# US 2016/0257772 A1 · Catalysts and methods of controlling long chain branching in polyolefins

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0257772 A1
- Document ID: US20160257772A1
- Status: Published application
- Kind: A1
- Application number: 15/058,375
- Filed: 2016-03-02
- Published: 2016-09-08
- Earliest claimed: 2015-03-02
- Assignees: Equistar Chemicals, LP
- Applicants: Equistar Chemicals, LP
- Inventors: MICHAEL W LYNCH; Mark K. Reinking
- Web page: https://patentgrep.com/patent/US20160257772A1

## CPC

- C08F 10/02: Ethene
- B01J 23/26: Chromium
- B01J 35/19: {Catalysts containing parts with different compositions}
- B01J 35/615: {100-500 m2/g}
- B01J 35/617: {500-1000 m2/g}
- B01J 35/635: {0.5-1.0 ml/g}
- B01J 35/638: {more than 1.0 ml/g}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F 2410/01: Additive used together with the catalyst, excluding compounds containing Al or B
- C08F 2410/06: Catalyst characterized by its size
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

The present disclosure relates to catalysts comprising two heterogeneous chromium catalysts for the polymerization of olefins are provided herein. The catalysts, as well as related compositions and methods using the same, may be used to for the production of polyolefins, including for the production of bimodal molecular weight distribution polyolefins, e.g., polyethylene and copolymers of ethylene and 1-hexene.

## Claims

### Claim 1

A composition comprising:
(A) a first catalyst comprising from 0.25-2 wt. % chromium deposited on a first solid oxide component, wherein the first catalyst has a pore volume from 1.0-3.5 mL/g and a surface area from 250-900 m2/g; and
(B) a second catalyst comprising from about 0.25-2 wt. % chromium deposited on a second solid oxide component, wherein the second catalyst has a pore volume from 1.0-2.5 mL solid/g and a surface area from 400-1000 m2/g;
wherein the first and second catalysts are present a weight ratio from 1:9-9:1, provided that the first catalyst and second catalyst are not the same.

### Claim 2 (depends on 1)

The composition of claim 1, wherein the first catalyst further comprises from 0.5-5.0 wt. % titanium or aluminum.

### Claim 3 (depends on 1)

The composition of claim 1, wherein the first catalyst has a surface area from 250-600 m2/g.

### Claim 4 (depends on 1)

The composition of claim 1, wherein the second catalyst further comprises from 0.5-5 wt. % aluminum, titanium, or zirconium or from 0.1-1 wt. % boron or fluorine.

### Claim 5 (depends on 1)

The composition of claim 1, wherein the second catalyst has a surface area from 500-1000 m2/g.

### Claim 6 (depends on 1)

The composition of claim 1, wherein the first catalyst has a pore volume from 1.0-2.5 mL/g.

### Claim 7 (depends on 1)

The composition of claim 1, wherein the first solid oxide component and the second solid oxide component consist essentially of silica.

### Claim 8

A method comprising:
(A) obtaining a first catalyst, wherein:
the first catalyst comprising from 0.25-2 wt. % chromium deposited on a first solid oxide component, wherein the first catalyst has a pore volume from 1.0-3.5 mL/g and a surface area from 250-900 m2/g;
(B) heating the first catalyst to a temperature from 700-900° C. to form an activated first catalyst;
(C) obtaining a second catalyst, wherein:
the second catalyst comprising from 0.25-2 wt. % chromium deposited on a second solid oxide component, wherein the second catalyst has a pore volume from 1.0-2.5 mL/g and a surface area from 400-1000 m2/g; and
either one of steps (D) and (E):
(D) heating the second catalyst to a temperature from 400-700° C. to form an activated second catalyst and then admixing the activated second catalyst to the first activated first catalyst; or
(E) admixing the second catalyst to the activated first catalyst and heating this catalyst mixture to a temperature from 400-700° C. to further activate this catalyst mixture;
wherein the first and second activated catalysts are present in a weight ratio from 1:9-9:1, provided that the first activated catalyst and second activated catalyst are not the same.

### Claim 9 (depends on 8)

The method of claim 8, wherein the first catalyst and second catalyst are heated in the presence of air.

### Claim 10 (depends on 1)

A method comprising:
(A) admixing a monomer, wherein the monomer is an olefin(C≦6), and the composition of claim 1 to form a reaction mixture; and
(B) reacting the monomer in the presence of the composition under conditions sufficient to form a polyolefin with a bimodal molecular weight distribution.

### Claim 11 (depends on 10)

The method of claim 10, wherein the monomer is ethylene and the polyolefin is polyethylene.

### Claim 12 (depends on 10)

The method of claim 10, wherein the first mode of the molecular weight distribution of the polyolefin is a low molecular weight mode from 80,000-130,000 Daltons and wherein the second mode of the molecular weight distribution of the polyolefin is a high molecular weight mode from about 84,000-300,000 Daltons, provided that the average molecular weight of the second mode is greater than the first mode.

### Claim 13 (depends on 10)

The method of claim 10, wherein the amount of the monomer is from 0.1-15 mol. % of the total soluble components.

### Claim 14 (depends on 10)

The method of claim 10, wherein the method further comprises adding a comonomer to the reaction mixture, wherein the comonomer is an olefin(C≦12).

### Claim 15 (depends on 14)

The method of claim 14, wherein the comonomer is hexene.

### Claim 16 (depends on 10)

The method of claim 10, wherein the high molecular weight mode of the polyolefin has a lower extent of long chain branching relative to the low molecular weight mode of the polyolefin, as measured by the long chain branching index.

### Claim 17 (depends on 14)

The method of claim 14, wherein the high molecular weight mode of the polyolefin contains more of the incorporated comonomer relative to the low molecular weight mode of the polyolefin, as measured by short chain branching index.

### Claim 18 (depends on 17)

The method of claim 17, wherein the high molecular weight mode of the polyolefin has a lower extent of long chain branching relative to the low molecular weight mode of the polyolefin, as measured by the long chain branching index.

### Claim 19 (depends on 10)

The method of claim 10, wherein the method further comprises adding:
(a) a co-catalyst selected from the group consisting of trialkylboron(C≦24), trialkylaluminum(C≦24), dialkylzinc(C≦18), and alkyllithium(C≦12);
(b) hydrogen gas; or
(c) both (a) and (b);
to the reaction mixture; and heating the reaction mixture to a temperature from about 75-120° C.

### Claim 20 (depends on 19)

The method of claim 19, wherein the trialkylboron(C≦12) is triethylboron.