# US 2016/0256592 A1 · Stretch laminates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0256592 A1
- Document ID: US20160256592A1
- Status: Published application
- Kind: A1
- Application number: 15/057,363
- Filed: 2016-03-01
- Published: 2016-09-08
- Earliest claimed: 2015-03-02
- Assignees: The Procter & Gamble Company
- Applicants: The Procter & Gamble Company
- Inventors: Torsten LINDNER; Matthias MORAND; Robert Haines TURNER; Ebrahim REZAI; Marc HAMM; Jinyu CHEN; Yuhong HU; Andy SWAIN; Jennifer THATCHER
- Web page: https://patentgrep.com/patent/US20160256592A1

## CPC

- A61L 15/24: Macromolecular compounds obtained by reactions only involving carbon-to-carbon unsaturated bonds; Derivatives thereof {(A61L15/225 takes precedence)}
- A61F 13/15739: {Sealing, e.g. involving cutting}
- A61F 13/49007: {Form-fitting, self-adjusting disposable diapers}
- A61L 15/58: Adhesives
- A61L 15/585: {Mixtures of macromolecular compounds}
- B32B 5/022: {Non-woven fabric}
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 25/08: of synthetic resin
- B32B 25/10: next to a fibrous or filamentary layer
- B32B 27/08: of synthetic resin
- B32B 27/12: next to a fibrous or filamentary layer
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- A61F 2013/49044: {being stretchable non-elastic panels, (A61F13/4902 takes precedence)}
- A61F 2013/49047: {at the ears}
- B32B 2250/40: Symmetrical or sandwich layers, e.g. ABA, ABCBA, ABCCBA
- B32B 2274/00: Thermoplastic elastomer material
- B32B 2307/51: Elastic
- B32B 2307/542: Shear strength
- B32B 2307/702: Amorphous
- B32B 2307/718: Weight, e.g. weight per square meter
- B32B 2307/72: Density
- B32B 2307/726: Permeability to liquids, absorption
- B32B 2555/02: Diapers or napkins
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- A61F: FILTERS IMPLANTABLE INTO BLOOD VESSELS; PROSTHESES; DEVICES PROVIDING PATENCY TO, OR PREVENTING COLLAPSING OF, TUBULAR STRUCTURES OF THE BODY, e.g. STENTS; ORTHOPAEDIC, NURSING OR CONTRACEPTIVE DEVICES; FOMENTATION; TREATMENT OR PROTECTION OF EYES OR EARS; BANDAGES, DRESSINGS OR ABSORBENT PADS; FIRST-AID KITS (dental prosthetics A61C)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

Stretch laminate hot melt adhesives and stretch laminates are described. The stretch laminate hot melt adhesives are suitable for adhering elastic materials with inelastic substrates, and allow permanent deformation of the inelastic substrate and extensions and retractions of the elastic materials. The stretch laminate hot melt adhesive is particularly suitable for back ear lamination for disposable absorbent articles.

## Claims

### Claim 1

A stretch laminate comprising:
one or more substrates adhesively bonded to an elastic film by a hot melt adhesive; wherein the hot melt adhesive comprises:
a. about 35 to about 70 weight percent of a polypropylene copolymer having (i) a heat of fusion less than about 15 J/g measured at 10° C./min heating and cooling rate in accordance with ASTM D3418-12; (ii) a propylene content greater than 50% of the copolymer;
b. about 2 to about 15 weight percent of a wax having (i) a heat of fusion greater than 50 J/g measured at 10° C./min heating and cooling rate in accordance with ASTM D3418-12, and (ii) a melting peak greater than 100° C. measured in accordance with ASTM D3418-12;
c. a tackifier
wherein the adhesive has (i) a storage modulus (G′40) of about 5×105 to about 5×107 Pascal at 40° C., 10 rad/s; (ii) a storage modulus (G′80) of about 5×103 to about 1×107 Pascal at 80° C., 10 rad/s; and (iii) a density range of about 0.75 to about 0.90 g/cm3 at 160° C. measured in accordance with ASTM D1475.

### Claim 2 (depends on 1)

The stretch laminate of claim 1, wherein the propylene copolymer is a mixture of propylene copolymers.

