# US 2016/0257810 A1 · Modified heterophasic polyolefin composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0257810 A1
- Document ID: US20160257810A1
- Status: Published application
- Kind: A1
- Application number: 15/062,004
- Filed: 2016-03-04
- Published: 2016-09-08
- Earliest claimed: 2015-03-05
- Assignees: Milliken & Company
- Applicants: Milliken & Company
- Inventors: Joseph J. Peterson; Daike Wang; Jason D. Sprinkle; Scott R. Trenor; Suchitra Datta; Adam J. Sobczak
- Web page: https://patentgrep.com/patent/US20160257810A1

## CPC

- C08L 23/36: by reaction with nitrogen-containing compounds, e.g. by nitration
- C08K 5/005: {Stabilisers against oxidation, heat, light, ozone}
- C08K 5/14: Peroxides
- C08L 23/10: Homopolymers or copolymers of propene
- C08L 23/12: Polypropene
- C08L 23/16: Ethylene-propylene or ethylene-propylene-diene copolymers
- C08L 23/26: modified by chemical after-treatment (saponified copolymers C08L23/0861; unsaturated acid salts C08L23/0876)
- C08L 23/28: by reaction with halogens or halogen-containing compounds (C08L23/32 takes precedence)
- C08L 2205/08: containing additives to improve the compatibility between two polymers
- C08L 2207/02: Heterophasic composition
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A heterophasic polymer composition comprises a propylene polymer phase, an ethylene polymer phase, and a compatibilizing agent. The compatibilizing agent comprises (i) at least one tertiary carbon-hydrogen bond having a bond-dissociation energy of about 380 kJ/mol or less and (ii) at least one acyclic carbon-carbon double bond. A method of making a heterophasic polyolefin polymer composition comprises the steps of (a) providing a propylene polymer phase and an ethylene polymer phase, (b) providing a compatibilizing agent, and (c) mixing the propylene polymer phase, the ethylene polymer phase and the compatibilizing agent, in the presence of free carbon radicals. The compatibilizing agent reacts with propylene polymers and ethylene polymers thereby bonding propylene polymers to ethylene polymers.

## Claims

### Claim 1

A heterophasic polymer composition comprising:
(a) a propylene polymer phase comprising propylene polymers selected from the group consisting of polypropylene homopolymers and copolymers of propylene and up to 50 wt. % of one or more comonomers selected from the group consisting of ethylene and C4-C10 α-olefin monomers;
(b) an ethylene polymer phase comprising ethylene polymers selected from the group consisting of ethylene homopolymers and copolymers of ethylene and one or more C3-C10 α-olefin monomers; and
(c) a compatibilizing agent, the compatibilizing agent comprising (i) at least one tertiary carbon-hydrogen bond having a bond-dissociation energy of about 380 kJ/mol or less and (ii) at least one acyclic carbon-carbon double bond.

### Claim 2 (depends on 1)

The heterophasic polymer composition of claim 1, wherein the acyclic carbon-carbon double bond has at least two hydrogen atoms bonded to the carbon atoms in the acyclic carbon-carbon double bond.

### Claim 3 (depends on 1)

The heterophasic polymer composition of claim 1, wherein the compatibilizing agent conforms to the structure of Formula (I) below
where R1, R2, and R3 are independently selected from the group consisting of aryl groups, substituted aryl groups, heteroaryl groups, substituted heteroaryl groups, electron withdrawing groups, and groups conforming to the structure of Formula (V), Formula (VI), Formula (VII), or Formula (VIII) below
where X1 is selected from the group consisting of oxygen and —N(H)— and R5 is selected from the group consisting of alkenyl groups, substituted alkenyl groups, substituted aryl groups, and substituted heteroaryl groups, provided the substituted aryl groups and substituted heteroaryl groups comprise at least one alkenyl group or substituted alkenyl group,
where R6 is selected from the group consisting of alkanediyl groups and substituted alkanediyl groups,
where X3 is selected from the group consisting of oxygen, —N(H)—, and —N(R7)—, R7 is selected from the group consisting of alkenyl groups, substituted alkenyl groups, substituted aryl groups, and substituted heteroaryl groups, provided the substituted aryl groups and substituted heteroaryl groups comprise at least one alkenyl group or substituted alkenyl group;
where R8 is selected from the group consisting of alkanediyl groups;
provided: (i) when two or more of R1, R2, and R3 are aromatic groups, two of the groups can be fused by a linking element selected from the group consisting of a direct bond, an oxygen atom, and a sulfur atom; (ii) at least one of R1, R2, and R3 is selected from the group consisting of aryl groups, substituted aryl groups, heteroaryl groups, and substituted heteroaryl groups; and (iii) at least one of R1, R2, and R3 comprises at least one acyclic carbon-carbon double bond.

