C26/00, or by combinations of methods providedfor in subclasses C23C and C25D, C23C28/00)
- C21D 6/004: {containing Cr and Ni}
- C21D 2211/002: Bainite
- C21D 2211/003: Cementite
- C22C 38/16: containing copper
- C22C 38/18: containing chromium
- C22C 38/24: with vanadium
- C22C 38/28: with titanium or zirconium
- C22C 38/32: with boron
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/54: with boron
- C22C 38/58: with more than 1.5% by weight of manganese
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B21D: WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS OR PROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL; PUNCHING METAL (working or processing of wire B21F)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25

## Abstract

A steel slab having a composition containing C: more than 0.07% and 0.2% or less, Si: 2.0% or less, Mn: 1.0% to 3.0%, Al: 0.1% or less, Ti: 0.05% to 0.3%, and V: 0.05% to 0.3% on a mass percent basis is heated to 1100° C. or more and is subjected to rough rolling and finish rolling. In the finish rolling, the total rolling reduction of two final passes is 30% or more, and the finish rolling temperature ranges from (Ar3 transformation temperature) to (Ar3 transformation temperature+120° C.). Cooling is started within 2 seconds after the finish rolling. Coiling is performed at an average cooling rate of 40° C./s or more at a coiling temperature in the range of 300° C. to 500° C. The resulting high-strength hot-rolled steel sheet has a microstructure in which a bainite phase constitutes more than 90% by volume, the average lath interval of bainite is 0.45 μm or less, and the ratio of Fe-based carbide precipitated in bainite lath to all Fe-based carbide is 10% or more, has a high tensile strength of 900 MPa or more, and has significantly improved punchability in mass production.

## Claims

### Claim 1

A high-strength hot-rolled steel sheet having a composition containing, on a mass percent basis,
C: 0.05% to 0.15%, Si: 1.5% or less,
Mn: 1.0% to 2.0%, P: 0.05% or less,
S: 0.005% or less, Al: 0.1% or less,
N: 0.01% or less, Ti: 0.05% to 0.2%, and
the balance being Fe and incidental impurities,
wherein the high-strength hot-rolled steel sheet has a microstructure comprising a bainite of more than 92% by volume, the bainite having an average lath interval of 0.60 μm or less, and Fe-based carbide precipitated in bainite lath grains having a ratio of 10% or more by number to all Fe-based carbide.

### Claim 2 (depends on 1)

The high-strength hot-rolled steel sheet according to claim 1, wherein the composition further contains at least one selected from Nb: 0.005% to 0.2% and B: 0.0002% to 0.0030% on a mass percent basis.

### Claim 3 (depends on 1)

The high-strength hot-rolled steel sheet according to claim 1, wherein the composition further contains at least one selected from Cu: 0.005% to 0.3%, Ni: 0.005% to 0.3%, and Sn: 0.005% to 0.3% on a mass percent basis.

### Claim 4 (depends on 2)

The high-strength hot-rolled steel sheet according to claim 2, wherein the composition further contains at least one selected from Cu: 0.005% to 0.3%, Ni: 0.005% to 0.3%, and Sn: 0.005% to 0.3% on a mass percent basis.

### Claim 5 (depends on 1)

The high-strength hot-rolled steel sheet according to claim 1, wherein the composition further contains at least one selected from Mo: 0.002% to 0.3% and Cr: 0.002% to 0.3% on a mass percent basis.

### Claim 6 (depends on 2)

The high-strength hot-rolled steel sheet according to claim 2, wherein the composition further contains at least one selected from Mo: 0.002% to 0.3% and Cr: 0.002% to 0.3% on a mass percent basis.

### Claim 7 (depends on 3)

The high-strength hot-rolled steel sheet according to claim 3, wherein the composition further contains at least one selected from Mo: 0.002% to 0.3% and Cr: 0.002% to 0.3% on a mass percent basis.

### Claim 8 (depends on 4)

The high-strength hot-rolled steel sheet according to claim 4, wherein the composition further contains at least one selected from Mo: 0.002% to 0.3% and Cr: 0.002% to 0.3% on a mass percent basis.

### Claim 9 (depends on 1)

The high-strength hot-rolled steel sheet according to claim 1, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 10 (depends on 2)

The high-strength hot-rolled steel sheet according to claim 2, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 11 (depends on 3)

The high-strength hot-rolled steel sheet according to claim 3, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 12 (depends on 4)

The high-strength hot-rolled steel sheet according to claim 4, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 13 (depends on 5)

The high-strength hot-rolled steel sheet according to claim 5, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 14 (depends on 6)

The high-strength hot-rolled steel sheet according to claim 6, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 15 (depends on 7)

The high-strength hot-rolled steel sheet according to claim 7, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 16 (depends on 8)

The high-strength hot-rolled steel sheet according to claim 8, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 17 (depends on 1)

A hot-dip galvanized steel sheet, having a hot-dip galvanizing layer or alloyed hot-dip galvanizing layer on a surface of the high-strength hot-rolled steel sheet according to claim 1.

