# US 2016/0254438 A1 · Piezoelectric thin film, manufacturing method therefor, and piezoelectric element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254438 A1
- Document ID: US20160254438A1
- Status: Published application
- Kind: A1
- Application number: 15/149,519
- Filed: 2016-05-09
- Published: 2016-09-01
- Earliest claimed: 2013-11-29
- Assignees: Murata Manufacturing Co., Ltd.; National Institute of Advanced Industrial Science and Technology
- Applicants: Murata Manufacturing Co., Ltd.; National Institute of Advanced Industrial Science and Technology
- Inventors: KEIICHI UMEDA; Atsushi Honda; Morito Akiyama; Keiko Nishikubo; Toshimi Nagase
- Web page: https://patentgrep.com/patent/US20160254438A1

## CPC

- H10N 30/852: {Composite materials, e.g. having 1-3 or 2-2 type connectivity}
- C23C 14/0036: {Reactive sputtering}
- C23C 14/3414: {Metallurgical or chemical aspects of target preparation, e.g. casting, powder metallurgy}
- C23C 14/3464: {using more than one target (C23C14/56 takes precedence)}
- C23C 16/34: Nitrides {(C23C16/303 takes precedence)}
- H03H 3/02: for the manufacture of piezoelectric or electrostrictive resonators or networks (H03H3/08 takes precedence)
- H03H 9/17: having a single resonator (crystal tuning forks H03H9/21)
- H04R 17/02: Microphones
- H10N 30/076: by vapour phase deposition
- H10N 30/853: Ceramic compositions
- H04R 2307/027: Diaphragms comprising metallic materials
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H03H: IMPEDANCE NETWORKS, e.g. RESONANT CIRCUITS; RESONATORS (waveguides, resonators, lines or other devices of the waveguide type H01P)
- H04R: LOUDSPEAKERS, MICROPHONES, GRAMOPHONE PICK-UPS OR LIKE ACOUSTIC ELECTROMECHANICAL TRANSDUCERS; ELECTRIC HEARING AIDS; PUBLIC ADDRESS SYSTEMS (producing sounds with frequency not determined by supply frequency G10K)

## Abstract

A piezoelectric thin film composed of aluminum nitride and which contains magnesium and 31 to 120 atomic percent of niobium relative to 100 atomic percent of the magnesium, and the total content of the magnesium and the niobium relative to the total sum of contents of the magnesium, the niobium and the aluminum nitride falls within the range of 10 to 67 atomic percent.

## Claims

### Claim 1

A piezoelectric film comprising:
aluminum nitride;
magnesium; and
31 to 120 atomic percent of niobium relative to 100 atomic percent of the magnesium,
wherein a total content of the magnesium and the niobium relative to a total sum of the magnesium, the niobium and the aluminum nitride falls within a range of 10 to 67 atomic percent.

### Claim 2 (depends on 1)

The piezoelectric film according to claim 1, wherein the total content of the magnesium and the niobium falls within the range of 30 to 63 atomic percent.

### Claim 3 (depends on 2)

The piezoelectric film according to claim 2, wherein the piezoelectric film contains 44 to 87 atomic percent of the niobium relative to 100 atomic percent of the magnesium.

### Claim 4 (depends on 1)

The piezoelectric film according to claim 1, wherein the piezoelectric film contains 44 to 87 atomic percent of the niobium relative to 100 atomic percent of the magnesium.

### Claim 5 (depends on 1)

The piezoelectric film according to claim 1, wherein the niobium includes pentavalent niobium and tetravalent niobium.

### Claim 6 (depends on 2)

The piezoelectric film according to claim 2, wherein the niobium includes pentavalent niobium and tetravalent niobium.

### Claim 7 (depends on 3)

The piezoelectric film according to claim 3, wherein the niobium includes pentavalent niobium and tetravalent niobium.

### Claim 8 (depends on 4)

The piezoelectric film according to claim 4, wherein the niobium includes pentavalent niobium and tetravalent niobium.

### Claim 9

A manufacturing method for a piezoelectric film, the method comprising:
providing a first target composed of aluminum;
providing a second target composed of magnesium;
providing a third target composed of niobium; and
using the first target, the second target and the third target in a ternary sputtering method under a nitrogen gas atmosphere to form a piezoelectric film having aluminum nitride; magnesium; 31 to 120 atomic percent of niobium relative to 100 atomic percent of the magnesium; and a total content of the magnesium and the niobium relative to a total sum of the magnesium, the niobium and the aluminum nitride within a range of 10 to 67 atomic percent.

### Claim 10 (depends on 9)

The manufacturing method for a piezoelectric film according to claim 9, further comprising changing a power ratio of the first, second and third targets to form the piezoelectric film.

### Claim 11 (depends on 9)

The manufacturing method for a piezoelectric film according to claim 9, wherein the total content of the magnesium and the niobium falls within the range of 30 to 63 atomic percent.

### Claim 12 (depends on 11)

The manufacturing method for a piezoelectric film according to claim 11, wherein the piezoelectric film contains 44 to 87 atomic percent of the niobium relative to 100 atomic percent of the magnesium.

### Claim 13 (depends on 9)

The manufacturing method for a piezoelectric film according to claim 9, wherein the piezoelectric film contains 44 to 87 atomic percent of the niobium relative to 100 atomic percent of the magnesium.

### Claim 14 (depends on 1)

The manufacturing method for a piezoelectric film according to claim 1, wherein the niobium includes pentavalent niobium and tetravalent niobium.

### Claim 15

A manufacturing method for a piezoelectric film, the method comprising:
providing a unitary target composed of an alloy of aluminum, magnesium and niobium; and
using the unitary target in a unitary sputtering method under a nitrogen gas atmosphere to form a piezoelectric film having aluminum nitride; magnesium; 31 to 120 atomic percent of niobium relative to 100 atomic percent of the magnesium; and a total content of the magnesium and the niobium relative to a total sum of the magnesium, the niobium and the aluminum nitride within a range of 10 to 67 atomic percent.

### Claim 16 (depends on 14)

The manufacturing method for a piezoelectric film according to claim 14, wherein the total content of the magnesium and the niobium falls within the range of 30 to 63 atomic percent.

### Claim 17 (depends on 16)

The manufacturing method for a piezoelectric film according to claim 16, wherein the piezoelectric film contains 44 to 87 atomic percent of the niobium relative to 100 atomic percent of the magnesium.

### Claim 18 (depends on 14)

The manufacturing method for a piezoelectric film according to claim 14, wherein the piezoelectric film contains 44 to 87 atomic percent of the niobium relative to 100 atomic percent of the magnesium.

### Claim 19 (depends on 14)

The manufacturing method for a piezoelectric film according to claim 14, wherein the niobium includes pentavalent niobium and tetravalent niobium.

### Claim 20 (depends on 1)

A piezoelectric element comprising:
a piezoelectric film according to claim 1; and
first and second electrodes in contact with the piezoelectric film.