# US 2016/0257099 A1 · Laminated metal sheet for containers, method for producing metal can, and method for evaluating formability of metal sheet (as amended)

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0257099 A1
- Document ID: US20160257099A1
- Status: Published application
- Kind: A1
- Application number: 15/032,816
- Filed: 2014-10-29
- Published: 2016-09-08
- Earliest claimed: 2013-10-30
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Yoichiro Yamanaka; Yusuke Nakagawa; Junichi Kitagawa; Hiroki Nakamaru
- Web page: https://patentgrep.com/patent/US20160257099A1

## CPC

- B32B 27/36: comprising polyesters
- B32B 15/04: comprising metal as the main or only constituent of a layer, {which is} next to another layer of {the same or of} a {different material (next to a bituminous or tarry layer B32B11/08; next to a water-setting substance layer B32B13/06; next to a glass layer B32B17/061; next to a cellulosic plastic layer B32B23/042)}
- B32B 15/09: comprising polyesters
- B32B 15/18: comprising iron or steel {(B32B15/011, B32B15/012 and B32B15/013 take precedence)}
- B32B 38/0036: {Heat treatment (for heating or cooling of layers during lamination B32B37/06, B32B37/08)}
- B65D 1/12: Cans, casks, barrels, or drums
- B65D 25/14: Linings or internal coatings (of containers made by folding or erecting blanks made of paper B65D5/56 {; linings for domestic water storage heaters F24H1/183})
- B32B 38/145: {Printing}
- B32B 2307/4026: within the layer by addition of a colorant, e.g. pigments, dyes
- B32B 2307/558: Impact strength, toughness
- B32B 2307/714: Inert, i.e. inert to chemical degradation, corrosion
- B32B 2307/75: Printability
- B32B 2311/00: Metals, their alloys or their compounds
- B32B 2367/00: Polyesters, e.g. PET, i.e. polyethylene terephthalate
- B32B 2439/00: Containers; Receptacles
- B32B 2439/66: Cans, tins
- B32B 2439/70: Food packaging
- B65D 1/165: {Cylindrical cans}
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- B65D: CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS, e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES, DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS; ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR; PACKAGING ELEMENTS; PACKAGES

## Abstract

Provided are a laminated metal sheet for containers that has excellent formability after heat treatment performed after coating, printing, etc. and is suitable for DR cans, a method for producing a metal can using the above metal sheet and a method for evaluating the formability of a metal sheet. The crystal structure of a top layer of a laminate layer of the laminated metal sheet for containers and the crystal structure inside the laminate layer are controlled in a sophisticated manner. Specifically, the intensity ratio I2968/I3085 of the Raman band intensity (I2968) at a peak position around 2,968 cm−1 to the Raman band intensity (I3085) at a peak position around 3,085 cm−1 that are obtained by laser Raman spectroscopy is used. This intensity ratio is controlled within a specific range.

## Claims

### Claim 1

A laminated metal sheet for containers, the laminated metal sheet comprising a metal sheet and a laminate layer that covers at least one side of the metal sheet, the laminate layer including a single layer composed mainly of polyester or a plurality of layers composed mainly of the polyester,
an intensity ratio I2968/I3085 of a Raman band intensity (I2968) at a peak top position around 2,968 cm−1 to a Raman band intensity (I3085) at a peak top position around 3,085 cm−1 being a range of 0.3 to 0.9, the Raman band intensity (I2968) and the Raman band intensity (I3085) being determined by a laser Raman method on a surface of the laminate layer and
when an entire thicknesswise cross section of the laminate layer is irradiated with linearly polarized laser light in a direction perpendicular to the cross section of the laminate layer, the Raman band intensity ratio I2968/I3085 being within a range of 0.7 to 1.5.

### Claim 2 (depends on 1)

The laminated metal sheet for containers according to claim 1, wherein an amount of change in the Raman band intensity ratio I2968/I3085 before and after a heat treatment is 0.4 or less, when the laminated metal sheet for containers is subjected to the heat treatment in a temperature range of 160 to 210° C. for 20 minutes, the Raman band intensity ratio I2968/I3085 determined by irradiating the entire thicknesswise cross section of the laminate layer with the linearly polarized laser light in the direction perpendicular to the cross section of the laminate layer.

### Claim 3 (depends on 1)

The laminated metal sheet for containers according to claim 1, wherein the laminate layer includes a top layer, an intermediate layer, and a steel sheet-adhesion layer that are stacked on one another, and the intermediate layer contains 5 PHR or more and 30 PHR or less of a white pigment.

### Claim 4 (depends on 3)

The laminated metal sheet for containers according to claim 3, wherein each of the top layer and the steel sheet-adhesion layer contains 2 PHR or less of the white pigment.

### Claim 5 (depends on 3)

The laminated metal sheet for containers according to claim 3, wherein the white pigment is titanium dioxide or barium sulfate.

### Claim 6 (depends on 1)

The laminated metal sheet for containers according to claim 1, wherein the laminate layer is formed on a side that later becomes an inner side of a container, and the polyester contained in the laminate layer contains at least 80% by mole of an ethylene terephthalate unit.

### Claim 7 (depends on 1)

The laminated metal sheet for containers according to claim 1, wherein
the laminate layer is formed on a side that later becomes an outer side of a container,
the laminate layer is composed mainly of the polyester,
the sum of the content of an ethylene terephthalate unit contained in the polyester and the content of a butylene terephthalate unit contained in the polyester is 80% by mole or more, and
the polyester has a glass transition temperature of 20 to 100° C.

### Claim 8 (depends on 1)

A method for producing a metal can, the method comprising:
a printing step of adhering an ink to the laminate layer of a laminated metal sheet for containers according to claim 1 and then heat-drying the adhered ink, the laminate layer being formed on a surface of the laminated metal sheet; and,
after the printing step, a can manufacturing step of subjecting the laminated metal sheet for containers to can manufacturing processing.

### Claim 9

A metal sheet formability evaluation method for evaluating formability of a laminated metal sheet for containers after heat treatment,
the laminated metal sheet for containers including a metal sheet and a laminate layer that covers at least one side of the metal sheet,
the laminate layer including a single layer composed mainly of polyester or a plurality of layers composed mainly of the polyester,
the method comprising:
a first step of determining, on a surface of the laminate layer before the heat treatment, a Raman band intensity (I2968) at a peak top position around 2,968 cm−1 and a Raman band intensity (I3085) at a peak top position around 3,085 cm−1 by a laser Raman method and then deriving an intensity ratio I2968/I3085;
a second step of, when an entire thicknesswise cross section of the laminate layer before the heat treatment is irradiated with linearly polarized laser light in a direction perpendicular to the cross section of the laminate layer, deriving the Raman band intensity ratio I2968/I3085; and
a third step of evaluating the formability of the laminated metal sheet for containers using the intensity ratio I2968/I3085 derived in the first step and the intensity ratio I2968/I3085 derived in the second step.