# US 2016/0254444 A1 · Magnetic memory with high thermal budget

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254444 A1
- Document ID: US20160254444A1
- Status: Published application
- Kind: A1
- Application number: 15/057,107
- Filed: 2016-02-29
- Published: 2016-09-01
- Earliest claimed: 2015-02-27
- Assignees: Globalfoundries Singapore Pte. Ltd.
- Applicants: GLOBALFOUNDRIES Singapore Pte. Ltd.
- Inventors: Taiebeh TAHMASEBI; Kah Wee GAN; Chim Seng SEET
- Web page: https://patentgrep.com/patent/US20160254444A1

## CPC

- H10N 50/01: Manufacture or treatment
- H10B 61/22: {of the field-effect transistor [FET] type}
- H10N 50/10: Magnetoresistive devices
- H10N 50/80: Constructional details
- H10N 50/85: Materials of the active region
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A magnetic memory having a base layer with a wetting layer and seed layer is disclosed. The wetting layer and seed layer promotes FCC structure along the (111) orientation to improve PMA. The seed layer includes first and second seed layer separated by a surface smoother, such as a surfactant layer. This enhances the smoothness of the seed layer, resulting in smoother interface in the MTJ stack, which leads to improved thermal endurance.

## Claims

### Claim 1

A method of forming a storage unit of a memory cell comprising:
forming a bottom electrode
forming a fixed layer disposed over the bottom electrode, wherein the fixed layer comprises a hard layer disposed over a base layer, the base layer promotes face-centered cubic (FCC) structure along (111) orientation to increase perpendicular magnetic anisotropy, the base layer comprises
a wetting layer,
a seed layer, wherein the seed layer comprises
a first seed layer,
a roughness smoother to improve surface smoothness of the first seed layer, and
a second seed layer formed over the roughness smoother, wherein the roughness smoother improves surface smoothness of the second seed layer, wherein improved surface smoothness of the seed layer improves surface smoothness of the hard layer to improve thermal endurance
forming at least a first tunneling barrier layer over the hard layer;
forming a storage layer over the first tunneling barrier layer; and
forming a top electrode over the storage layer.

### Claim 2 (depends on 1)

The method of claim 1 wherein the hard layer is formed over the seed layer.

### Claim 3 (depends on 2)

The method of claim 2 wherein each of the first and second seed layers includes n bilayers, wherein a bilayer comprises a first layer Y having a thickness t1 and a second layer X having a thickness t2 and the n bilayers of the first or second seed layer is defined by (Yt1/Xt2)n, and wherein a total thickness of the first or second seed layer is equal to (t1+t2)*n.

### Claim 4 (depends on 3)

The method of claim 3 wherein n is about 2-20 and the total thickness of the seed layer which includes the first and second seed layers and the roughness smoother is about 5 nm or less.

### Claim 5 (depends on 3)

The method of claim 3 wherein:
the first layer Y is disposed below the second layer X; and
the first layer Y is a magnetic layer and the second layer X is a non-magnetic layer having a body-centered cubic (BCC) structure along (110) orientation with high recrystallization temperature.

### Claim 6 (depends on 3)

The method of claim 3 wherein the hard layer comprises a synthetic antiferromagnetic (SAF) layer which includes first and second antiparallel (AP) layers separated by a coupling layer.

### Claim 7 (depends on 6)

The method of claim 6 wherein an AP layer of the first and second AP layers comprises a bilayer and the AP layers are configured with a FCC structure along the (111) orientation facilitated by the base layer.

### Claim 8 (depends on 7)

The method of claim 7 wherein the bilayer of the AP layer comprises Co/Ni, CoFe/Ni or CoFeB/Ni.

### Claim 9 (depends on 3)

The method of claim 3 wherein the wetting layer comprises multiple layers which include Mg and layers having a BCC structure along (110) orientation or layers having a hexagonal close packed (HCP) structure along (0002) orientation which together promote the FCC structure along the (111) orientation.

### Claim 10 (depends on 3)

The method of claim 3 wherein the roughness smoother comprises first and second surfactant layers, wherein the first surfactant layer is a layer with small atoms for filling gaps to clean the interface while the second surfactant layer is deposited over the first surfactant layer.

