# US 2016/0257773 A1 · Copolymer rubber containing nitrile groups

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0257773 A1
- Document ID: US20160257773A1
- Status: Published application
- Kind: A1
- Application number: 15/032,076
- Filed: 2014-10-29
- Published: 2016-09-08
- Earliest claimed: 2013-10-30
- Assignees: Arlanxeo Deutschland GmbH
- Applicants: Arlanxeo Deutschland GmbH
- Inventors: Werner OBRECHT; Hiyam SALEM; Susanna LIEBER; Irene MOLL; Andreas KAISER
- Web page: https://patentgrep.com/patent/US20160257773A1

## CPC

- C08F 236/12: with nitriles
- C08F 236/06: Butadiene
- C08L 9/02: Copolymers with acrylonitrile
- C08L 15/005: {Hydrogenated nitrile rubber}
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present invention relates to copolymer rubbers containing nitrile groups and to the preparation thereof, to vulcanizable mixtures comprising copolymer rubbers containing nitrile groups and to the production thereof, and to vulcanizates based on copolymer rubbers containing nitrile groups, to the production thereof and to the use thereof as technical material.

## Claims

### Claim 1

A copolymer rubber containing nitrile groups, the rubber comprising:
10% to 60% by weight of an αβ-ethylenically unsaturated nitrile unit,
31% to 89% by weight of a conjugated diene unit, and
1% to 9% by weight of at least one αβ-ethylenically unsaturated monocarboxylic acid monoester unit,
wherein the rubber has
a glass transition temperature lower than −20° C., and
an oil swelling of not more than more than 20.

### Claim 2 (depends on 1)

The copolymer rubber according to claim 1, wherein the conjugated diene units have a level of hydrogenation of 50% or more.

### Claim 3 (depends on 1)

The copolymer rubber according to claim 1, wherein the α,β-ethylenically unsaturated nitrile units are selected from a group that includes acrylonitrile, methacrylonitrile, ethacrylonitrile, and mixtures thereof.

### Claim 4 (depends on 1)

The copolymer rubber according to claim 1, wherein the conjugated diene units are selected from a group that includes 1,3-butadiene, isoprene, 2,3-dimethylbutadiene, 1,3-pentadiene (piperylene), and mixtures thereof.

### Claim 5 (depends on 1)

The copolymer rubber according to claim 1, wherein the α,β-ethylenically unsaturated monocarboxylic acid monoesters are selected from a group that includes methoxyethyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, and polyethylene glycol (meth)acrylate.

### Claim 6 (depends on 1)

A process for preparing the copolymer rubbers according to claim 1, the process comprising polymerizing the α,β-ethylenically unsaturated nitrile units, the conjugated diene unit, and the α,β-ethylenically unsaturated monocarboxylic acid monoester units by emulsion polymerization.

### Claim 7 (depends on 1)

Vulcanizable mixtures comprising the copolymer rubbers according to claim 1 and at least one crosslinker.

### Claim 8 (depends on 1, 7)

A process for producing the vulcanizable mixtures according to claim 7, the process comprising mixing the copolymer rubber according to claim 1 with at least one crosslinker.

### Claim 9 (depends on 7)

A process for producing vulcanizates comprising copolymer rubbers containing nitrile groups, the process comprising subjecting the vulcanizable mixtures according to claim 7 to vulcanization at temperatures of 100° C. to 200° C.

### Claim 10 (depends on 1)

A vulcanizate comprising the copolymer rubbers containing nitrile groups according to claim 1.

### Claim 11 (depends on 9)

A method for production of mouldings from the vulcanizate according to claim 9, the method comprising extruding or injection moulding of the vulcanizate into a moulding.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the mouldings are one of belts, rollers, shoe components, gaskets, hoses, damping elements, stators or cable sheaths.

### Claim 13 (depends on 1)

A moulding comprising the copolymer rubber containing nitrile groups according to claim 1.

### Claim 14 (depends on 9)

A moulding produced by the process according to claim 9.

### Claim 15 (depends on 1)

The copolymer rubber according to claim 1, wherein:
the rubber comprises:
20% to 50% by weight of an α,β-ethylenically unsaturated nitrile unit,
42% to 78.75% by weight of a conjugated diene unit, and
1.25% to 8% by weight of at least one α,β-ethylenically unsaturated monocarboxylic acid monoester unit,
the glass transition temperature is lower than −23° C., and
the oil swelling is not more than 18%.

### Claim 16 (depends on 15)

The copolymer rubber according to claim 15, wherein:
the α,β-ethylenically unsaturated nitrile units are selected from a group that includes acrylonltrile, methacrylonitrile, ethacrylonitrile, and mixtures thereof,
the conjugated diene units have a level of hydrogenation of 50% or more and are selected from a group that includes 1,3-butadiene, isoprene, 2,3-dimethylbutadiene, 1,3-pentadiene (piperylene), and mixtures thereof, and
α,β-ethylenically unsaturated monocarboxylic acid monoesters are selected from a group that includes methoxyethyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, or and polyethylene glycol (meth)acrylate.

### Claim 17 (depends on 1)

The copolymer rubber according to claim 1, wherein:
the rubber comprises:
34% to 43% by weight of an α,β-ethylenically unsaturated nitrile unit,
49% to 64.5% by weight of a conjugated diene unit, and
1.5% to 8% by weight of at least one α,β-ethylenically unsaturated monocarboxylic acid monoester unit,
the glass transition temperature is lower than −25° C., and
the oil swelling is not more than 15%.

### Claim 18 (depends on 15)

The copolymer rubber according to claim 15, wherein:
the α,β-ethylenically unsaturated nitrile units (a) are selected from a group that includes acrylonltrile, methacrylonitrile, ethacrylonitrile, and mixtures thereof,
the conjugated diene units have a level of hydrogenation of 75% or more, and are selected from a group that includes 1,3-butadiene, isoprene, 2,3-dimethylbutadiene, 1,3-pentadiene (piperylene), and mixtures thereof, and
α,β-ethylenically unsaturated monocarboxylic acid monoesters are selected from a group that includes methoxy or ethoxy polyethylene glycol (meth)acrylate having 1 to 20 repeat ethylene glycol units.

### Claim 19 (depends on 18)

The copolymer rubber according to claim 18, wherein:
the α,β-ethylenically unsaturated nitrile units are acrylonitrile,
the conjugated diene units have a level of hydrogenation of 85% or more, and are 1,3-butadiene, and
the α,β-ethylenically unsaturated monocarboxylic acid monoesters (c) are selected from a group that includes methoxy or ethoxy polyethylene glycol (meth)acrylate having 1 to 5 repeat ethylene glycol units.

### Claim 20 (depends on 9)

The process according to claim 9, wherein the vulcanizable mixtures are subjected to vulcanization at temperatures of 130° C. to 200° C.