### Claim 4 (depends on 3)

The heterophasic polymer composition of claim 3, wherein the compatibilizing agent conforms to the structure of Formula (X) below
where R10, R11, and R12 are independently selected from the group consisting of hydrogen, halogens, alkenyl groups, substituted alkenyl groups, groups conforming to the structure of Formula (V), and groups conforming to the structure —O—R15 where R15 is selected from the group consisting of alkenyl groups and substituted alkenyl groups, provided at least one of R10, R11, and R12 comprises at least one acyclic carbon-carbon double bond.

### Claim 5 (depends on 3)

The heterophasic polymer composition of claim 3, wherein the compatibilizing agent conforms to the structure of Formula (XL) below
where R41 is selected from the group consisting of groups conforming to the structure of Formula (V) or Formula (VII).

### Claim 6 (depends on 5)

The heterophasic polymer composition of claim 5, wherein R41 is a group conforming to the structure of Formula (VII), X3 is —N(H)—, and R7 is a substituted aryl group.

### Claim 7 (depends on 6)

The heterophasic polymer composition of claim 6, wherein R7 is a 4-ethenylphenyl group.

### Claim 8 (depends on 5)

The heterophasic polymer composition of claim 5, wherein R41 is a group conforming to the structure of Formula (V), X1 is —N(H)—, and R5 is a substituted alkenyl group.

### Claim 9 (depends on 8)

The heterophasic polymer composition of claim 8, wherein R5 is a 2-phenylethenyl group.

### Claim 10 (depends on 3)

The heterophasic polymer composition of claim 3, wherein the compatibilizing agent conforms to the structure of Formula (L) below
where R51 is selected from the group consisting of a direct bond and oxygen, and R55 is selected from the group consisting of substituted aryl groups, groups conforming to the structure of Formula (V), and groups conforming to the structure of Formula (VI).

### Claim 11 (depends on 10)

The heterophasic polymer composition of claim 10, wherein R51 is a direct bond and R55 is a 4-ethenylphenyl group.

### Claim 12 (depends on 10)

The heterophasic polymer composition of claim 10, wherein R51 is an oxygen and R55 is a 4-ethenylphenyl group.

### Claim 13 (depends on 10)

The heterophasic polymer composition of claim 10, wherein R51 is a direct bond, R55 is a group conforming to the structure of Formula (V), X1 is an oxygen, and R5 is a 1-methylethenyl group.

### Claim 14 (depends on 10)

The heterophasic polymer composition of claim 10, wherein R51 is a direct bond, R55 is a group conforming to the structure of Formula (VIII), R8 is a methanediyl group, X3 is —N(H)—, and R7 is a 4-ethenylphenyl group.

### Claim 15 (depends on 3)

The heterophasic polymer composition of claim 3, wherein R1 is a cyano group, R2 is a phenyl group, and R3 is a 4-ethenylphenyl group.

### Claim 16 (depends on 1)

The heterophasic polymer composition of claim 1, wherein the compatibilizing agent conforms to the structure of Formula (XX)
where X20 is selected from the group consisting of an oxygen and —N(H)—, R20 and R21 are independently selected from the group consisting of hydrogen, C1-C4 alkyl groups, and groups conforming to the structure of Formula (V) below
where X1 is selected from the group consisting of oxygen and —N(H)— and R5 is selected from the group consisting of alkenyl groups, substituted alkenyl groups, substituted aryl groups, and substituted heteroaryl groups, provided the substituted aryl groups and substituted heteroaryl groups comprise at least one alkenyl group or substituted alkenyl group; R22 is selected from the group consisting of aryl groups, substituted aryl groups, heteroaryl groups, and substituted heteroaryl groups; provided at least one of R20, R21, and R22 comprises at least one acyclic carbon-carbon double bond.

