# US 2016/0254404 A1 · Photovoltaic panel and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254404 A1
- Document ID: US20160254404A1
- Status: Published application
- Kind: A1
- Application number: 15/028,185
- Filed: 2014-10-16
- Published: 2016-09-01
- Earliest claimed: 2013-10-17
- Assignees: Das Energy GmbH
- Applicants: Das Energy GmbH
- Inventors: Christian DRIES; Manfred ZIPPER; Boris KRASNIK; Johann HARTER
- Web page: https://patentgrep.com/patent/US20160254404A1

## CPC

- H10F 19/804: {Materials of encapsulations}
- H10F 19/80: Encapsulations or containers for integrated devices, or assemblies of multiple devices, having photovoltaic cells
- H10F 19/807: {Double-glass encapsulation, e.g. photovoltaic cells arranged between front and rear glass sheets}
- Y02E 10/50: Photovoltaic [PV] energy
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A photovoltaic panel (1) with at least one solar cell (2) covered with a transparent composite material (5a, 5b) at least at a side (3) facing towards the light and an opposite side (4) facing away from the light, wherein the composite material (5a, 5b) is a plastic (7a, 7b) on the basis of an acrylate containing epoxy groups, reinforced with glass fibers (6a, 6b).

## Claims

### Claim 1

A photovoltaic panel (1) with at least one solar cell (2) covered with a transparent composite material (5a, 5b) at least at a side (3) facing towards the light and an opposite side (4) facing away from the light, characterized in that the composite material (5a, 5b) is a plastic (7a, 7b) on the basis of an acrylate containing epoxy groups, reinforced with glass fibers (6a, 6b).

### Claim 2 (depends on 1)

The photovoltaic panel (1) according to claim 1, characterized in that the acrylate containing epoxy groups is glycide methacrylate.

### Claim 3 (depends on 1, 2)

The photovoltaic panel (1) according to claim 1 or 2, characterized in that the glass fibers (6a, 6b) have a filament diameter in the range of 3 to 15 μm, preferably in the range of 6 to 12 μm, and particularly preferred of 9 μm.

### Claim 4 (depends on 3)

The photovoltaic panel (1) according to claim 3, characterized in that the glass fibers (6a) at the side of the at least one solar cell (2) facing towards the light are designed to form a fabric (8a) with a weight in the range of 50 to 300 g/m2, preferably in the range of 100 to 200 g/m2, and particularly preferred in the range of 160 to 165 g/m2.

### Claim 5 (depends on 4)

The photovoltaic panel (1) according to claim 4, characterized in that the fabric (8a) comprises a warp yarn (9a) and a weft yarn (106a) with a yarn count in the range of 30 to 120 tex, preferably in the range of 45 to 100 tex, and particularly preferred in the range of 60 to 70 tex.

### Claim 6 (depends on 3, 4, 5)

The photovoltaic panel (1) according to any of claims 3 to 5, characterized in that the glass fibers (6b) at the side (4) of the at least one solar cell (2) facing away from the light are designed to form a fabric (8b) with a weight in the range of 100 to 600 g/m2, preferably in the range of 200 to 500 g/m2, and particularly preferred of 390 g/m2.

### Claim 7 (depends on 6)

The photovoltaic panel (1) according to claim 6, characterized in that the fabric (8b) comprises a warp yarn (9b) consisting of 1 to 9, preferably 3 to 7, particularly preferred 5, joined yarns with a yarn count in the range of 30 to 120 tex, preferably in the range of 45 to 100 tex, and particularly preferred in the range of 60 to 70 tex, and a weft yarn (10b) with a yarn count in the range of 100 to 450 tex, preferably in the range of 200 to 350 tex, and particularly preferred in the range of 270 to 280 tex.

### Claim 8 (depends on 1, 2, 3, 4, 5, 6, 7)

A method for manufacturing a photovoltaic panel (1) according to any of claims 1 to 7, comprising the steps of:
applying powdered acrylate containing epoxy groups on a first fabric (8a) of glass fibers (6a),
placing at least one solar cell (2) and electrical branch lines (11) connected with the solar cell (2) as well as possible connection lines (12) connecting a plurality of solar cells (2) on the powdered acrylate containing epoxy groups or on a layer (13) of ethylene vinyl acetate applied on the powdered acrylate containing epoxy groups,
placing a second fabric (8b) of glass fibers (6b) on the at least one solar cell (2), the branch lines (11) and the possible connection lines (12),
applying powdered acrylate containing epoxy groups on the second fabric (8b), and
laminating the entire structure.

### Claim 9 (depends on 8)

The method according to claim 8, characterized in that glycidyl methacrylate is applied as an acrylate containing epoxy groups.

### Claim 10 (depends on 9)

The method according to claim 9, characterized in that laminating takes place in a temperature range of 150 to 200° C., at a pressure of up to 500 mbar and under a vacuum of 0 to 300 mbar.

### Claim 11 (depends on 8, 9, 10)

The method according to any of claims 8 to 10, characterized in that the glass fibers (6a, 6b) of the first and second fabrics (8a, 8b) are coated at least partially with a finish (14) as an adhesion agent prior to their placing.

### Claim 12 (depends on 8, 9, 10, 11)

The method according to any of claims 8 to 11, characterized in that the first and second fabrics (8a, 8b) are tempered, after the respective application of the powdered acrylate containing epoxy groups, in a temperature range of 70 to 120° C., preferably in a temperature range of 85 to 110° C., and particularly preferred at 100° C. and at a pressure of up to 500 mbar.

### Claim 13 (depends on 8, 9, 10, 11, 12)

The method according to any of claims 8 to 12, characterized in that powdered acrylate containing epoxy groups is applied on the first and second fabrics (8a, 8b) with a grain size in the range of 10 to 500 μm, preferably in the range of 25 to 100 μm, and particularly preferred in the range of 40 to 50 μm.

### Claim 14 (depends on 8, 9, 10, 11, 12, 13)

The method according to any of claims 8 to 13, characterized in that powdered acrylate containing epoxy groups is applied on the first and second fabrics (8a, 8b) with an optical refraction index substantially equal to that of the glass fibers (6a, 6b) after laminating.