# US 2016/0257614 A1 · Additive for cementitious materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0257614 A1
- Document ID: US20160257614A1
- Status: Published application
- Kind: A1
- Application number: 14/915,664
- Filed: 2014-08-28
- Published: 2016-09-08
- Earliest claimed: 2013-09-06
- Assignees: Upm-Kymmene Corporation
- Applicants: Upm-Kymmene Corporation
- Inventors: Hannele Kuosa; Anna Suurnakki; Antti Laukkanen; Jan-Erik Teirfolk; Markku Leivo
- Web page: https://patentgrep.com/patent/US20160257614A1

## CPC

- C04B 24/383: {Cellulose or derivatives thereof}
- C04B 7/36: Manufacture of hydraulic cements in general
- C04B 20/006: {Microfibres; Nanofibres}
- C04B 28/02: containing hydraulic cements other than calcium sulfates
- C04B 38/02: by adding chemical blowing agents
- C04B 38/10: by using foaming agents (C04B38/02 takes precedence){or by using mechanical means, e.g. adding preformed foam}
- C04B 2103/48: Foam stabilisers
- C04B 2111/00103: {Self-compacting mixtures}
- C04B 2111/29: {Frost-thaw resistance}
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The invention relates to use of nano-fibrillar cellulose as an gas-entrainment stabilizer, which when used in cementitious materials, provides improved gas pore structure quality and/or stability and/or robustness with regard to water content variation. The invention further relates to a method for stabilizing gasentrainment of cementitious materials and to a method for providing cementitious material with improved air pore structure quality and/or stability and/or robustness with regard to water content variation.

## Claims

### Claim 1

Use of nanofibrillar cellulose (NFC) as a gas-entrainment stabilizer.

### Claim 2 (depends on 1)

The use as claimed claim 1, wherein NFC is used in a cementitious composition, paste, or material.

### Claim 3 (depends on 1)

The use as claimed in claim 1, wherein the diameter of the NFC or NFC bundles is less than 1 μm, preferably less than 200 nm, more preferably less than 100 nm.

### Claim 4 (depends on 1)

The use as claimed in claim 1, wherein the used amount of dry NFC is 0.01% or more by weight based on dry weight of binder in the cementitious composition, preferably from 0.01% to 0.3%, more preferably from 0.02% to 0.2% , most preferably from 0.05% to 0.11%.

### Claim 5 (depends on 1)

The use as claimed in claim 1, wherein the NFC is native NFC.

### Claim 6 (depends on 1)

The use as claimed in claim 1, wherein the NFC is chemically and physically modified NFC, preferably anionically charged NFC, more preferably particular oxidized NFC or carboxymethylated NFC, most preferably mechanically disintegrated TEMPO oxidized NFC.

### Claim 7 (depends on 1)

The use as claimed in claim 1, wherein NFC is used together with at least one gas-entraining agent or admixture.

### Claim 8 (depends on 1)

The use of NFC as claimed in claim 1 for providing gas-entrained cementitious material with improved gas pore structure quality and/or stability and/or robustness with regard to water content variation.

### Claim 9 (depends on 8)

The use as claimed in claim 8, wherein the gas-entrained cementitious material is air-entrained cementitious material, such as concrete, in particular foamed concrete or self-compacting concrete (SCC).

### Claim 10 (depends on 8)

The use as claimed in claim 8, wherein the gas-entrained cementitious material is hydrogen-entrained cementitious material, such as autoclaved aerated concrete (ACC).

### Claim 11

A method for stabilizing gas-entrainment of cementitious materials, comprising the steps of:
providing nanofibrillar cellulose (NFC);
mixing said NFC and with a cementitious composition and water to obtain a cementitious paste; and
allowing the thus obtained cementitious paste to harden to obtain gas-entrained cementitious material.

### Claim 12

A method for the preparation of gas-entrained concrete, comprising the steps of:
providing nanofibrillar cellulose (NFC);
providing at least one gas-entraining agent
mixing said NFC and the at least one gas-entraining agent with a cementitious composition, comprising at least binder, and water to obtain a cementitious paste; and
allowing the thus obtained cementitious paste to harden to obtain gas-entrained cementitious material.

### Claim 13 (depends on 11)

The method as claimed in claim 11, wherein the amount of NFC is 0.01% or more by based on dry weight of binder in the cementitious composition, preferably from 0.01% to 0.3%, more preferably from 0.02% to 0.2%, most preferably from 0.05% to 0.11%.

### Claim 14 (depends on 11)

The method as claimed in claim 11, wherein the water/cement ratio of the cementitious paste is from 0.25 to 1.50, preferably from 0.35 to 0.8, more preferably from 0.40 to 0.65.

### Claim 15 (depends on 11)

The method as claimed in claim 11, wherein the hardened gas-entrained cementitious normal weight material and cement paste fraction included in it, or normal weight cement paste fraction included in any lightweight material have air pore spacing factor less than 0.4 mm, preferably from 0.2 to 0.35 mm, more preferably from 0.22 to 0.3 mm.

### Claim 16 (depends on 11)

The method as claimed in claim 11, wherein the gas pores in the hardened normal weight material and cement paste fraction included in it, or normal weight cement paste fraction included in any lightweight material, have air pore specific surface greater than 20 mm2/mm3, preferably greater than 25 mm2/mm3.

### Claim 17

A hardened gas-entrained cementitious material comprising nanofibrillar cellulose (NFC).

### Claim 18 (depends on 17)

The hardened gas-entrained cementitious material as claimed in claim 17, which is foamed concrete, self-compacting concrete (SCC) or autoclaved aerated concrete (ACC), in particular foamed concrete or SCC.

### Claim 19 (depends on 17)

The hardened gas-entrained cementitious material as claimed in claim 17, wherein the amount of dry NFC is 0.01% or more by weight based on the dry weight of binder in cementitious composition, preferably from 0.01% to 0.3%, more preferably from 0.02% to 0.2%, most preferably from 0.05% to 0.11%.

### Claim 20 (depends on 17)

The hardened gas-entrained cementitious material as claimed in claim 17, having spacing factor less than 0.4 mm, preferably less than 0.30, more preferably less than 0.20.

### Claim 21 (depends on 17)

The hardened gas-entrained cementitious material as claimed in claim 17, having specific surface greater than 20 mm2/mm3, preferably greater than 25 mm2/mm3.

### Claim 22 (depends on 12, 17)

The hardened gas-entrained cementitious material as claimed in claim 17, obtained by the process defined in claim 12.