# US 2016/0257617 A1 · A reduction and harmless method for recycling heavy metal waste

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0257617 A1
- Document ID: US20160257617A1
- Status: Published application
- Kind: A1
- Application number: 14/419,255
- Filed: 2014-03-13
- Published: 2016-09-08
- Earliest claimed: 2014-01-16
- Assignees: University of Science and Technology Beijing
- Applicants: University of Science and Technology Beijing
- Inventors: De an Pan; Shen gen ZHANG; Ling jie LI; Bin GUO; Bo LIU
- Web page: https://patentgrep.com/patent/US20160257617A1

## CPC

- C04B 28/085: {Slags from the production of specific alloys, e.g. ferrochrome slags}
- C01F 11/46: Sulfates (dehydration of gypsum {for the production of calcium sulfate cements} C04B11/02)
- C04B 5/00: Treatment of {metallurgical} slag (manufacture of slag wool C03B; in, or for, the production of metals C21B, C22B); Artificial stone from molten {metallurgical} slag {(other cast stone C04B32/005; mechanical aspects B28B1/54)}
- C04B 12/005: {Geopolymer cements, e.g. reaction products of aluminosilicates with alkali metal hydroxides or silicates}
- C04B 14/22: Glass {; Devitrified glass}
- C04B 18/0445: {Synthetic gypsum, e.g. phosphogypsum (gypsum from smoke purification C04B18/064)}
- C04B 18/0472: {Waste material contaminated by heavy metals}
- C04B 28/008: {Mineral polymers other than those of the Davidovits type, e.g. from a reaction mixture containing waterglass}
- C22B 7/04: Working-up slag
- C22C 11/00: Alloys based on lead
- Y02P 40/10: Production of cement, e.g. improving or optimising the production methods; Cement grinding
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

An amount-reduction, harmless, disposal method for heavy metal waste gypsum (HMWG), which belongs to the technical fields of recycling economy and environmental protection. The HMWG used as raw material is subjected to processes of smelting fluxpreparation, lead smelting, fuming, and geopolymeric gelling, to realize amount-reduction, harmless and resources recycling utilization of heavy metal waste gypsum. The smoke containing sulfur dioxide produced in the smelting process is sent to the acid making system, and the produced dust with heavy metal is sent to the dedicated system for heavy mental disposing. The smoke dust produced in the fuming process is returned to the lead smelting system. The secondary HMWG produced in the acid making system would be returned to the preparation process of smelting flux. And the final products would be sulfuric acid and geopolymer material.

## Claims

### Claim 1

A disposal method for heavy metal waste gypsum, comprising the following steps:
(1a) a step of smelting flux preparation wherein, in order
dried heavy metal waste gypsum and waste glass are mixed by ball milling into a mixture,
the mixture is heated in a heat treatment furnace, obtaining pre-sintering material of smelting flux;
smoke containing sulfur dioxide produced from placing the mixture in the heat treatment furnace is sent to an acid making system producing sulfuric acid and a secondary heavy metal waste gypsum;
(1b) returning the secondary heavy metal waste gypsum produced in the acid making system and further carrying out said smelting flux preparation described in steps (1a) partially substituting said secondary heavy metal waste gypsum for said dried heavy metal waste gypsum
(2) sending dust comprising heavy metal produced in said heat treatment furnace to a heavy metal disposal system comprising lead smelting; said lead smelting comprising steps of ball milling and mixing into a lead smelting mixture the pre-sintering material of smelting flux obtained in steps (1a), additional smelting fluxes and raw material for lead smelting,
placing said lead smelting mixture in a lead smelting furnace to smelt lead, wherein slags of lead and smoke containing sulfur are produced in the lead smelting furnace, and said slags of lead and dust comprising heavy metal are each sent to one of an acid making system and heavy metal disposition system;
(3) in a step of fuming,
placing in a fuming furnace said lead smelting slags are fumed until obtaining a product with different chemical properties from fuming said slags;
sending dust produced in the step of fuming be smelted in step (2); and
(4) a step of geopolymeric gelling, wherein:
the fuming slags obtained in step (3) are ground by a mechanical method to a voluminal median diameter of 100 μm;
adding an activating solution to said fuming slags and stirring for 5˜20 min;
casting a resultant of said activating solution, said fuming slag into a mold and curing, producing a geopolymer material, wherein a mass ratio of said activating solution to fuming slag is 0.40˜0.56, and said activating solution comprises NaOH, H2O, and Sodium silicate hydrate, namely Na2O.nSiO2.mH2O, and the solute in said activating solution was calculated with Na2O (NaOH calculated with Na2O) and SiO2, the proportion of SiO2 was 10˜18 wt %, and the proportion of Na2O was 6˜25 wt %, and in case that the proportion of SiO2 is 10˜18 wt %, if the content of Na2O in the activating solution was less than 6˜25 wt %, then NaOH would be added to meet the demand of Na.

### Claim 2 (depends on 1)

The method of claim 1, wherein a mass ratio between sulfur dioxide and calcium oxide is 1:1˜3:1 in the ball milling mixture composed of said heavy metal waste gypsum and waste glass, a heating temperature is 800° C.˜1100° C., heating time is 0.5 h˜2 h, and heating atmosphere is air.

### Claim 3 (depends on 1)

The method of claim 1, wherein smelting fluxes from step (2) are selected from the group consisting of limestone, quartz sand, and scrap iron; and
when said smelting flux pre-sintering material, other smelting fluxes, and the raw material for lead smelting are mixed by ball milling, the mass ratio between mixtures of smelting flux pre-sintering material and other smelting fluxes and said raw material for lead smelting is 10:100˜15:100, a mass ratio between SiO2 and Fe in said ball milling mixture is 0.8˜1.0, and a mass ratio between SiO2 and CaO is 1.50˜1.65.

### Claim 4 (depends on 1)

The method of claim 1, wherein in step (4), said curing is divided into to two stages including a low temperature curing and high temperature curing stage; wherein said low temperature curing stage is at a temperature of 30˜40° C., the curing time is 1˜24 h, and the relative humidity is 20˜80%; and
wherein said high temperature curing stage is at a temperature of 60˜90° C., the curing time is 1˜24 h, and the relative humidity is 20˜80%.