# US 2016/0254546 A1 · Method of preparing positive electrode material for lithium secondary battery, positive electrode material for lithium secondary battery, and lithium secondary battery including the positive electrode material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254546 A1
- Document ID: US20160254546A1
- Status: Published application
- Kind: A1
- Application number: 14/907,990
- Filed: 2015-09-10
- Published: 2016-09-01
- Earliest claimed: 2014-09-12
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Ick Soon Kwak; Seung Beom Cho; Yeo June Yoon; Sung Wook Mhin
- Web page: https://patentgrep.com/patent/US20160254546A1

## CPC

- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- B01J 13/0047: {containing a metal oxide}
- H01M 4/0402: {Methods of deposition of the material}
- H01M 4/0419: {involving spraying}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0568: characterised by the solutes
- H01M 10/0569: characterised by the solvents
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- H01M 2220/30: Batteries in portable systems, e.g. mobile phone, laptop
- H01M 2300/0028: characterised by the solvent
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y02T 10/70: Energy storage systems for electromobility, e.g. batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

The present invention relates to a method of preparing a positive electrode material for a lithium secondary battery including a first step of synthesizing a lithium transition metal oxide represented by Chemical Formula 1, a second step of preparing lithium transition metal oxide powder by grinding the lithium transition metal oxide, a third step of preparing a positive electrode material including an alumina coating layer by mixing as well as dispersing the lithium transition metal oxide powder in an alumina nanosol, and a fourth step of drying the positive electrode material, a positive electrode material for a lithium secondary battery prepared by the above method, and a lithium secondary battery including the positive electrode material, Li(1+a)(Ni(1−a−b−c)MnbCoc)On [Chemical Formula 1] where 0≦a≦0.1, 0≦b≦1, 0<c≦1, and n is an integer of 2 or 4.

## Claims

### Claim 1

A method of preparing a positive electrode material for a lithium secondary battery, the method comprising steps of:
a first step of synthesizing a lithium transition metal oxide represented by Chemical Formula 1;
a second step of preparing lithium transition metal oxide powder by grinding the lithium transition metal oxide;
a third step of preparing a positive electrode material including an alumina coating layer by mixing as well as dispersing the lithium transition metal oxide powder in an alumina nanosol; and
a fourth step of drying the positive electrode material,
Li(1+a)(Ni(1−a−b−c)MnbCoc)On [Chemical Formula 1]
where 0≦a≦0.1, 0≦b≦1, 0<c≦1, and n is an integer of 2 or 4.

### Claim 2 (depends on 1)

The method of claim 1, wherein the alumina coating layer comprises a γ-alumina phase in an amount of 95 wt % or more based on a total weight of the alumina coating layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the lithium transition metal oxide is Li(Ni0.6Mn0.2Co0.2O2), Li(Ni0.8Mn0.1Co0.1O2), Li(Ni0.5Mn0.3Co0.2O2), Li(Ni1/3Mn1/3Co1/3O2), or LiCoO2.

### Claim 4 (depends on 1)

The method of claim 1, wherein a particle diameter of the lithium transition metal oxide powder ground in the second step is in a range of 10 μm to 30 μm.

### Claim 5 (depends on 1)

The method of claim 1, wherein, in the third step, the lithium transition metal oxide powder and the alumina nanosol are mixed at a weight ratio of 1:80 to 1:100.

### Claim 6 (depends on 1)

The method of claim 1, wherein, in the third step, the lithium transition metal oxide powder is directly dispersed in the alumina nanosol, or
is dispersed after a lithium transition metal oxide powder solution is prepared by spaying the lithium transition metal oxide powder in an organic solvent.

### Claim 7 (depends on 6)

The method of claim 6, wherein the organic solvent is 1-methoxy-2-propanol, ethyl alcohol, methyl alcohol, or isopropyl alcohol.

### Claim 8 (depends on 6)

The method of claim 6, wherein the organic solvent is used in an amount of 70 wt % to 99 wt % based on a total weight of the positive electrode material.

### Claim 9 (depends on 1)

The method of claim 1, wherein the drying of the fourth step is performed in a temperature range of 100° C. to 350° C.

### Claim 10 (depends on 1)

The method of claim 1, further comprising a fifth step of sintering the dried positive electrode material after the fourth step.

### Claim 11 (depends on 10)

The method of claim 10, wherein the sintering of the fifth step is performed in a temperature range of 400° C. to 1200° C.