### Claim 11 (depends on 10)

The method of claim 10 wherein the roughness smoother comprises a plasma treatment to improve surface smoothness of the first seed layer.

### Claim 12 (depends on 2)

The method of claim 2 comprising forming a second tunneling barrier layer over the storage layer, wherein the first and second tunneling barrier layers form a dual tunneling barrier storage unit.

### Claim 13 (depends on 3)

The method of claim 3 wherein the base layer further comprises a crystallinity enhancing layer formed between the roughness smoother and the second seed layer.

### Claim 14 (depends on 13)

The method of claim 13 wherein the crystallinity enhancing layer comprises a Mg layer, or layer having a body-centered cubic (BCC) structure along (110) orientation or a hexagonal close packed (HCP) structure along (0002) orientation which enhances crystallinity of the fixed layer to have the FCC structure along the (111) orientation.

### Claim 15

A method of forming a memory cell comprising:
forming a select unit on a substrate, wherein the select unit comprises a transistor having
a first source/drain (S/D) region,
a second S/D region, and
a gate between the first and second S/D regions;
forming a dielectric layer on the substrate covering the select unit, wherein the dielectric layer includes a storage pad coupled to the first S/D region;
forming a storage unit on the storage pad, wherein the storage unit comprises
forming a bottom electrode,
forming a fixed layer disposed over the bottom electrode, wherein the fixed layer comprises a hard layer disposed over a base layer, the base layer promotes face-centered cubic (FCC) structure along (111) orientation to increase perpendicular magnetic anisotropy, the base layer comprises
a wetting layer,
a seed layer, wherein the seed layer comprises
a first seed layer,
a roughness smoother to improve surface smoothness of the first seed layer, and
a second seed layer formed over the roughness smoother,
wherein the roughness smoother improves surface smoothness of the second seed layer, wherein improved surface smoothness of the seed layer improves surface smoothness of the hard layer to improve thermal endurance,
forming at least a first tunneling barrier layer over the hard layer,
forming a storage layer over the first tunneling barrier layer, and
forming a top electrode over the storage layer; and
forming a bitline coupled to the top electrode layer.

### Claim 16

A storage unit of a memory cell comprising:
a bottom electrode;
a fixed layer disposed over the bottom electrode, wherein the fixed layer comprises a hard layer disposed over a base layer, the base layer promotes face-centered cubic (FCC) structure along (111) orientation to increase perpendicular magnetic anisotropy, the base layer comprises
a wetting layer,
a seed layer, wherein the seed layer comprises
a first seed layer,
a roughness smoother to improve surface smoothness of the first seed layer, and
a second seed layer disposed over the roughness smoother, wherein the roughness smoother improves surface smoothness of the second seed layer, wherein improved surface smoothness of the seed layer improves surface smoothness of the hard layer to improve thermal endurance;
at least a first tunneling barrier layer disposed over the hard layer;
a storage layer disposed over the first tunneling barrier layer; and
a top electrode disposed over the storage layer.

### Claim 17 (depends on 16)

The storage unit of claim 16 wherein each of the first and second seed layers includes n bilayers, wherein a bilayer comprises a first layer Y having a thickness t1 and a second layer X having a thickness t2 and the n bilayers of the first or second seed layer is defined by (Yt1/Xt2)n, and wherein a total thickness of the first or second seed layer is equal to (t1+t2)*n.

### Claim 18 (depends on 17)

The storage unit of claim 17 wherein:
the first layer Y is disposed below the second layer X; and
the first layer Y is a magnetic layer and the second layer X is a non-magnetic layer having a body-centered cubic (BCC) structure along (110) orientation with high recrystallization temperature.

### Claim 19 (depends on 17)

The storage unit of claim 17 wherein the wetting layer comprises multiple layers which include Mg and layers having a BCC structure along (110) orientation or layers having a HCP structure along (0002) orientation which together promote the FCC structure along the (111) orientation.

### Claim 20 (depends on 17)

The storage unit of claim 17 wherein the base layer further comprises a crystallinity enhancing layer disposed between the roughness smoother and the second seed layer.