# US 2016/0257791 A1 · A method for treating lignin and for producing a binder composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0257791 A1
- Document ID: US20160257791A1
- Status: Published application
- Kind: A1
- Application number: 15/033,732
- Filed: 2014-11-25
- Published: 2016-09-08
- Earliest claimed: 2013-11-26
- Assignees: Upm-Kymmene Corporation
- Applicants: Upm-Kymmene Corporation
- Inventors: Suvi PIETARINEN; Sanna VALKONEN; Okko RINGENA
- Web page: https://patentgrep.com/patent/US20160257791A1

## CPC

- C08H 6/00: {Macromolecular compounds derived from lignin, e.g. tannins, humic acids}
- B27N 3/002: {characterised by the type of binder (compositions of macromolecular compounds C08L)}
- C07G 1/00: Low-molecular-weight derivatives of lignin (high-molecular-weight derivatives of lignin {C08H6/00})
- C08K 5/0025: {Crosslinking or vulcanising agents; including accelerators}
- C08K 5/07: Aldehydes; Ketones
- C09J 197/005: {Lignin}
- B27N 3/00: Manufacture of substantially flat articles, e.g. boards, from particles or fibres
- C08H: DERIVATIVES OF NATURAL MACROMOLECULAR COMPOUNDS (polysaccharides C08B; natural rubber C08C; natural resins or their derivatives C09F; bituminous materials C10)
- B27N: MANUFACTURE BY DRY PROCESSES OF ARTICLES, WITH OR WITHOUT ORGANIC BINDING AGENTS, MADE FROM PARTICLES OR FIBRES CONSISTING OF WOOD OR OTHER LIGNOCELLULOSIC OR LIKE ORGANIC MATERIAL (containing cementitious material B28B; shaping of substances in a plastic state B29C; fibreboards made from fibrous suspensions D21J; drying F26B17/00)
- C07G: COMPOUNDS OF UNKNOWN CONSTITUTION (sulfonated fats, oils or waxes of undetermined constitution C07C309/62)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

The present invention relates to a method for treating lignin, wherein the method comprises the following steps: a) dissolving lignin into an aqueous composition, which contains a compound selected from the class of phenols and alkali, while keeping the temperature of the composition at 40-85° C., wherein the alkali comprises a hydroxide of an alkali metal; and b) heating the composition at a temperature, which is higher than the temperature of the composition in step a), with the proviso that the temperature of the composition does not exceed 100° C., while keeping the pH of the composition at a pH value of 6-14.

## Claims

### Claim 1

A method for treating lignin, characterized in that the method comprises the following steps:
a) dissolving lignin into an aqueous composition, which contains a compound selected from the class of phenols and alkali, while keeping the temperature of the composition at 40-85° C., wherein the alkali comprises a hydroxide of an alkali metal; and
b) heating the composition at a temperature, which is higher than the temperature of the composition in step a), with the proviso that the temperature of the composition does not exceed 100° C., while keeping the pH of the composition at a pH value of 6-14.

### Claim 2 (depends on 1)

The method of claim 1, wherein the compound selected from the class of phenols is selected from a group consisting of phenol, cresol, resorcinol and combinations thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein the temperature of the composition is kept, in step a), at a temperature of 65-80° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein step b) comprises heating the composition at a temperature, which is at least 5° C., higher than the temperature of the composition in step a).

### Claim 5 (depends on 1)

The method of claim 1, wherein the pH of the composition is kept, in step a), at the pH value of 4-10.

### Claim 6 (depends on 5)

The method of claim 5, wherein the pH of the composition is kept, in step b), at the pH value of 6-10.

### Claim 7 (depends on 1)

The method of claim 1, wherein the pH of the composition is kept, in step a), at the pH value of 4-14.

### Claim 8 (depends on 7)

The method of claim 7, wherein the pH of the composition is kept, in step b), at the pH value of 7-14.

### Claim 9 (depends on 1)

The method of claim 1, wherein the composition is heated, in step b), at a temperature of 60-100° C.

### Claim 10

A method for producing a binder composition, characterized in that the method comprises the following steps:
a) dissolving lignin into an aqueous composition, which contains a compound selected from the class of phenols and alkali, while keeping the temperature of the composition at 40-85° C., wherein the alkali comprises a hydroxide of an alkali metal;
b) heating the composition at a temperature, which is higher than the temperature of the composition in step a), with the proviso that the temperature of the composition does not exceed 100° C., while keeping the pH of the composition at a pH value of 6-14; and
c) mixing the composition formed in step b) with a crosslinking agent and heating the composition at a temperature of 60-100° C. while keeping the pH of the composition at a pH value of 6-14.

### Claim 11 (depends on 10)

The method of claim 10, wherein step b) comprises heating the composition at a temperature, which is at least 5° C. higher than the temperature of the composition in step a).

### Claim 12 (depends on 10)

The method of claim 10, wherein step c) comprises heating the composition at a temperature of 65-95° C.

### Claim 13 (depends on 10)

The method of claim 10, wherein the pH of the composition is kept, in step a), at the pH value of 4-10.

### Claim 14 (depends on 13)

The method of claim 13, wherein the pH of the composition is kept, in step b), at the pH value of 6-10.

### Claim 15 (depends on 10)

The method of claim 10, wherein the pH of the composition is kept, in step a), at the pH value of 4-14.

### Claim 16 (depends on 15)

The method of claim 15, wherein the pH of the composition is kept, in step b), at the pH value of 7-14.

### Claim 17 (depends on 10)

The method of claim 10, wherein the pH of the composition is kept, in step c), at a pH value of 6-10.

### Claim 18 (depends on 10)

The method of claim 10, wherein the pH of the composition is kept, in step c), at a pH value of 7-14.

### Claim 19 (depends on 10)

The method of claim 10, wherein the crosslinking agent is an aldehyde, and preferably formaldehyde, paraformaldehyde or a combination thereof.

### Claim 20

(canceled)

### Claim 21 (depends on 10)

A binder composition obtainable by the method of claim 10.

### Claim 22 (depends on 21)

An adhesive composition comprising the binder composition of claim 21.

### Claim 23

(canceled)

### Claim 24

(canceled)

### Claim 25

(canceled)