### Claim 18

A method for producing a high-strength hot-rolled steel sheet, comprising:
heating a steel slab and subjecting the steel slab to hot rolling having rough rolling and finish rolling to form a hot-rolled steel sheet,
wherein the steel slab contains, on a mass percent basis,
C: 0.05% to 0.15%, Si: 1.5% or less,
Mn: 1.0% to 2.0%, P: 0.05% or less,
S: 0.005% or less, Al: 0.1% or less,
N: 0.01% or less, Ti: 0.05% to 0.2%, and
the balance being Fe and incidental impurities,
wherein the hot rolling includes heating the steel slab to 1100° C. or more, a total rolling reduction of two final passes in the finish rolling being 30% or more, a finish-rolling finishing temperature being in a range of (Ar3 transformation temperature) to (Ar3 transformation temperature+120° C.), starting cooling within 2 seconds after the finish rolling, cooling the hot-rolled steel sheet to a coiling temperature at an average cooling rate of 50° C./s or more, and coiling the hot-rolled steel sheet at a coiling temperature: 300° C. to 500° C.

### Claim 19 (depends on 18)

The method for producing a high-strength hot-rolled steel sheet according to claim 18, wherein the composition further contains at least one from Nb: 0.005% to 0.2% and B: 0.0002% to 0.0030% on a mass percent basis.

### Claim 20 (depends on 18)

The method for producing a high-strength hot-rolled steel sheet according to claim 18, wherein the composition further contains at least one selected from Cu: 0.005% to 0.3%, Ni: 0.005% to 0.3%, and Sn: 0.005% to 0.3% on a mass percent basis.

### Claim 21 (depends on 19)

The method for producing a high-strength hot-rolled steel sheet according to claim 19, wherein the composition further contains at least one selected from Cu: 0.005% to 0.3%, Ni: 0.005% to 0.3%, and Sn: 0.005% to 0.3% on a mass percent basis.

### Claim 22 (depends on 18)

The method for producing a high-strength hot-rolled steel sheet according to claim 18, wherein the composition further contains at least one selected from Mo: 0.002% to 0.3% and Cr: 0.002% to 0.3% on a mass percent basis.

### Claim 23 (depends on 19)

The method for producing a high-strength hot-rolled steel sheet according to claim 19, wherein the composition further contains at least one selected from Mo: 0.002% to 0.3% and Cr: 0.002% to 0.3% on a mass percent basis.

### Claim 24 (depends on 20)

The method for producing a high-strength hot-rolled steel sheet according to claim 20, wherein the composition further contains at least one selected from Mo: 0.002% to 0.3% and Cr: 0.002% to 0.3% on a mass percent basis.

### Claim 25 (depends on 21)

The method for producing a high-strength hot-rolled steel sheet according to claim 21, wherein the composition further contains at least one selected from Mo: 0.002% to 0.3% and Cr: 0.002% to 0.3% on a mass percent basis.

### Claim 26 (depends on 18)

The method for producing a high-strength hot-rolled steel sheet according to claim 18, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 27 (depends on 19)

The method for producing a high-strength hot-rolled steel sheet according to claim 19, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 28 (depends on 20)

The method for producing a high-strength hot-rolled steel sheet according to claim 20, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 29 (depends on 21)

The method for producing a high-strength hot-rolled steel sheet according to claim 21, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 30 (depends on 22)

The method for producing a high-strength hot-rolled steel sheet according to claim 22, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 31 (depends on 23)

The method for producing a high-strength hot-rolled steel sheet according to claim 23, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 32 (depends on 24)

The method for producing a high-strength hot-rolled steel sheet according to claim 24, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 33 (depends on 25)

The method for producing a high-strength hot-rolled steel sheet according to claim 25, wherein the composition further contains at least one selected from Ca: 0.0002% to 0.004% and REM: 0.0002% to 0.004% on a mass percent basis.

### Claim 34 (depends on 18)

A method for producing a hot-dip galvanized steel sheet, comprising:
pickling a high-strength hot-rolled steel sheet produced by the method for producing a high-strength hot-rolled steel sheet according to claim 18, and subjecting the high-strength hot-rolled steel sheet to annealing and plating treatment to form a coated steel sheet having a coated layer on a surface thereof,
wherein the annealing is performed at a soaking temperature of 730° C. or less, and the plating treatment after the annealing includes passing the high-strength hot-rolled steel sheet through a hot-dip galvanizing bath to form a hot-dip galvanizing layer on a surface of the hot-rolled steel sheet and optionally subjecting the high-strength hot-rolled steel sheet to alloying treatment for alloying the hot-dip galvanizing layer.