# US 2016/0254540 A1 · Improved lithium metal oxide cathode materials and method to make them

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254540 A1
- Document ID: US20160254540A1
- Status: Published application
- Kind: A1
- Application number: 15/028,081
- Filed: 2014-10-16
- Published: 2016-09-01
- Earliest claimed: 2013-10-24
- Assignees: Dow Global Technologies LLC
- Applicants: Dow Global Technologies LLC
- Inventors: Edward L. Lee; Fu Zhou
- Web page: https://patentgrep.com/patent/US20160254540A1

## CPC

- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- C01G 53/44: containing manganese
- C01G 53/502: containing lithium and cobalt
- C01G 53/82: Compounds containing nickel, with or without oxygen or hydrogen, and containing two or more other elements
- H01B 1/08: oxides
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01P 2002/50: Solid solutions
- C01P 2002/54: one element only
- C01P 2004/03: obtained by SEM
- C01P 2004/32: Spheres
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/11: Powder tap density
- C01P 2006/40: Electric properties
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An improved method of forming a precipitated transition metal salt useful to make a lithium transition metal oxide useful for making a lithium ion battery comprises the following. A transition metal solution comprised of a dissolved transition metal salt in water and an alkali solution comprised of an alkali salt dissolved in water are introduced into a reactor having an inlet and an outlet connected by a tubular member having therein packing. The rate in which said solutions are introduced are such that the pH of the overall solution in the reactor has pH of 5 to 12 and the time of reaction (mere seconds to several minutes) in the reactor is sufficient to form a precipitated transition metal salt in an effluent liquid. The transition metal salt precipitate in the effluent is discharged from the reactor and the salt separated from the effluent, where it can be purified by washing and dried and subsequently heated with a lithium compound to form a lithium metal oxide useful for making lithium ion batteries.

## Claims

### Claim 1

A method of forming a precipitated transition metal salt useful to make a lithium transition metal oxide useful for making a lithium ion battery comprising:
(a) providing (i) a transition metal solution comprised of a dissolved transition metal salt in water, and (ii) an alkali solution comprised of an alkali salt dissolved in water,
(b) providing a reactor having an inlet and an outlet connected by a tubular member having therein packing,
(c) introducing the transition metal solution and alkali solution into the inlet of the plug flow reactor each at a rate to realize a pH (5-12) within the plug flow reactor and a reaction time sufficient to form a precipitated transition metal salt in an effluent liquid;
(d) discharging the precipitated transition metal salt in the effluent liquid from the outlet of the reactor; and
(e) separating the precipitated transition metal salt from the effluent.

### Claim 2 (depends on 1)

The method of claim 1, wherein the transition metal solution is comprised of at least two transition metals dissolved therein.

### Claim 3 (depends on 1)

The method of claim 1, wherein the transition metal solution is comprised of at least three transition metals dissolved therein.

### Claim 4 (depends on 1)

The method of claim 1, wherein the transition metal salts are a sulfate, chlorite, nitrate, fluorite or combination thereof.

### Claim 5 (depends on 1)

The method of claim 1, wherein the method is performed in the absence of ammonium.

### Claim 6 (depends on 1)

The method of claim 1, wherein the plug flow reactor is comprised of two or more plug flow reactors interconnected in series, parallel or a combination thereof.

### Claim 7 (depends on 1)

The method of claim 1, wherein the plug flow reactor is comprised of at least two plug flow reactors interconnected in parallel in which the alkali solution and transition metal solution are separately introduced into the inlet of each said plug flow reactors such that the effluent are combined to make a combined precipitated transition metal salt and the precipitated transition metal salt from each said plug flow reactor has at least one characteristic dissimilar to the precipitated transition metal salt from each of the other plug flow reactors.

### Claim 8 (depends on 7)

The method of claim 7, wherein the combined precipitated transition metal salt has a bimodal size distribution.

### Claim 9 (depends on 1)

The method of claim 1, wherein the packing of the plug flow reactor is comprised of beads.

### Claim 10 (depends on 9)

The method of claim 9, wherein the packing is beads having a bimodal distribution.

### Claim 11 (depends on 6)

The method of claim 6, wherein the beads are packed such that the packing results in a void fraction of the plug flow reactor that is 20% to 60%.

### Claim 12 (depends on 1)

The method of claim 1, wherein the alkali solution, transition metal solution and water are separately pumped into a premixing chamber that is in direct communication with inlet of the plug flow reactor such that said transition metal solution, water, and alkali are contacted with each other prior to introducing into the plug flow reactor.

### Claim 13 (depends on 1)

The method of claim 1, wherein the transition metal solution has a total molar concentration of transition metal salt from 0.1 to 10 M.

### Claim 14 (depends on 1)

The method of claim 1, wherein the alkali solution has a total salt concentration of from 0.1 to 20 M.

### Claim 15 (depends on 1)

The method of claim 1 wherein the temperature of the precipitation is from 10° C. to 90° C.

### Claim 16 (depends on 1)

The method of claim 1, wherein the reaction time is from 5 seconds to 10 minutes.

### Claim 17 (depends on 1)

The method of claim 1, wherein the precipitated transition metal salt has a secondary particle size distribution that is bi-modal.

### Claim 18 (depends on 1)

A method of forming a lithium metal oxide comprising,
(a) mixing the precipitated transition metal oxide of claim 1 with a source of lithium to form a mixture; and
(b) heating the mixture to a temperature and time sufficient to form the lithium metal oxide.

### Claim 19 (depends on 1)

The method of claim 1, wherein the effluent is recycled by introducing the effluent into the plug flow reactor in step (c).

### Claim 20 (depends on 18)

A lithium ion battery comprised of the lithium metal oxide of claim 18.