# US 2016/0254399 A1 · Method of manufacturing pattern using trench structure and pattern manufactured thereby, and method of manufacturing solar battery using the manufacturing method and solar battery manufactured thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254399 A1
- Document ID: US20160254399A1
- Status: Published application
- Kind: A1
- Application number: 14/378,228
- Filed: 2014-04-15
- Published: 2016-09-01
- Earliest claimed: 2013-04-15
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Yong-Sung Goo; Joon-Hyung Kim
- Web page: https://patentgrep.com/patent/US20160254399A1

## CPC

- H10F 10/14: Photovoltaic cells having only PN homojunction potential barriers
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 77/211: {for photovoltaic cells}
- Y02E 10/50: Photovoltaic [PV] energy
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02E 70/30: Systems combining energy storage with energy generation of non-fossil origin
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present disclosure provides a method of manufacturing a pattern including: forming a trench structure on a substrate using an inkjet method; filling an interior portion of the trench structure with a filler; and removing the trench structure, and a pattern manufactured using the same, and a method of manufacturing a solar battery using the method of manufacturing a pattern and a solar battery manufactured using the same.

## Claims

### Claim 1

A method of manufacturing a pattern, comprising:
forming a trench structure on a substrate;
filling an interior portion of the trench structure with a filler; and
removing the trench structure,
wherein the trench structure is formed by an inkjet method, using hot melt ink.

### Claim 2 (depends on 1)

The method of claim 1, wherein the trench structure is composed of a plurality of printing patterns for forming a trench structure.

### Claim 3 (depends on 1)

The method of claim 1, wherein a ratio of an internal height to an internal width of the trench structure is 6:1 to 1:10.

### Claim 4 (depends on 1)

The method of claim 1, wherein the hot melt ink is a thermoplastic hot melt ink or an UV curable hot melt ink.

### Claim 5 (depends on 1)

The method of claim 1, wherein the filler includes a conductive material containing one or more selected from a group consisting of silver (Ag), copper (Cu), aluminum (Al), indium tin oxide (ITO), gold (Au), nickel (Ni), carbon nanotubes (CNT) and poly(3,4-ethylenedioxythiophene) (PEDOT), or an insulating material containing one or more selected from a group consisting of acrylate, urethane, polyimide and epoxy resin.

### Claim 6 (depends on 1)

The method of claim 1, wherein the removing of the trench structure includes one or more selected from a group consisting of a thermal treatment process and a solution treatment process.

### Claim 7 (depends on 1)

A pattern manufactured by the method of claim 1.

### Claim 8

A method of manufacturing a solar battery, comprising:
forming a dopant layer on a substrate;
forming a trench structure on the dopant layer;
etching the dopant layer;
filling an interior portion of the trench structure with a filler; and
removing the trench structure,
wherein the trench structure is formed by an inkjet method, using hot melt ink.

### Claim 9 (depends on 8)

The method of claim 8, wherein the trench structure is composed of a plurality of printing patterns for forming a trench structure.

### Claim 10 (depends on 8)

The method of claim 8, wherein a ratio of an internal height to an internal width of the trench structure is 6:1 to 1:10.

### Claim 11 (depends on 8)

The method of claim 8, wherein the hot melt ink is a thermoplastic hot melt ink or an UV curable hot melt ink.

### Claim 12 (depends on 8)

The method of claim 8, wherein the substrate is a silicon wafer.

### Claim 13 (depends on 8)

The method of claim 8, wherein the filler includes a conductive material containing one or more selected from a group consisting of silver (Ag), copper (Cu), aluminum (Al), indium tin oxide (ITO), gold (Au), nickel (Ni), carbon nanotubes (CNT) and poly(3,4-ethylenedioxythiophene) (PEDOT).

### Claim 14 (depends on 8)

The method of claim 8, further comprising: forming a reflection prevention layer on the substrate, after the etching of the dopant layer.

### Claim 15 (depends on 8)

A solar battery manufactured by the method of claim 8.