### Claim 17 (depends on 1)

The heterophasic polymer composition of claim 1, wherein the compatibilizing agent conforms to the structure of Formula (XXX)
where R30 is selected from the group consisting of substituted aryl groups and substituted heteroaryl groups, provided the substituted aryl groups and substituted heteroaryl groups comprise at least one alkenyl group or substituted alkenyl group.

### Claim 18 (depends on 1)

The heterophasic polymer composition of claim 1, wherein the ethylene polymers are selected from the group consisting of ethylene-propylene elastomers, ethylene-butene elastomers, ethylene-hexene elastomers, ethylene-octene elastomers, and mixtures thereof.

### Claim 19 (depends on 1)

The heterophasic polymer composition of claim 1, wherein the ethylene polymer comprises from 5 to 80 wt. % of the heterophasic polyolefin polymer composition, based on the total weight of propylene polymers and ethylene polymers in the composition.

### Claim 20 (depends on 19)

The heterophasic polymer composition of claim 19, wherein the ethylene polymer comprises about 5 to 60 wt. % of the heterophasic polyolefin polymer composition, based on the total weight of propylene polymers and ethylene polymers in the composition.

### Claim 21 (depends on 1)

The heterophasic polymer composition of claim 1, wherein the propylene content of the propylene polymer phase is 80 wt. % or greater.

### Claim 22 (depends on 1)

The heterophasic polymer composition of claim 1, wherein the ethylene polymer phase is a discontinuous phase in the heterophasic polyolefin polymer composition.

### Claim 23 (depends on 1)

The heterophasic polymer composition of claim 1, wherein the compatibilizing agent is present in the heterophasic polyolefin polymer composition in a concentration of from 10 ppm to 5 wt. %, based on the total weight of the composition.

### Claim 24

A heterophasic polymer composition comprising a continuous phase comprising polypropylene polymers selected from the group consisting of polypropylene homopolymers and copolymers of propylene and up to 80 wt. % of one or more comonomers selected from the group consisting of ethylene and C4-C10 α-olefin monomers and a discontinuous phase comprising elastomeric ethylene copolymers having an ethylene content of from 8 to 90 wt. % selected from the group consisting of copolymers of ethylene and one or more C3-C10 α-olefin monomers, provided that the propylene content of the propylene polymer phase is greater than the propylene content of the ethylene polymer phase, wherein the composition further comprises propylene polymers bonded to ethylene copolymers by a compatibilizing agent, wherein the compatibilizing agent comprises (i) at least one tertiary carbon-hydrogen bond having a bond-dissociation energy of about 380 kJ/mol or less and (ii) at least one acyclic carbon-carbon double bond.

### Claim 25 (depends on 24)

The heterophasic polymer composition of claim 24, wherein the discontinuous phase comprises from 5 to 35 wt. % of the heterophasic polyolefin polymer composition, based on the weight of propylene polymers and ethylene copolymers in the composition.

### Claim 26 (depends on 24)

The heterophasic polymer composition of claim 24, wherein the ethylene copolymer comprising the discontinuous phase has an ethylene content of from 8 to 80 wt. %.

### Claim 27 (depends on 24)

The heterophasic polymer composition of claim 24, wherein the heterophasic polyolefin polymer composition comprises from 5 to 30 wt. % ethylene, based on the total weight of propylene polymers and ethylene copolymers in the composition.

### Claim 28 (depends on 24)

The heterophasic polymer composition of claim 24, wherein the heterophasic polyolefin polymer composition is obtained by operating in at least two polymerization stages.

### Claim 29 (depends on 24)

The heterophasic polymer composition of claim 24, wherein the propylene content of the propylene polymer phase is 80 wt. % or greater.

### Claim 30 (depends on 24)

The heterophasic polymer composition of claim 24, wherein the compatibilizing agent is present in the heterophasic polyolefin polymer composition in a concentration of from 10 ppm to 5 wt. %, based on the total weight of the composition.

