# US 2016/0254391 A1 · N-type aluminum nitride single-crystal substrate and vertical nitride semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254391 A1
- Document ID: US20160254391A1
- Status: Published application
- Kind: A1
- Application number: 15/028,033
- Filed: 2014-10-15
- Published: 2016-09-01
- Earliest claimed: 2013-10-15
- Assignees: Tokuyama Corporation
- Applicants: Tokuyama Corporation
- Inventors: Toru Kinoshita; Toshiyuki Obata; Toru Nagashima
- Web page: https://patentgrep.com/patent/US20160254391A1

## CPC

- H10D 8/60: Schottky-barrier diodes
- C30B 25/20: the substrate being of the same materials as the epitaxial layer
- C30B 29/403: {AIII-nitrides}
- H10D 8/051: {of Schottky diodes}
- H10D 62/40: Crystalline structures
- H10D 62/53: the imperfections being within the semiconductor body
- H10D 62/60: Impurity distributions or concentrations
- H10D 62/824: comprising only Group III-V materials heterojunctions, e.g. GaN/AlGaN heterojunctions
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10D 62/854: further characterised by the dopants
- H10D 64/64: Electrodes comprising a Schottky barrier to a semiconductor
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2908: {Nitrides}
- H10P 14/3416: {Nitrides}
- H10P 14/3442: {N-type}
- H10P 14/3458: {Monocrystalline}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A vertical nitride semiconductor device includes an n-type aluminum nitride single-crystal substrate having an Si content of 3×1017 to 1×1020 cm−3 and a dislocation density of 106 cm−2 or less. An ohmic electrode layer is formed on an N-polarity side of the n-type aluminum nitride single-crystal substrate.

## Claims

### Claim 1

A n-type aluminum nitride single crystal substrate wherein a Si content is 3×1017 to 1×1020 cm−3, a dislocation density is 106 cm−2 or less, and a thickness is 50 to 500 μm.

### Claim 2 (depends on 1)

A vertical nitride semiconductor device comprising electrode layers on top and bottom of principal planes of the n-type aluminum nitride single crystal substrate as set forth in claim 1.

### Claim 3 (depends on 2)

A vertical Schottky barrier diode comprising an ohmic electrode layer on one principal plane side and a Schottky electrode layer on the other principal plane of the n-type aluminum nitride single crystal substrate in the vertical nitride semiconductor device as set forth in claim 2.

### Claim 4 (depends on 1)

A laminated body stacked with a layer represented by AlXGa1-XN, wherein X is a rational number satisfying 0.3≦X≦0.8 and having a Si content of 1×1018 to 5×1019 cm−3, on at least one principal plane of the n-type aluminum nitride single crystal substrate as set forth in claim 1.

### Claim 5 (depends on 4)

A vertical nitride semiconductor device comprising electrode layers on top and bottom of principal planes of the layered body as set forth in claim 4.

### Claim 6 (depends on 5)

The vertical nitride semiconductor device as set forth in claim 5 wherein one electrode layer on the layer represented by AlXGa1-XN, wherein X is a rational number satisfying 0.3≦X≦0.8 is an ohmic electrode layer.

### Claim 7 (depends on 6)

A vertical Schottky barrier diode wherein one electrode layer on the n-type aluminum nitride single crystal substrate in the vertical nitride semiconductor device as set forth in claim 6 is a Schottky electrode layer.

### Claim 8 (depends on 3)

The vertical Schottky barrier diode as set forth in claim 3 wherein an electric current density is 10−6 Acm−2 or less when a reverse voltage is 100V.

### Claim 9 (depends on 1)

A production method of the n-type aluminum nitride single crystal substrate as set forth in claim 1 comprising: forming a n-type aluminum nitride single crystal layer having a Si content of 1×1017 to 1×1020 cm−3 and a dislocation density of 106 cm−2 or less on an aluminum nitride single crystal seed substrate having a dislocation density of 104 cm−2 or less, and
separating said aluminum nitride single crystal seed substrate and said n-type aluminum nitride single crystal layer to thereby obtaining the n-type aluminum single crystal substrate from said n-type aluminum nitride single crystal layer.

### Claim 10 (depends on 7)

The vertical Schottky barrier diode as set forth in claim 7 wherein an electric current density is 10−6 Acm−2 or less when a reverse voltage is 100V.