# US 2016/0254553 A1 · Electrode plate and methods for manufacturing and testing an electrode plate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254553 A1
- Document ID: US20160254553A1
- Status: Published application
- Kind: A1
- Application number: 15/029,275
- Filed: 2014-10-14
- Published: 2016-09-01
- Earliest claimed: 2013-10-15
- Assignees: RedFlow R&D Pty Ltd
- Applicants: Redflow R&D Pty Ltd
- Inventors: Alexander Rudolf WINTER; Thomas JOHN
- Web page: https://patentgrep.com/patent/US20160254553A1

## CPC

- H01M 8/0297: Arrangements for joining electrodes, reservoir layers, heat exchange units or bipolar separators to each other (H01M8/0271 takes precedence)
- G01M 3/20: using special tracer materials, e.g. dye, fluorescent material, radioactive material
- H01M 8/0273: with sealing or supporting means in the form of a frame
- H01M 8/0284: Organic resins; Organic polymers
- H01M 8/0286: Processes for forming seals
- H01M 8/04283: {Supply means of electrolyte to or in matrix-fuel cells}
- H01M 8/188: {by recharging of redox couples containing fluids; Redox flow type batteries}
- H01M 8/20: Indirect fuel cells, e.g. fuel cells with redox couple being irreversible (H01M8/18 takes precedence)
- H01M 8/2484: characterised by external manifolds
- H01M 10/0486: {Frames for plates or membranes}
- H01M 10/365: {Zinc-halogen accumulators}
- H01M 10/4228: {Leak testing of cells or batteries}
- H01M 10/4285: {Testing apparatus}
- H01M 10/4214: {Arrangements for moving electrodes or electrolyte}
- H01M 50/70: Arrangements for stirring or circulating the electrolyte
- Y02E 60/10: Energy storage using batteries
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- G01M: TESTING STATIC OR DYNAMIC BALANCE OF MACHINES OR STRUCTURES; TESTING OF STRUCTURES OR APPARATUS, NOT OTHERWISE PROVIDED FOR
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

An electrode plate, method for manufacturing an electrode plate, and method of testing an electrode plate enable efficient production of robust flowing electrolyte batteries. The method of testing an electrode plate includes forming a frangible portion in the electrode plate; providing a seal around a periphery of the electrode plate, wherein the periphery extends across the frangible portion; applying a gas adjacent a surface on a first side of the electrode plate; and detecting whether there is a presence of the gas adjacent a surface on a second side of the electrode plate, if the electrode plate passes testing, the frangible portion is removed from the electrode plate to define a cut-away region. The electrode plate is then positioned in a battery cell stack including a plurality of other electrode plates. A manifold is then attached to the cell stack adjacent the cut-away region of the electrode plate.

## Claims

### Claim 1

An electrode plate for a flowing electrolyte battery, wherein the electrode plate includes one or more frangible portions.

### Claim 2 (depends on 1)

The electrode plate of claim 1, wherein the one or more frangible portions are located adjacent one or more corners of the electrode plate.

### Claim 3 (depends on 1)

The electrode plate of claim 1, wherein the electrode plate is planar and includes a top surface and a bottom surface.

### Claim 4 (depends on 1)

The electrode plate of claim 1, wherein an edge of a periphery of the bottom surface is substantially flat for sealing against a seal of a test rig.

### Claim 5 (depends on 1)

The electrode plate of claim 1, wherein an interface between at least one of the frangible portions and a remainder of the electrode plate includes a groove.

### Claim 6 (depends on 5)

The electrode plate of claim 5, wherein the groove is formed in a top surface of the electrode plate.

### Claim 7 (depends on 1)

The electrode plate of claim 1, wherein the frangible portions are defined in a polymer frame of the electrode plate.

### Claim 8 (depends on 7)

The electrode plate of claim 7, wherein the polymer is High-Density Polyethylene (HDPE).

### Claim 9

A method of manufacturing an electrode plate for a flowing electrolyte battery, the method comprising:
forming one or more frangible portions in the electrode plate;
removing the one or more frangible portions from the electrode plate to define one or more cut-away regions;
positioning the electrode plate in a battery cell stack; and
attaching one or more manifolds to the battery cell stack adjacent the one or more cut-away regions.

### Claim 10 (depends on 9)

The method of claim 9, wherein the one or more frangible portions are located adjacent one or more corners of the electrode plate.

### Claim 11 (depends on 9)

The method of claim 9, further comprising forming a substantially flat edge along a periphery of a bottom surface of the electrode plate and across the one or more frangible portions.

### Claim 12

A method of testing an electrode plate for a flowing electrolyte battery, the method comprising:
forming one or more frangible portions in the electrode plate;
providing a seal around a periphery of the electrode plate, wherein the periphery extends across the one or more frangible portions;
applying a gas adjacent a surface on a first side of the electrode plate; and
detecting whether there is a presence of the gas adjacent a surface on a second side of the electrode plate.

### Claim 13 (depends on 12)

The method of claim 12, wherein the gas is applied adjacent a top surface of the electrode plate and further comprising evacuating adjacent a bottom surface of the electrode plate.

### Claim 14 (depends on 12)

The method of claim 12, wherein the gas is hydrogen.

### Claim 15 (depends on 13)

The method of claim 13, wherein evacuating adjacent a bottom surface of the electrode plate is performed using a vacuum pump.

### Claim 16 (depends on 12)

The method of claim 12, further comprising:
removing the one or more frangible portions from the electrode plate to define a cut-away region of the electrode plate;
positioning the electrode plate in a battery cell stack including a plurality of other electrode plates; and
attaching a manifold to the cell stack adjacent the cut-away region of the electrode plate.

### Claim 17 (depends on 12)

The method of claim 12, wherein the one or more frangible portions are defined in a High-Density Polyethylene (HDPE) frame of the electrode plate.

### Claim 18 (depends on 12)

The method of claim 12, wherein the one or more frangible portions are formed by defining a groove or a series of indentations in the electrode plate.