### Claim 31

A heterophasic polyolefin polymer composition obtained by the process comprising the steps of:
(a) providing a propylene polymer phase comprising propylene polymers selected from the group consisting of polypropylene homopolymers and copolymers of propylene and up to 50 wt. % of one or more comonomers selected from the group consisting of ethylene and C4-C10 α-olefin monomers and an ethylene polymer phase comprising ethylene polymers selected from the group consisting of ethylene homopolymers and copolymers of ethylene and one or more C3-C10 α-olefin monomers provided that the ethylene content of the ethylene polymer phase is at least 8 wt. %,
(b) providing a compatibilizing agent, wherein the compatibilizing agent comprises (i) at least one tertiary carbon-hydrogen bond having a bond-dissociation energy of about 380 kJ/mol or less and (ii) at least one acyclic carbon-carbon double bond; and
(c) mixing the propylene polymer phase, the ethylene polymer phase and the compatibilizing agent in the presence of free carbon radicals, whereby propylene polymers are bonded to ethylene polymers by the compatibilizing agent, and whereby the propylene polymer phase and the ethylene polymer phase form a heterophasic composition.

### Claim 32 (depends on 31)

The heterophasic polymer composition of claim 31, wherein the propylene polymer phase, the ethylene polymer phase and the compatibilizing agent are mixed in the presence of free carbon radicals by melt compounding, and the composition is heterophasic at 25° C.

### Claim 33 (depends on 31)

The heterophasic polymer composition of claim 31, wherein the propylene polymer phase is the continuous phase and the propylene content of the propylene polymer phase is 80 wt. % or greater, and the ethylene polymer phase is the discontinuous phase and the ethylene polymers have an ethylene content of from 8 to 80 wt. % and are selected from the group consisting of copolymers of ethylene and one or more C3-C10 α-olefin monomers.

### Claim 34

A method of making a heterophasic polyolefin polymer composition, the method comprising the steps of:
(a) providing a propylene polymer phase comprising propylene polymers selected from the group consisting of polypropylene homopolymers and copolymers of propylene and up to 50 wt. % of one or more comonomers selected from the group consisting of ethylene and C4-C10 α-olefin monomers, and an ethylene polymer phase comprising ethylene polymers selected from the group consisting of ethylene homopolymers and copolymers of ethylene and one or more C3-C10 α-olefin monomers provided that the ethylene content of the ethylene polymer phase is at least 8 wt. %,
(b) providing a compatibilizing agent, wherein the compatibilizing agent comprises (i) at least one tertiary carbon-hydrogen bond having a bond-dissociation energy of about 380 kJ/mol or less and (ii) at least one acyclic carbon-carbon double bond; and
(c) mixing the propylene polymer phase, the ethylene polymer phase and the compatibilizing agent, in the presence of free carbon radicals, whereby the compatibilizing agent reacts with propylene polymers and ethylene polymers thereby bonding propylene polymers to ethylene polymers, and whereby the propylene polymer phase and the ethylene polymer phase form a heterophasic composition.

### Claim 35 (depends on 34)

The method of claim 34, wherein the propylene polymer phase, the ethylene polymer phase and the compatibilizing agent are mixed in the presence of free carbon radicals by melt compounding, and the composition is heterophasic at 25° C.

### Claim 36 (depends on 34)

The method of claim 34, wherein the propylene polymer phase is the continuous phase and the propylene content of the propylene polymer phase is 80 wt. % or greater, and the ethylene polymer phase is the discontinuous phase and the ethylene polymers have an ethylene content of from 8 to 80 wt. % and are selected from the group consisting of copolymers of ethylene and one or more C3-C10 α-olefin monomers.

### Claim 37 (depends on 34)

The method of claim 34, wherein the polypropylene phase and the ethylene phase are provided to the mixture as a heterophasic impact copolymer obtained by operating in at least two polymerization stages.

### Claim 38 (depends on 34)

The method of claim 34, wherein the compatibilizing agent is present in the heterophasic polyolefin polymer composition in a concentration of from 10 ppm to 5 wt. %, based on the total weight of the composition, and wherein a reaction between the unsaturated bond of the compatibilizing agent and the ethylene polymer is conducted in the presence of a free radical generator selected from the group consisting of organic peroxides incorporating one or more peroxide bonds, and the compatibilizing agent and the organic peroxide are present in a ratio of moles of compatibilizing agent to molar equivalents of peroxide bonds of 1:10 to 10:1.