### Claim 12

A positive electrode material for a secondary battery, the positive electrode material comprising:
lithium transition metal oxide particles represented by Chemical Formula 1; and
an alumina coating layer formed on surfaces of the lithium transition metal oxide particles and including a γ-alumina phase in an amount of 95% or more,
wherein a coverage of the alumina coating layer is in a range of 30% to 50% based on a total surface area of the lithium transition metal oxide particles,
Li(1+a)(Ni(1−a−b−c)MnbCoc)On [Chemical Formula 1]
where 0≦a≦0.1, 0≦b≦1, 0<c≦1, and n is an integer of 2 or 4.

### Claim 13 (depends on 12)

The positive electrode material for a secondary battery of claim 12, wherein a thickness of the alumina coating layer is 30 nm or less.

### Claim 14 (depends on 12)

The positive electrode material for a secondary battery of claim 12, wherein the alumina coating layer has a surface roughness (Ra) of 10 nm over an entire surface.

### Claim 15 (depends on 12)

The positive electrode material for a secondary battery of claim 12, wherein an amount of aluminum in the alumina coating layer is in a range of 5 ppm to 100 ppm based on a total weight of the positive electrode material.

### Claim 16

A positive electrode for a secondary battery, the positive electrode comprising:
a positive electrode material; and
selectively a conductive agent, a binder, and a filler in addition to the positive electrode material,
wherein the positive electrode material comprises lithium transition metal oxide particles represented by Chemical Formula 1; and
an alumina coating layer formed on surfaces of the lithium transition metal oxide particles and including a γ-alumina phase in an amount of 95% or more,
wherein a coverage of the alumina coating layer is in a range of 30% to 50% based on a total surface area of the lithium transition metal oxide particles,
Li(1+a)(Ni(1−a−b−c)MnbCoc)On [Chemical Formula 1]
where 0≦a≦0.1, 0≦b≦1, 0<c≦1, and n is an integer of 2 or 4.

### Claim 17

A lithium secondary battery comprising:
a positive electrode;
a negative electrode;
a separator disposed between the positive electrode and the negative electrode; and
an electrolyte solution,
wherein the positive electrode comprises a positive electrode material represented by Chemical Formula 2,
Li(1+a)(Ni(1−a−b−c)MnbCocM′x)On [Chemical Formula 2]
where 0≦a≦0.1, 0≦b≦1, 0<c≦1, 0<x≦1, n is an integer of 2 or 4, and M′ is Al2O3 having a gamma phase.

### Claim 18 (depends on 17)

The lithium secondary battery of claim 17, wherein the lithium secondary battery has an HF content of 900 ppm or less based on a total weight of the electrolyte solution after an activation process and initial charge and discharge.

### Claim 19 (depends on 17)

The lithium secondary battery of claim 17, wherein the lithium secondary battery has an HF content of 100 ppm or less based on a total weight of the electrolyte solution after 50 charge cycles.

### Claim 20 (depends on 17)

The lithium secondary battery of claim 17, wherein the positive electrode comprises:
lithium transition metal oxide particles represented by Chemical Formula 1; and
an alumina coating layer formed on surfaces of the lithium transition metal oxide particles and including a γ-alumina phase in an amount of 95% or more,
wherein a coverage of the alumina coating layer is in a range of 30% to 50% based on a total surface area of the lithium transition metal oxide particles,
Li(1+a)(Ni(1−a−b−c)MnbCoc)On [Chemical Formula 1]
where 0≦a≦0.1, 0≦b≦1, 0<c≦1, and n is an integer of 2 or 4.

### Claim 21

A method of preparing an alumina nanosol, the method comprising:
mixing alumina nanopowder and a solvent to prepare an alumina nanopowder suspension; and
dispersing the suspension with a bead mill to prepare an alumina nanosol,
wherein the alumina nanosol comprises a γ-alumina phase in an amount of 99% of more.

### Claim 22 (depends on 21)

The method of claim 21, wherein the dispersion of the suspension with the bead mill is performed at a rotation speed of a center of 3,000 rpm.

### Claim 23 (depends on 21)

The method of claim 21, wherein a diameter of beads in the bead mill is in a range of 0.05 mm to 0.1 mm.

### Claim 24 (depends on 21)

The method of claim 21, wherein the solvent is 1-methoxy-2-propanol, ethyl alcohol, methyl alcohol, or isopropyl alcohol.

### Claim 25 (depends on 21)

The method of claim 21, wherein the solvent is used in an amount of 70 wt % to 99 wt % based on a total amount of the alumina nanosol.

### Claim 26 (depends on 21)

The method of claim 21, wherein a particle diameter of the alumina nanopowder is in a range of 1 nm to 50 nm.

### Claim 27 (depends on 21)

The method of claim 21, wherein the alumina nanopowder is γ-alumina nanopowder.

### Claim 28 (depends on 21)

The method of claim 21, wherein the alumina nanosol comprises alumina nanopowder having a particle diameter of 1 nm to 20 nm.