# US 2016/0254439 A1 · Process for making lead zirconate titanate (pzt) layers and/or platinum electrodes and products thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254439 A1
- Document ID: US20160254439A1
- Status: Published application
- Kind: A1
- Application number: 15/061,205
- Filed: 2016-03-04
- Published: 2016-09-01
- Earliest claimed: 2011-10-17
- Assignees: U.S. Army Research Laboratory ATTN: RDRL-LOC-I
- Applicants: U.S. Army Research Laboratory ATTN: RDRL-LOC-I
- Inventors: Daniel M. Potrepka; James R. Mulcahy; Ronald G. Polcawich
- Web page: https://patentgrep.com/patent/US20160254439A1

## CPC

- C23C 14/088: {of the type ABO3 with A representing alkali, alkaline earth metal or Pb and B representing a refractory or rare earth metal}
- C23C 14/185: {by cathodic sputtering}
- C23C 14/5853: {Oxidation}
- C30B 1/02: by thermal treatment, e.g. strain annealing (C30B1/12 takes precedence)
- C30B 1/10: by solid state reactions or multi-phase diffusion
- C30B 23/025: {characterised by the substrate}
- C30B 29/02: Elements
- C30B 29/16: Oxides
- C30B 29/32: Titanates; Germanates; Molybdates; Tungstates
- C30B 29/68: Crystals with laminate structure, e.g. "superlattices"
- H10N 30/05: Manufacture of multilayered piezoelectric or electrostrictive devices, or parts thereof, e.g. by stacking piezoelectric bodies and electrodes
- H10N 30/076: by vapour phase deposition
- H10N 30/079: using intermediate layers, e.g. for growth control
- H10N 30/708: {Intermediate layers, e.g. barrier, adhesion or growth control buffer layers}
- H10N 30/8554: {Lead-zirconium titanate [PZT] based}
- C30B 25/183: {being provided with a buffer layer, e.g. a lattice matching layer}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

A method of making a piezoelectric device comprising providing a deposition chamber, the deposition chamber having reduced pressure therein; loading a substrate into the deposition chamber; sputter depositing hexagonal 001 oriented titanium on the substrate; providing an oxygen anneal to convert 001 oriented titanium into 100 oriented rutile TiO2; sputter depositing a 111 or 100 oriented textured conducting material for use as an electrode; sputter depositing a hexagonal 001 oriented titanium and providing an oxygen anneal in a lead oxide environment to convert 001 oriented titanium into 100 oriented rutile TiO2 or PbxTi1-xO3; sputter depositing textured lead zirconate titanate PbZrxTi1-x03 having an 001 orientation as a piezoelectric layer, and sputter depositing a textured electrode on top of the textured lead zirconate titanate; whereby processing of the layers within the deposition chamber provides minimized exposure to ambient contamination and improved texturing in the resulting films.

## Claims

### Claim 1

A method of making a piezoelectric device comprising:
providing a deposition chamber, the deposition chamber having reduced pressure therein;
loading a substrate into the deposition chamber;
sputter depositing hexagonal 001 oriented titanium on the substrate;
providing an oxygen anneal to convert 001 oriented titanium into 100 oriented rutile TiO2;
sputter depositing a 111 or 100 oriented textured conducting material for use as an electrode;
sputter depositing a hexagonal 001 oriented titanium and providing an oxygen anneal in a lead oxide environment to convert 001 oriented titanium into 100 oriented rutile TiO2 or PbxTi1-xO3;
sputter depositing textured lead zirconate titanate PbZrxTi1-x03 having an 001 orientation as a piezoelectric layer, and
sputter depositing a textured electrode on top of the textured lead zirconate titanate;
whereby processing of the layers within the deposition chamber or chambers provides minimized exposure to ambient contamination and improved texturing in the resulting films.

### Claim 2 (depends on 1)

The method of claim 1 wherein the 111 or 100 textured conducting material is 111 textured platinum which is deposited on the 100-oriented rutile TiO2, and the textured lead zirconate titanate layer is sputter deposited on the 100 oriented rutile TiO2 or PbxTi1-xO3.

