# US 2016/0256928 A1 · Macro-chip reinforced alloy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0256928 A1
- Document ID: US20160256928A1
- Status: Published application
- Kind: A1
- Application number: 15/061,542
- Filed: 2016-03-04
- Published: 2016-09-08
- Earliest claimed: 2015-03-04
- Assignees: Orrvilon, Inc.
- Applicants: Orrvilon Inc.
- Inventors: Krishna P. Singh; Thomas G. Haynes, III; Luke Chester Sobus
- Web page: https://patentgrep.com/patent/US20160256928A1

## CPC

- C22C 21/00: Alloys based on aluminium
- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- B22F 3/10: Sintering only
- B22F 7/008: {characterised by the composition}
- C22C 1/1084: {by mechanical alloying (blending, milling)}
- C22C 32/0057: {based on B4C}
- G21F 1/047: {with metals}
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- G21F: PROTECTION AGAINST X-RADIATION, GAMMA RADIATION, CORPUSCULAR RADIATION OR PARTICLE BOMBARDMENT; TREATING RADIOACTIVELY CONTAMINATED MATERIAL; DECONTAMINATION ARRANGEMENTS THEREFOR (radiation protection by pharmaceutical means A61K8/00, A61Q17/04; in cosmonautic vehicles B64G1/54; combined with a reactor G21C11/00; combined with X-ray tubes H01J35/16; combined with X-ray apparatus H05G1/02)

## Abstract

Described herein is a powder blend comprising a first component comprising a blend of a first metal particle and a first ceramic particle; and a second component comprising a reinforcing chip, the reinforcing chip comprising a second ceramic particle dispersed within a chip metal matrix.

## Claims

### Claim 1

A powder blend comprising:
a first component comprising a blend of a first metal particle and a first ceramic particle; and
a second component comprising a reinforcing chip, the reinforcing chip comprising a second ceramic particle dispersed within a chip metal matrix.

### Claim 2 (depends on 1)

The powder blend according to claim 1, wherein the first component and the second component are present in a weight ratio ranging from about 100:1 to about 2:1.

### Claim 3 (depends on 1)

The powder blend according to claim 1, wherein the first ceramic particle and the second ceramic particle are formed from the same material.

### Claim 4 (depends on 1)

The powder blend according to claim 1, wherein the first ceramic particle and the second ceramic particle are formed from different materials.

### Claim 5 (depends on 1)

The powder blend according to claim 1, wherein the first ceramic particle and the second ceramic particle are each independently selected from the group consisting of alumina, titanium carbide, silicon carbide, tungsten carbide, boron carbide, and mixtures thereof.

### Claim 6 (depends on 1)

The powder blend according to claim 1, wherein the first metal particle and the chip metal matrix are formed from the same material.

### Claim 7 (depends on 1)

The powder blend according to claim 1, wherein the first metal particle and the chip metal matrix are formed from different materials.

### Claim 8 (depends on 1)

The powder blend according to claim 1, wherein the first metal particle and the chip metal matrix are each independently selected from the group consisting of pure aluminum, an aluminum alloy, steel, a nickel alloy, a titanium alloy, and combinations thereof.

### Claim 9 (depends on 1)

The powder blend according to claim 1, wherein the reinforcing chip has a height to width aspect ratio ranging from about 1:3 to about 1:1.25.

### Claim 10 (depends on 1)

The powder blend according to claim 1, wherein the reinforcing chip has a height to thickness aspect ratio ranging from about 2:1 to about 10:1.

### Claim 11 (depends on 1)

The powder blend according to claim 1, wherein the alloy chips have a width ranging from about 2.0 mm to about 10.0 mm.

### Claim 12 (depends on 1)

The powder blend according to claim 1, wherein the alloy chips have a thickness ranging from about 0.1 mm to about 1.0 mm.

### Claim 13 (depends on 1)

The powder blend according to claim 1, wherein the first ceramic particle and the second ceramic particle each have a particle distribution of 100% less than about 250 μm.

### Claim 14 (depends on 1)

The powder blend according to claim 1, wherein the first metal particle has a d50 ranging from about 1 μm to about 20 μm.

### Claim 15 (depends on 1)

The powder blend according to claim 1, wherein the first metal particle is an aluminum particle and has a natural oxide formation layer having a thickness ranging from about 3 nm to about 7 nm.

### Claim 16 (depends on 1)

The powder blend according to claim 1, wherein the first ceramic particle and the first metal particle are present in a weight ratio ranging from about 1:15 to about 1:7.

### Claim 17

A method of forming a neutron shielding material comprising:
a) mixing together a first metal particle having a first grain growth temperature; a first ceramic particle; and a reinforcing chip to form a powder blend; and
b) processing the powder blend at a hot-work temperature;
wherein the reinforcing chip comprises a second ceramic particle dispersed within a chip metal matrix, having a second grain growth temperature; and
wherein the hot-work temperature is lower than both of the first and second grain growth temperatures.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the hot-work temperature is less than about 1100° F.

### Claim 19 (depends on 17)

The method according to claim 17, wherein the reinforcing chip is present in a non-zero amount ranging up to about 35 wt. % based on the total weight of the powder blend.

### Claim 20 (depends on 17)

The method according to claim 17, wherein the processing of step b) comprises vacuum sintering the powder blend into a billet and subsequently extruding the billet into a sheet material.