# US 2016/0254527 A1 · Composite silicon or composite tin particles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254527 A1
- Document ID: US20160254527A1
- Status: Published application
- Kind: A1
- Application number: 15/149,112
- Filed: 2016-05-07
- Published: 2016-09-01
- Earliest claimed: 2012-02-14
- Inventors: Shailesh Upreti
- Web page: https://patentgrep.com/patent/US20160254527A1

## CPC

- H01M 4/366: {as layered products}
- C01B 33/021: Preparation (chemical coating from the vapour phase C23C16/00)
- F02P 3/053: {using digital techniques}
- F02P 3/0554: {using digital techniques (F02P3/0558 takes precedence)}
- F02P 11/02: Preventing damage to engines or engine-driven gearing
- H01M 4/0447: {of complete cells or cells stacks}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/364: {as mixtures}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/387: {Tin or alloys based on tin}
- H01M 4/48: of inorganic oxides or hydroxides
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- F02P: IGNITION, OTHER THAN COMPRESSION IGNITION, FOR INTERNAL-COMBUSTION ENGINES; TESTING OF IGNITION TIMING IN COMPRESSION-IGNITION ENGINES ({anti-pollution means for internal-combustion engines F02B17/00}; specially adapted for rotary-piston or oscillating-piston engines F02B53/12; {ignition of gas turbine plants F02C7/26; ignition of jet propulsion plants F02K9/95; starting of combustion engines F02N9/00}; ignition of combustion apparatus in general, glowing plugs F23Q; measuring of physical variables in general G01; controlling in general G05; data processing in general G06; electrical components in general see Section H; {ignition coils H01F38/12}; sparking plugs H01T13/00)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The specification relates to a composite particle for storing lithium. The composite particle is used in an electrochemical cell. The composite particle includes a metal oxide on the surface of the composite particle, a major dimension that is approximately less than or equal to 40 microns and a formula of MM′Z, wherein M is from the group of Si and Sn, M′ is from a group of Mn, Mg, Al, Mo, Bronze, Be, Ti, Cu, Ce, Li, Fe, Ni, Zn, Co. Zr, K, and Na, and Z is from the group of O, Cl, P, C, S, H, and F.

## Claims

### Claim 1

An electrochemical rechargeable cell comprising: an anode comprising a particulate composite MM′Z, a binder and a solvent, the MM′Z composite being subtractively removed from an alloy in which M content is not dominant in the alloy and a cooling rate from a melt temperature of the alloy was sufficient to allow a formation of a structure having an extended M phase network and a substantially differentiated phase, the MM′Z composite including a portion of the M′ remaining within the structure, the MM′Z composite further including an amorphous component on the surface of the composite, wherein the structure of MM′Z composite particle possesses rods arranged in an array such that the rods are joined crystallographically and extend into space in a manner providing for a space of separation between crystallite extensions thereby accommodating for volume expansion when storing lithium, and wherein M is from the group of Si and Sn, M′ is from a group of Mn, Mg, Al, Mo, Bronze, Be, Ti, Cu, Ce, Li, Fe, Ni, Zn, Co, Zr, K, and Na and Z is from the group of O, Cl, P, C, S, H, and F.

### Claim 2 (depends on 1)

The electrochemical rechargeable cell as claimed in claim 1 wherein the MM′Z composite has (1) at least 10 m2/g of surface area due to an open structure, (2) a total surface area of greater than 20 m2/g, (3) greater than 50% of the composite particle having rods wherein each rod has a length greater than at least 10 times the diameter, and (4) greater than 30% of the rods being oriented in the same crystallographic plane.

### Claim 3 (depends on 1)

The electrochemical rechargeable cell as claimed in claim 1 wherein the MM′Z composite is at least 80-95% M by weight.

### Claim 4 (depends on 1)

The electrochemical rechargeable cell as claimed in claim 1 wherein the MM′Z composite is subtractively removed from the alloy using one or more acids selected from the group consisting of HCl, H2SO4, CH3COOH, H3PO4 and HNO3.

### Claim 5 (depends on 4)

The electrochemical rechargeable cell as claimed in claim 4 wherein the one or more acids selectively texture on surface of the MM′Z composite, create the MZ or M′Z or both on surface of the MM′Z composite.