### Claim 3 (depends on 1)

The method of claim 1 wherein the oxygen anneal of the hexagonal 001 oriented titanium is conducted in the deposition chamber at a temperature in the range of 500-800° C. with a partial pressure of lead oxide to incorporate lead or lead oxide into the converted 100 oriented rutile TiO2 or PbxTi1-xO3.

### Claim 4 (depends on 1)

The method of claim 1 wherein the deposition chamber is a sealed vacuum deposition chamber containing one or more of lead oxide, argon or oxygen and wherein the chamber interior has a base pressure of less than 10−3 torr.

### Claim 5 (depends on 1)

The method of claim 1 wherein the deposition chamber comprises a series of deposition chambers forming a sealed in-situ containment system comprising a plurality of process modules and a connecting vacuum transfer chamber for substrate load-unload into and out of wafer boats and transfer between chambers; and wherein there is no exposure of the substrate to an environment containing undesirable gases and/or particles from the time of the substrate is loaded to the textured electrode deposition; on top of the textured lead zirconate titanate preferably allowing substrate exposure only to purified Ar or O2 flow or vacuum.

### Claim 6 (depends on 1)

The method of claim 1 wherein the substrate remains in the deposition chamber between and during the sputtering processes, and wherein 111 or 100 textured conducting material is 111 platinum; and wherein the sputter processing of the 111 textured platinum, oriented rutile TiO2 or PbxTi1-xO3, and the textured lead zirconate titanate PbZrxTi1-xO3 within the sealed deposition container minimizes exposure to ambient contamination and improves texturing

### Claim 7 (depends on 6)

The method of claim 6 wherein the sputter depositing of the 001 oriented titanium, the sputter depositing of the 111 or 100 oriented textured conducting material, the sputter depositing of textured lead zirconate titanate, and the sputter depositing of the 100 Pt for use as a top electrode is conducted in the deposition chamber without removal of the substrate from the sealed deposition chamber and without allowing ambient air into the sealed deposition chamber to thereby improve texturing and minimize exposure to ambient contamination.

### Claim 8

A method of making a ferroelectric device comprising
providing at least one sealed container with a vacuum system having at least one input and at least one output;
providing a substrate within the sealed container;
coating the substrate with an amorphous coating;
growing a crystalline textured layer on the amorphous coating;
epitaxially growing a first electrode layer comprising a thin layer of metallic material having a crystal lattice structure; the textured layer and the first electrode layer being in registration;
epitaxially growing a seed layer;
epitaxially growing at least one ferroelectric material layer on the seed layer; the ferroelectric material layer, the seed layer, and first electrode layer being in registration with the preceding layer; the ferroelectric material growth resulting in a high degree of spontaneous and field induced polarization normal to the growth plane;
whereby processing of the layers within the at least one sealed container provides minimized exposure to ambient contamination and improved texturing in the resulting films.

### Claim 9 (depends on 8)

The method of claim 8 wherein the sealed container is a sealed vacuum deposition chamber containing one or more of lead oxide, argon or oxygen and wherein the chamber interior has a base pressure less than 10−3 torr.

### Claim 10 (depends on 8)

The method of claim 8 wherein the substrate remains in the sealed container continuously between and during all of the sputtering depositions and wherein the growing of at least one ferroelectric material layer comprises sputter depositing of a textured lead zirconate titanate layer by bombarding a lead zirconate titanate target positioned above the substrate with atoms such that the lead zirconate titanate falls from the lead zirconate titanate target and forms on the 100 oriented rutile TiO2 or PbxTi1-xO3.

### Claim 11 (depends on 8)

The method of claim 8 further comprising growing a second electrode on the ferroelectric material layer, the second electrode having a thickness in the range of approximately 10 nm to 500 nm and wherein the second electrode comprises one or more of Pt, Ir, Ru, Pd, Ni, Au, Cu, Ag, IrO2, RuO2, LaSrCoO3, SrRuO3, LaNiO3, InSnO2.

