# US 2016/0254526 A1 · Wet Method for the Production of Thin Films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254526 A1
- Document ID: US20160254526A1
- Status: Published application
- Kind: A1
- Application number: 15/033,618
- Filed: 2014-10-31
- Published: 2016-09-01
- Earliest claimed: 2013-10-31
- Assignees: Prayon; Universite De Liege
- Applicants: Prayon S.A.; Universite De Liege
- Inventors: Dimitri Liquet; Cedric Calberg; David Eskenazi; Carlos Paez; Jean-Paul Pirard; Benoit Heinrichs; Christelle Alie
- Web page: https://patentgrep.com/patent/US20160254526A1

## CPC

- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0409: {by a doctor blade method, slip-casting or roller coating}
- H01M 4/0414: {by screen printing}
- H01M 4/0419: {involving spraying}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/0497: {Chemical precipitation}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/662: {Alloys (collectors of lead alloys H01M4/685)}
- H01M 4/663: {containing carbon or carbonaceous materials as conductive part, e.g. graphite, carbon fibres}
- H01M 4/664: {Ceramic materials}
- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 4/669: {Steels}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method produces thin films. The method includes preparing a solution containing transition metal oxide precursors, a chelating agent, and a polar organic solvent. The solution is agitated to form a sol. The sol is used in the form of the transition metal oxide film. The chelating agent is selected from among di- or tri-aliphatic carboxylic acids, or salts or mixtures thereof. The polar organic solvent has a boiling temperature at atmospheric pressure of less than 150° C.

## Claims

### Claim 28

A method for manufacturing transition metal oxide films of formula AaMbOd, in which:
A is an alkali metal, A advantageously being chosen from the group consisting of Li, Na and K, or their mixtures;
M is a metal or a mixture of metals chosen from the transition metals, M preferably being a transition metal or a mixture of transition metals chosen from the elements of columns 3 to 12 of the periodic table, M advantageously being chosen from the group consisting of Co, Ni, Mn, Fe, Cu, Ti, Cr, V and Zn, and their mixtures;
O is oxygen; and
a, b and d are real numbers higher than 0 and are chosen so as to ensure electroneutrality, said method comprising the following steps:
(A) preparing a solution comprising one or more, preferably two or more than two, precursors containing one or more of the elements A, M and O, a chelating agent and a polar organic solvent having a boiling point at atmospheric pressure below 150° C.;
(B) forming a sol by stirring said solution; and
(C) implementing the sol in the form of said transition metal oxide film,
wherein the chelating agent is chosen from aliphatic dicarboxylic acids comprising 2 to 20 carbon atoms and salts or mixtures thereof, or the chelating agent is a mixture between at least one carboxylic diacid such as defined above and at least one aliphatic tricarboxylic acid comprising 2 to 20 carbon atoms and salts or mixtures thereof, the proportion of said at least one tricarboxylic acid being lower than 30 mol % relative to the total molar amount of said at least one dicarboxylic acid and said at least one tricarboxylic acid in the solution of step a).

### Claim 29 (depends on 28)

The method according to claim 28 wherein the solution prepared in step (a) also comprises a stabilising agent chosen from the group consisting of water or a carboxylic acid comprising 1 to 20 carbon atoms or a salt of said acid or a mixture thereof, the stabilising agent being different from the chelating agent.

### Claim 30 (depends on 28)

The method according to claim 28 wherein said transition metal oxide film prepared is of formula AaMbOd, in which: A is Li; M is chosen from the group consisting of Co, Ni, Mn, Fe, Cu, Ti, Cr, V and Zn; O is oxygen; and a, b and d are real numbers higher than 0 and chosen so as to ensure electroneutrality.

### Claim 31 (depends on 28)

The method according to claim 28 wherein the sol formed in step (b) has a viscosity lower than 0.1 Pa·s.

### Claim 32 (depends on 28)

The method according to claim 28 wherein the chelating agent is chosen from aliphatic carboxylic diacids comprising 2 to 10 carbon atoms, their salts or their mixtures.

### Claim 33 (depends on 28)

The method according to claim 28 wherein the solvent is chosen from methanol, ethanol, propan-1-ol, isopropanol, butanol, pentanol, acetone, butanone, tetrahydrofuran, dimethylformamide, acetonitrile, diethyl ether, dichloromethane, 2-methoxyethanol and ethyl acetate.

### Claim 34 (depends on 28)

The method according to claim 28 wherein said one or more, preferably two or more than two, precursors of step a) are selected from the group consisting of salts or hydroxides of lithium, sodium, potassium, cobalt, nickel, manganese, iron, copper, titanium, chromium, vanadium and zinc and their mixtures.

### Claim 35 (depends on 28)

The method according to claim 28 wherein one or more, preferably two or more than two, precursors of step (a) comprise a first precursor chosen from salts or hydroxides of lithium or sodium, and a second precursor chosen from salts or hydroxides of cobalt, nickel, titanium, chromium or manganese.