### Claim 3 (depends on 1)

The stretch laminate of claim 1, wherein the propylene copolymer is a propylene homopolymer.

### Claim 4 (depends on 1)

The stretch laminate of claim 1, wherein the propylene copolymer comprises a comonomer selected from the group consisting of C2, C4, C5, C6, C7, C8, C9, C10, C11, C12 and mixtures thereof.

### Claim 5 (depends on 3)

The stretch laminate of claim 3, wherein the comonomer is selected from the group consisting of C2, C4, C8 and mixtures thereof.

### Claim 6 (depends on 1)

The stretch laminate of claim 1, wherein the heat of fusion of the wax is greater than 100 J/g.

### Claim 7 (depends on 1)

The stretch laminate of claim 1, wherein the tackifier is selected from C5 resins, petroleum distillates, hydrogenated hydrocarbons, C5/C9 resins, C9 resins, polyterpenes, rosins, hydrogenated rosins, rosin esters and mixtures there.

### Claim 8 (depends on 1)

The stretch laminate of claim 1, wherein the hot melt adhesive has a loss modulus (G″) of at least about 5×104 Pascal at 40° C., 10 rad/s.

### Claim 9 (depends on 1)

The stretch laminate of claim 1, wherein the hot melt adhesive has a Brookfield melt viscosity of about 6,000 to about 20,000 cps at 160° C., measured with spindle #27 in accordance with ASTM 3236-88.

### Claim 10 (depends on 1)

The stretch laminate of claim 1, wherein the percent change between the initial bond strength and the aged bonded strength is less than about 15%, wherein the initial bond strength is measured at 23° C. within 24 hours of the stretch laminate formation, and wherein the aged bond strength is measured at 23° C. after aging the stretch laminate for 4 weeks at 40° C.

### Claim 11 (depends on 10)

The stretch laminate of claim 10, wherein the percent change between the initial bond strength and the aged bond strength is less than about 10%.

### Claim 12 (depends on 1)

The stretch laminate of claim 1, wherein the hot melt adhesive is characterized by a time to reach tan δ=1 of less than 100 seconds.

### Claim 13 (depends on 1)

The stretch laminate of claim 1, wherein the adhesive is characterized by a crossover temperature in the melt region of greater than 75° C.

### Claim 14 (depends on 1)

The stretch laminate of claim 1, wherein the stretch laminate is a back ear laminate.

### Claim 15 (depends on 1)

An absorbent article comprising the stretch laminate of claim 1.

### Claim 16 (depends on 15)

The absorbent article of claim 15, wherein the stretch laminate is a back ear laminate.

### Claim 17 (depends on 1)

The absorbent article of claim 1, wherein the stretch laminate is mechanically activated.

### Claim 18 (depends on 1)

The absorbent article of claim 1, wherein the substrates are a first nonwoven and a second nonwoven, and the elastic film is adhesively bonded between the first and second nonwoven.

### Claim 19

A mechanically activated stretch laminate comprising:
a first nonwoven, a second nonwoven, and an elastic film therebetween, wherein each of the first and second nonwovens is adhesively bonded to the film by at most about 13 grams/m2 of a hot melt adhesive;
wherein the stretch laminate has:
a) an initial bond strength of at least about 1.0 N; and
b) an initial engineering strain at 9.8 N of at least about 90%; and
c) a percent change between the initial bond strength and the aged bond strength is less than about 15%.

### Claim 20 (depends on 19)

An absorbent article comprising the stretch laminate of claim 19.

### Claim 21

A mechanically activated stretch laminate comprising:
a first nonwoven, a second nonwoven, and an elastic film therebetween, wherein each of the first and second nonwovens is adhesively bonded to the film by a hot melt adhesive;
wherein the hot melt adhesive has:
a) a time to reach tan δ=1 of less than 100 seconds;
b) a loss modulus (G″) of at least about least about 5×104 Pascal at 40° C., 10 rad/s; and
c) a crossover temperature in the melt region greater than 75° C.

### Claim 22 (depends on 21)

An absorbent article comprising the stretch laminate of claim 21.