### Claim 12 (depends on 8)

The method of claim 8 wherein the step of epitaxially growing at least one ferroelectric layer comprises maintaining the crystal planes within column-like structure of the ferroelectric material substantially parallel to the growth plane to provide optimum spontaneous polarization perpendicular to the growth plane and wherein the granular regions of the seed layer, at least one ferroelectric layer and first electrode are in registration such that the columns in the ferroelectric layer extend from the granular regions of the seed layer, and the granular regions of the seed layer extend from the granular regions of first electrode, and wherein the crystallographic planes within the granular regions and the column-like structures are substantially planar to the growth plane with a tilt of less than or equal to approximately 10 degrees from the growth plane, and wherein the crystal orientation within the ferroelectric material layer is predominately {001}.

### Claim 13

A method of making a piezoelectric device comprising:
providing a deposition chamber, the deposition chamber having reduced pressure therein;
loading a substrate into the deposition chamber;
coating the substrate with an amorphous coating;
growing a crystalline textured layer on the amorphous coating; the textured growth resulting in granular regions;
sputter depositing a 111 textured platinum layer for use as an electrode;
sputter depositing hexagonal 001 oriented Ti and converting it to a 100 oriented TiO2 seed textured layer;
sputter depositing of textured lead zirconate titanate PbZrxTi1-xO3 having an 001 orientation as a piezoelectric, and
sputter depositing an electrode on top of the textured lead zirconate titanate;
whereby in-situ processing of the layers provides minimized exposure to ambient contamination and improved texturing in the resulting films.

### Claim 14 (depends on 13)

The method of claim 13 wherein the textured lead zirconate titanate is sputter deposited on the TiO2 seed textured layer; the TiO2 seed textured layer comprising a Ti layer converted to TiO2 with an anneal in excess of 500° C. within an oxygen environment with a partial pressure of lead oxide.

### Claim 15 (depends on 13)

The method of claim 13 wherein the deposition chamber is a sealed vacuum deposition chamber containing one or more of lead oxide, argon or oxygen and wherein the chamber interior has a base pressure less than 10−3 torr.

### Claim 16 (depends on 13)

The method of claim 13 wherein the sputter depositing comprises DC magnetron sputtering or pulsed DC magnetron sputtering for the titanium and platinum layers and RF magnetron sputtering for the lead zirconate titanate.

### Claim 17 (depends on 13)

The method of claim 13 wherein the crystalline textured layer is formed from one of the group of TiO2, SnO2, MgO, CaO, SrO, FeO, ZnO, NiO, CeO, CoO, TiN, AlN, CrN, BN, GaN, and CaF2.

### Claim 18 (depends on 13)

The method of claim 13 wherein the crystalline textured layer is approximately 1 nm to 300 nm thick and wherein the crystalline textured layer is the result of an oxidation anneal and forms a rutile structure which facilitates the formation of a granular structure and wherein the first electrode layer has a thickness in the range of 10 to 500 nm, and is formed by sputter depositing an epitaxial layer, and wherein the electrode layer material comprises one or more of Pt, Ir, Ru, Pd, Au, Ag, Cu.

### Claim 19 (depends on 13)

The method of claim 13 wherein the crystalline seed layer is one of a textured oxide having perovskite structure and a thickness in the range of 1-200 nm, preferably 20-50 nm and wherein the polycrystalline {001}-textured perovskite seed with RC-FWHM≦100 and wherein the volume of {100}-textured grains is greater than 90% and the volume of {001}/({001}+{100})>80%.

### Claim 20 (depends on 13)

The method of claim 13 wherein the crystalline seed layer comprises one of (PbLa)TiO3, SrTiO3, BaTiO3, PbNiNbO3, Pb(ZrTi)O3, PbYbNbO3, PbScTaO3, or PbTiO3.