### Claim 36 (depends on 28)

The method according to claim 28 wherein the chelating agent is chosen from oxalic acid, succinic acid, adipic acid or salts thereof or their mixtures.

### Claim 37 (depends on 28)

The method according to claim 28 wherein said transition metal oxide film has an average thickness comprised between 0.01 μm and 250 μm.

### Claim 38 (depends on 28)

The method according to claim 28 wherein said transition metal oxide film has a monolayer or multilayer structure, each layer having a thickness comprised between 0.01 and 2.5 μm.

### Claim 39 (depends on 1)

The method according to claim 1 wherein step (C) of the present method comprises steps of:
(C′) depositing one or more layers of said sol on a substrate; and
(C″) preparing said transition metal oxide film by calcinating said one or more layers formed in step (C′).

### Claim 40 (depends on 39)

The method according to claim 39 wherein said substrate comprises carbon, platinum, gold, stainless steel, platinum on silicon, ITO, platinum on a silicon wafer or metal alloys comprising at least two elements selected from nickel, chromium and iron.

### Claim 41 (depends on 40)

The method according to claim 40 wherein the substrate has an Ra roughness lower than 500 nm.

### Claim 42 (depends on 41)

The method according to claim 41 wherein step (C′) is carried out by spin coating, dip coating, spray coating, slide coating, screen printing, inject printing or roll coating.

### Claim 43 (depends on 42)

The method according to claim 42 wherein a heat treatment is carried out at a temperature below 250° C. in order to dry said layers deposited in step (C′), before the calcinating step (C″).

### Claim 44 (depends on 43)

The method according to claim 43 wherein the calcinating step (C″) is carried out at a temperature comprised between 350 and 800° C.

### Claim 45 (depends on 28)

The method according to claim 28 wherein the transition metal oxide film prepared is chosen from the group consisting of LiCoO2, LiMnO2, LiNi0.5Mn1.5O4, LiCr0.5Mn1.5O4, LiCo0.5Mn1.5O4, LiCoMnO4, LiNi0.5Mn0.5O2, LiNi1/3Mn1/3Co1/3O2 3, LiNi0.8Co0.2O2, LiNi0.5Mn1.5-zTizO4, where z is a number between 0 and 1.5, LiMn2O4, LiNiO2, Li4Mn5O12, and Li4Ti5O12, preferably LiNiO2, Li4Mn5O12, LiMn2O4, LiMnO2, LiCoO2 and Li4Ti5O12.

### Claim 46 (depends on 28)

A sol comprising one or more, preferably two or more than two, precursors containing one or more of the elements A, M and O such as defined in claim 28, a polar organic solvent having a boiling point at atmospheric pressure below 150° C., and a chelating agent chosen from aliphatic dicarboxylic acids comprising 2 to 20 carbon atoms.

### Claim 47 (depends on 28)

A sol comprising one or more, preferably two or more than two, precursors containing one or more of the elements A, M and O such as defined in claim 28, a polar organic solvent having a boiling point at atmospheric pressure below 150° C., and a chelating agent comprising a mixture between at least one dicarboxylic acid and at least one tricarboxylic acid or salts thereof, said di- or tricarboxylic acids being aliphatic acids comprising 2 to 20 carbon atoms, the proportion of said at least one tricarboxylic acid being lower than 30 mol % relative to the total molar amount of said at least one dicarboxylic acid and said at least one tricarboxylic acid in the sol.

### Claim 48 (depends on 46)

The sol according to claim 46, comprising a stabilising agent chosen from the group consisting of water or a carboxylic acid comprising 1 to 20 carbon atoms or a salt of said acid or a mixture thereof, the stabilising agent being different from the chelating agent.

### Claim 49 (depends on 48)

The sol according to claim 48, in which the stabilising agent is chosen from water, acetic acid, propanoic acid, butanoic acid or pentanoic acid.

### Claim 50 (depends on 48)

The sol according to claim 48, in which the proportion of stabilising agent in the sol may be comprised between 0.1 and 30% and preferably between 1 and 20% of the amount of sol by weight.

### Claim 51 (depends on 50)

The sol according to claim 50, in which said two or more than two precursors are chosen from a salt or hydroxide of lithium, sodium, potassium, cobalt, nickel, manganese, iron, copper, titanium, chromium, vanadium, zinc and their mixtures; and the chelating agent is a mixture of succinic or adipic acid, the salts or mixtures thereof and the citric acid or salt thereof.

### Claim 52 (depends on 51)

The sol according to claim 51, wherein it has a viscosity lower than 0.1 Pa·s.

### Claim 53 (depends on 52)

The sol according to claim 52, wherein it is homogeneous, said sol preferably not containing particles that are larger than 2 μm in size.

### Claim 54 (depends on 28)

The use of a transition metal oxide film prepared according to claim 28 as an electrode material, preferably a positive electrode material.

### Claim 55 (depends on 28)

The use of a transition metal oxide film prepared according to claim 28 as a material for protecting an electrode material.