# US 2016/0254544 A1 · LIFePO4 FLAKES FOR LI-ION BATTERY AND METHOD FOR MANUFACTURING THE SAME

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254544 A1
- Document ID: US20160254544A1
- Status: Published application
- Kind: A1
- Application number: 15/152,023
- Filed: 2016-05-11
- Published: 2016-09-01
- Earliest claimed: 2011-06-22
- Assignees: National Tsing Hua University
- Applicants: National Tsing Hua University
- Inventors: Lih-Hsin CHOU; Kuei-Chao WU
- Web page: https://patentgrep.com/patent/US20160254544A1

## CPC

- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C01B 25/45: containing plural metal, or metal and ammonium
- C01G 49/0027: {containing one alkali metal}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2220/30: Batteries in portable systems, e.g. mobile phone, laptop
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

LiFePO4 flakes for a Li-ion battery and a method for manufacturing the same are disclosed. The LiFePO4 flakes of the present invention have a thickness of 5 nm-200 nm, and the angle between the flat surface normal of the flake and the Li-ion diffusion channel is 0°-80°. In addition, according to the present invention, the LiFePO4 flakes with short Li ion diffusion path can be prepared through a simple process. Hence, not only the charge-discharge efficiency of the Li-ion battery can be improved by use of the LiFePO4 flakes of the present invention, but also the cost of the Li-ion battery can be further reduced.

## Claims

### Claim 1

A method for manufacturing LiFePO4 flakes for a Li-ion battery, comprising the following steps:
(A) providing a mixed organic solution by reflux, which comprises Li, Fe, and P, wherein the Li contained in the mixed organic solution is derived from a Li-containing precursor or a P and Li-containing precursor, the Fe contained in the mixed organic solution is derived from an Fe-containing precursor or a P and Fe-containing precursor, and the P contained in the mixed solution is derived from a P-containing precursor, a P and Li-containing precursor, or a P and Fe-containing precursor;
(B) heating the organic mixed solution to obtain preliminary products; and
(C) heat-treating the preliminary products to obtain LiFePO4 flakes.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the organic mixed solution is heated under an atmosphere or with an introduced gas flow to obtain the preliminary products, in step (B).

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the preliminary products are heat-treated under an atmosphere or with an introduced gas flow to obtain the LiFePO4 flakes, in step (C).

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the Li-containing precursor is at least one selected from the group consisting of LiOH, Li2CO3, LiNO3, CH3COOLi, Li2C2O4, Li2SO4, LiCl, LiBr, and LiI.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the Fe-containing precursor is at least one selected from the group consisting of FeCl2, FeBr2, FeI2, FeSO4, (NH4)2Fe(SO4)2, Fe(NO3)2, FeC2O4, (CH3COO)2Fe, and FeCO3.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein the P-containing precursor is at least one selected from the group consisting of H3PO4, NaH2PO4, Na2HPO4, Mg3(PO4)2, and NH4H2PO4.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the P and Li-containing precursor is at least one selected from the group consisting of LiH2PO4, Li2HPO4, and Li3PO4.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein the P and Fe-containing precursor is at least one selected from the group consisting of Fe3(PO4)2, and FePO4.

### Claim 9 (depends on 1)

The method as claimed in claim 1, wherein the mixed organic solution further comprises: at least one selected from the group consisting of a surfactant, a polymer electrolyte, and a stabilizer.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein an organic solvent in the mixed organic solution is at least one selected from the group consisting of ethylene glycol (EG), diethylene glycol (DEG), glycerol, triethylene glycol (TEG), tetraethylene glycol (TTEG), polyethylene glycol (PEG), Dimethyl sulfoxide (DMSO), and N,N-dimethylmethanamide (DMF).

### Claim 11 (depends on 2)

The method as claimed in claim 2, wherein the atmosphere or the introduced gas flow comprises one selected from the group consisting of N2, He, Ne, Ar, Kr, Xe, CO, methane, N2—H2 mixed gas, and a mixture thereof.

### Claim 12 (depends on 3)

The method as claimed in claim 3, wherein the atmosphere or the introduced gas flow comprises one selected from the group consisting of N2, He, Ne, Ar, Kr, Xe, CO, methane, N2—H2 mixed gas, and a mixture thereof.

### Claim 13 (depends on 9)

The method as claimed in claim 9, wherein the surfactant is Cetyltrimethylammonium bromide (CTAB), sodium dodecylbenzene sulfonate (SDBS), sodium dodecyl sulfate (SDS), or Triton-X100.

### Claim 14 (depends on 9)

The method as claimed in claim 9, wherein the polymer electrolyte is polyvinylpyrollidone (PVP), peroxyacetic acid (PAA), Polyethyleneimine (PEI), or polyacrylamide (PAM).

### Claim 15 (depends on 9)

The method as claimed in claim 9, wherein the stabilizer is Polyvinyl Alcohol (PVA), or polyvinyl acetate (PVAc).

### Claim 16 (depends on 1)

The method as claimed in claim 1, wherein the organic mixed solution is heated to and reacted at 105°-350° C., in step (B).

### Claim 17 (depends on 1)

The method as claimed in claim 1, wherein the organic mixed solution is reacted for 10 hrs-20 hrs.

### Claim 18 (depends on 1)

The method as claimed in claim 1, wherein the preliminary products are heat-treated at 300°-700° C., in step (C).

### Claim 19 (depends on 1)

The method as claimed in claim 1, wherein the preliminary products are heat-treated for 1 hr-20 hrs.

### Claim 20 (depends on 1)

The method as claimed in claim 1, wherein the LiFePO4 flakes have a thickness of 5 nm-200 nm, and an angle between a flat surface normal of the LiFePO4 flakes and a Li-ion diffusion channel is 0°-80°.

### Claim 21 (depends on 1)

The method as claimed in claim 1, wherein the LiFePO4 flakes have olivine structures.