# US 2016/0254549 A1 · Metal Supported Solid Oxide Fuel Cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254549 A1
- Document ID: US20160254549A1
- Status: Published application
- Kind: A1
- Application number: 14/992,531
- Filed: 2016-01-11
- Published: 2016-09-01
- Earliest claimed: 2013-09-04
- Assignees: Ceres Intellectual Property Company Limited
- Applicants: Ceres Intellectual Property Company Limited
- Inventors: Robert Leah; Mike Lankin; Robin Pierce; Adam Bone
- Web page: https://patentgrep.com/patent/US20160254549A1

## CPC

- H01M 4/8652: {as mixture}
- C23C 18/02: by thermal decomposition
- H01M 4/8621: {containing only metallic or ceramic material, e.g. made by sintering or sputtering}
- H01M 4/8803: {Supports for the deposition of the catalytic active composition (H01M4/90 takes precedence)}
- H01M 4/8828: {Coating with slurry or ink}
- H01M 4/8885: {Sintering or firing}
- H01M 4/8896: {Pressing, rolling, calendering (membrane electrode assemblies H01M8/1004)}
- H01M 4/9025: {Oxides specially used in fuel cell operating at high temperature, e.g. SOFC}
- H01M 4/9033: {Complex oxides, optionally doped, of the type M1MeO3, M1 being an alkaline earth metal or a rare earth, Me being a metal, e.g. perovskites}
- H01M 8/1213: characterised by the electrode/electrolyte combination or the supporting material
- H01M 8/1226: characterised by the supporting layer
- H01M 8/2425: High-temperature cells with solid electrolytes
- H01M 8/2432: Grouping of unit cells of planar configuration
- H01M 4/8889: {Cosintering or cofiring of a catalytic active layer with another type of layer}
- H01M 2004/8684: {Negative electrodes}
- H01M 2008/1293: {Fuel cells with solid oxide electrolytes}
- Y02E 60/50: Fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A process for forming a metal supported solid oxide fuel cell, the process comprising the steps of: a) applying a green anode layer including nickel oxide, copper oxide and a rare earth-doped ceria to a metal substrate; b) firing the green anode layer to form a composite including oxides of nickel, copper, and a rare earth-doped ceria; c) providing an electrolyte; and d) providing a cathode. Metal supported solid oxide fuel cells comprising an anode a cathode and an electrolyte, wherein the anode includes nickel, copper and a rare earth-doped ceria, fuel cell stacks and uses of these fuel cells.

## Claims

### Claim 1

A process for forming a metal supported solid oxide fuel cell, the process comprising the steps of:
a) applying a green anode layer including nickel oxide, copper oxide and a rare earth-doped ceria to a metal substrate;
b) firing the green anode layer to form a composite including oxides of nickel, copper, and a rare earth-doped ceria;
c) providing an electrolyte; and
d) providing a cathode.

### Claim 2 (depends on 1)

The process according to claim 1, further comprising a step of compressing the green anode layer at pressures in the range 100 to 300 MPa.

### Claim 3 (depends on 1)

The process according to claim 1, wherein the firing of the green anode layer occurs at a temperature in the range 950 to 1100° C.

### Claim 4 (depends on 1)

The process according to claim 1, wherein the nickel oxide, copper oxide and rare earth-doped ceria are powdered, the powders being of particle size distribution d90 in the range 0.1 to 4 μm.

### Claim 5 (depends on 1)

The process according to claim 1, wherein the nickel oxide, copper oxide and rare earth-doped ceria are applied as an ink.

### Claim 6 (depends on 5)

The process according to claim 5, wherein the ink comprises in the range 5 to 50 wt % of the total metal oxide of copper oxide.

### Claim 7 (depends on 6)

The process according to claim 6, wherein the application of the green anode layer includes an initial application of the ink to the metal substrate, and drying the ink to provide a printed layer of thickness in the range 5 to 40 μm.

### Claim 8 (depends on 1)

The process according to claim 1, further comprising heating the printed layer to remove the ink base leaving a green anode layer comprising nickel oxide, copper oxide and a rare earth-doped ceria.

### Claim 9 (depends on 1)

The process according to claim 1, wherein the step of providing an electrolyte occurs before the step of firing the green anode layer, so that the electrolyte and green anode layer are simultaneously fired.

### Claim 10

A metal supported solid oxide fuel cell comprising an anode, a cathode and an electrolyte, wherein the anode includes nickel, copper and a rare earth-doped ceria.

### Claim 11 (depends on 10)

The fuel cell according to claim 10, wherein the nickel, copper and rare earth-doped ceria are sintered.

### Claim 12 (depends on 10)

The fuel cell according to claim 10, wherein a weight ratio of nickel oxide to copper oxide is in the range 20:1 to 4:1.

### Claim 13 (depends on 10)

The fuel cell according to claim 10, wherein the nickel is in a form selected from metallic nickel, nickel oxide, a nickel-copper alloy, a nickel-copper oxide and combinations thereof.

### Claim 14 (depends on 10)

The fuel cell according to claim 10, wherein the copper is in a form selected from metallic copper, copper (II) oxide, copper (I) oxide, a nickel-copper alloy, a nickel-copper oxide and combinations thereof.

### Claim 15 (depends on 10)

The fuel cell according to claim 10, comprising:
(i) a ferritic stainless steel support including a porous region and a non-porous region bounding the porous region;
(ii) a ferritic stainless steel bi-polar plate located under one surface of the porous region of the support and being sealingly attached to the non-porous region of the support about the porous region thereof;
(iii) an anode comprising an anode layer located over the other surface of the porous region of the support;
(iv) an electrolyte comprising an electrolyte layer located over the anode layer; and
(v) a cathode comprising a cathode layer located over the electrolyte layer;
wherein the anode includes nickel, copper and a rare earth-doped ceria.

### Claim 16 (depends on 10)

The fuel cell according to claim 10, wherein the rare earth-doped ceria comprises gadolinium doped cerium oxide.

### Claim 17 (depends on 10)

A fuel cell stack comprising two or more fuel cells according to claim 10.