### Claim 6 (depends on 1)

The electrochemical rechargeable cell as claimed in claim 1 further comprising: a binder inserted into the space of separation between the crystallite extensions of the MM′Z composite.

### Claim 7 (depends on 1)

The electrochemical rechargeable cell as claimed in claim 1 wherein the MM′Z composite is heated at an elevated temperature >100.degree. C. under different atmospheres to increase electrochemical performance of the silicon composite or tin composite.

### Claim 8 (depends on 1)

The electrochemical rechargeable cell as claimed in claim 1 wherein the composite is admixed with a carbon material.

### Claim 9

A method of preparing a composite for storing lithium, the method comprising the steps of: subtractively removing a MM′Z composite particle from an alloy in which M content is not dominant in the alloy and a cooling rate from a melt temperature of the alloy was sufficient to allow a formation of a structure having an extended M phase network and a substantially differentiated phase, the MM′Z composite particle including a portion of the M′ remaining within the structure, the composite particle further including an amorphous component Z on the surface of the MM′Z composite particle, wherein the structure of MM′Z composite particle possesses rods arranged in an array such that the rods are joined crystallographically and extend into space in a manner providing for a space of separation between crystallite extensions thereby accommodating for volume expansion when storing lithium, and wherein M is from the group of Si and Sn, M′ is from a group of Mn, Mg, Al, Mo, Bronze, Be, Ti, Cu, Ce, Li, Fe, Ni, Zn, Co, Zr, K, and Na and Z is from the group of O, Cl, P, C, S, H, and F.

### Claim 10 (depends on 9)

The method as claimed in claim 9 wherein the MM′Z composite particle has (1) at least 10 m2/g of surface area due to an open structure, (2) a total surface area of greater than 20 m2/g, (3) greater than 50% of the composite particle having rods wherein each rod has a length greater than at least 10 times the diameter, and (4) greater than 30% of the rods being oriented in the same crystallographic plane.

### Claim 11

The method as claimed in claim; 9 wherein the MM′Z composite particle is at least 80-95% M by weight.

### Claim 12 (depends on 9)

The method as claimed in claim 9 wherein the MM′Z composite particle is subtractively removed from an alloy using one or more acids selected from the group consisting of HCl, HF, H2SO4, CH3COOH, H3PO4 and HNO3 in a pH controlled environment.

### Claim 13 (depends on 12)

The method as claimed in claim 12 wherein the one or more acids selectively texture a surface of the MM′Z composite particle to create the MZ or M′Z or both on surface of the MM′Z composite particle.

### Claim 14 (depends on 9)

The method as claimed in claim 9 further comprising: a binder inserted into the space of separation between the crystallite extensions of the MM′Z composite particle.

### Claim 15 (depends on 9)

The method as claimed in claim 9 wherein the MM′Z composite particle is heated at an elevated temperatures >100.degree. C. under an inert or reducing or oxidizing atmosphere to increase electrochemical performance of the MM′Z composite particle.

### Claim 16 (depends on 9)

The method as claimed in claim 9 wherein the MM′Z composite particle is mixed with a carbon material.

### Claim 17

An electrochemical rechargeable cell comprising: an anode comprising a particulate composite, a binder and a solvent, the particulate composite having a general formula of MM′Z, wherein M is from the group of Si and Sn, M′ is from a group of Mn, Mg, Al, Mo, Bronze, Be, Ti, Cu, Ce, Li, Fe, Ni, Zn, Co, Zr, K, and Na, and Z is from the group of O, Cl, P, C, S, H, and F, the particulate composite having a surface composition being an oxide, the surface composition being textured, and wherein a major dimension of the particle is less than 100 microns, and wherein at least 2% by weight of M′ is doped into a crystal structure of M, and wherein M is arranged in an array of columns joined by crystallographic alignments with separation between the columns.

### Claim 18 (depends on 17)

The electrochemical rechargeable cell particle of claim 17 wherein a content of the surface composition of the particulate composite is at least 1% (by weight) MZ and/or M′Z.

### Claim 19 (depends on 17)

The electrochemical rechargeable cell particle of claim 17 wherein the electrochemical rechargeable cell is one of lithium ion, sodium ion, lithium sulfur and lithium air.

### Claim 20 (depends on 17)

The electrochemical rechargeable cell particle of claim 17 wherein the particulate composite has M′ dissolved within the crystal structure of M, and has MZ and/or M′Z on the surface.