# US 2016/0257805 A1 · Coupled Glass-Fiber Reinforced Polyoxymethylene

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0257805 A1
- Document ID: US20160257805A1
- Status: Published application
- Kind: A1
- Application number: 15/087,036
- Filed: 2016-03-31
- Published: 2016-09-08
- Earliest claimed: 2010-10-14
- Assignees: Ticona LLC
- Applicants: Ticona GmbH
- Inventors: Kirsten Markgraf; Lowell Larson
- Web page: https://patentgrep.com/patent/US20160257805A1

## CPC

- C08K 7/14: Glass
- C08G 18/56: Polyacetals
- C08G 18/7671: {containing only one alkylene bisphenyl group}
- C08K 5/29: Compounds containing {one or more} carbon-to-nitrogen double bonds
- C08K 5/34922: {Melamine; Derivatives thereof}
- C08L 59/02: Polyacetals containing polyoxymethylene sequences only
- C08L 61/02: Condensation polymers of aldehydes or ketones only
- C08L 2201/08: Stabilised against heat, light or radiation or oxydation
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present invention relates to a molding composition, a process for the manufacturing of said molding composition, molded parts obtainable therefrom as well as the use of the molding composition for the manufacturing of molded parts used in the automotive industry, for housings, latches, window winding systems, wiper systems, pulleys, sun roof systems, seat adjustments, levers, gears, claws, pivot housing, brackets, wiper arms or seat rails.

## Claims

### Claim 1

A molding composition comprising
a) at least one polyoxymethylene (A) having terminal OH-groups of more than 15 mmol/kg,
b) at least one coupling agent (B) comprising a polyisocyanate,
c) at least one reinforcing fiber (C) and
d) at least one formaldehyde scavenger (D).

### Claim 2 (depends on 1)

The molding composition according to claim 1, wherein at least 25% of the terminal groups of the polyoxymethylene (A) are hydroxyl groups.

### Claim 3 (depends on 1)

The molding composition according to claim 1, wherein the polyoxymethylene (A) comprises at least 50 mol-% —CH2O— repeat units.

### Claim 4 (depends on 1)

The molding composition according to claim 1, wherein polyoxymethylene (A) is present in an amount up to 95 wt.-%, wherein the weight is based on the total weight of the molding composition.

### Claim 5 (depends on 1)

The molding composition according to claim 1, wherein the polyisocyanate is selected from the group consisting of an aliphatic diisocyanate, a cycloaliphatic diisocyanate, an aromatic diisocyanate and mixtures thereof.

### Claim 6 (depends on 1)

The molding composition according to claim 1, wherein the coupling agent (B) is present in an amount ranging from 0.1 to 5 wt.-%, wherein the weight is based on the total weight of the composition.

### Claim 7 (depends on 1)

The molding composition according to claim 1, wherein the formaldehyde scavenger (D) is an aromatic compound.

### Claim 8 (depends on 1)

The molding composition according to claim 1, wherein the formaldehyde scavenger (D) has a melting point higher than 235° C.

### Claim 9 (depends on 1)

The molding composition according to claim 1, wherein the formaldehyde scavenger (D) has a pKa value ranging from 4.5 to 10.

### Claim 10 (depends on 1)

The molding composition according to claim 1, wherein the formaldehyde scavenger (D) has a melting point which is at least 10° C. higher than the melting point of the polyoxymethylene (A).

### Claim 11 (depends on 1)

The molding composition according to claim 1, wherein the formaldehyde scavenger (D) is melamine.

### Claim 12 (depends on 1)

The molding composition according to claim 1, wherein the formaldehyde scavenger (D) is present in the composition in an amount up to 2 wt.-%, wherein the weight is based on the total weight of the composition.

### Claim 13 (depends on 1)

The molding composition according to claim 1, further comprising one or more tribological modifiers.

### Claim 14 (depends on 13)

The molding composition according to claim 13, wherein the tribological modifier is an ultrahigh molecular weight polyethylene having a viscosity number of higher than 1000 ml/g (determined according to ISO 1628, part 3; concentration in decahydronaphthalin: 0.0002 g/ml).

### Claim 15 (depends on 13)

The molding composition according to claim 13, wherein the tribological modifier is an ultrahigh molecular weight polyethylene which has a mean particle diameter D50 ranging from 1 to 5000 μm.

### Claim 16 (depends on 15)

The molding composition according to claim 15, wherein the tribological modifier is an ultrahigh molecular weight polyethylene which is present in the molding composition in an amount up to 30 wt.-%, wherein the weight is based on the total weight of the composition.

### Claim 17 (depends on 1)

The molding composition according to claim 1 wherein the reinforcing fiber (C) is a continuous-filament fiber.

### Claim 18 (depends on 1)

A molded part obtained by molding the molding composition according to claim 1.

### Claim 19

(canceled)

### Claim 20 (depends on 1)

A process for manufacturing a molding composition, the process comprising the following steps:
melt mixing the molding composition according to claim 1
at a temperature ranging from between 120° C. to 260° C.,
wherein the melting point of the formaldehyde scavenger is at least 10° C. higher than the melt mixing temperature.

### Claim 21

A process for manufacturing a long fiber reinforced molding composition comprising
a) impregnating a continuous fiber filament with a polymer matrix comprising
i) at least one polyoxymethylene (A) having terminal OH groups of more than 15 mmol/kg,
ii) at least one coupling agent (B), and
iii) optionally at least one formaldehyde scavenger (D) and/or other additives; and
b) optionally cutting the impregnated fiber filament into pellets.

### Claim 22 (depends on 21)

The process according to claim 21 wherein the polymer matrix is melt mixed prior to the impregnation of the continuous fiber filament.

### Claim 23 (depends on 21)

The process according to claim 21 wherein the continuous fiber filament is part of a roving or yarn.

### Claim 24 (depends on 21)

The process according to claim 21 wherein the polyoxymethylene (A) has a MVR of more than 35 cm3/10 min, determined according to ISO 1133 at 190° C. and 2.16 kg.

### Claim 25 (depends on 21)

The process according to claim 21 wherein the polyoxymethylene (A) has a content of terminal hydroxyl groups of at least 20 mmol/kg.

### Claim 26 (depends on 21)

The process according to claim 21 wherein the molding composition comprises
40 to 90 wt-% of polyoxymethylene (A),
0.1 to 5.0 wt.-% of a coupling agent (B) comprising a polyisocyanate; and
5 to 45 wt.-% of the continuous fiber filament.

### Claim 27 (depends on 21)

The process according to claim 21 which is a pultrusion process.