# US 2016/0254382 A1 · Integrated circuits with fets having nanowires and methods of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254382 A1
- Document ID: US20160254382A1
- Status: Published application
- Kind: A1
- Application number: 14/633,351
- Filed: 2015-02-27
- Published: 2016-09-01
- Earliest claimed: 2015-02-27
- Assignees: Globalfoundries Inc.
- Applicants: GLOBALFOUNDRIES, Inc.
- Inventors: Jan Hoentschel; Stefan Flachowsky; Gerd Zschaetzsch
- Web page: https://patentgrep.com/patent/US20160254382A1

## CPC

- H10D 30/6211: {having fin-shaped semiconductor bodies integral with the bulk semiconductor substrates}
- H10B 12/056: {the transistor being a FinFET}
- H10B 12/36: {the transistor being a FinFET}
- H10D 30/0194: {the stacked channels having different properties}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/0243: {using dummy structures having essentially the same shapes as the semiconductor bodies, e.g. to provide stability}
- H10D 30/0323: {comprising monocrystalline silicon}
- H10D 30/504: {wherein the stacked channels have different properties}
- H10D 30/62: Fin field-effect transistors [FinFET]
- H10D 30/6219: {characterised by the source or drain electrodes}
- H10D 30/6735: {having gates fully surrounding the channels, e.g. gate-all-around}
- H10D 30/6744: {Monocrystalline silicon}
- H10D 30/6757: {characterised by the structure of the channel, e.g. transverse or longitudinal shape or doping profile (TFTs having channel structures for preventing kink or snapback effects H10D30/6708; TFTs having lightly-doped source or drain extensions H10D30/6715)}
- H10D 30/792: {comprising applied insulating layers, e.g. stress liners}
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/122: {oriented at angles to substrates, e.g. perpendicular to substrates}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D 62/832: being Group IV materials comprising two or more elements, e.g. SiGe
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D 84/0158: {the components including FinFETs}
- H10D 84/0193: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/834: {comprising FinFETs}
- H10D 84/853: {comprising FinFETs}
- H10D 86/011: {comprising FinFETs}
- H10P 14/20: of semiconductor materials
- H10P 14/3211: {Silicon, silicon germanium or germanium}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/38: {characterised by treatments done after the formation of the materials}
- H10P 14/6309: {of silicon in uncombined form, i.e. pure silicon}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Integrated circuits and methods for producing the same are provided. A method for producing an integrated circuit includes forming a stack overlying a substrate. The stack includes a silicon germanium layer and a silicon layer, where the silicon germanium layer has a first germanium concentration. The stack is condensed to produce a second germanium concentration in the germanium layer, where the second germanium concentration is greater than the first germanium concentration. A fin is formed that includes the stack, and a gate is formed overlying the fin.

## Claims

### Claim 1

A method of forming an integrated circuit comprising:
forming a stack overlying a substrate, wherein the stack comprises a silicon germanium layer and a silicon layer, wherein the silicon germanium layer has a first germanium concentration;
condensing the stack to produce a second germanium concentration in the silicon germanium layer, wherein the second germanium concentration is greater than the first germanium concentration;
forming a fin that includes the stack; and
forming a gate overlying the fin.

### Claim 2 (depends on 1)

The method of claim 1 wherein condensing the stack comprises producing the second germanium concentration of from about 70 weight percent to about 90 weight percent germanium based on the total weight of the silicon germanium layer.

### Claim 3 (depends on 2)

The method of claim 2 wherein condensing the stack comprises increasing a germanium concentration from the first germanium concentration of about 20 to about 50 weight percent based on the total weight of the silicon germanium layer to the second germanium concentration.

### Claim 4 (depends on 1)

The method of claim 1 wherein condensing the stack comprises heating the stack to about 900 to about 1,100 degrees centigrade for about 0.5 to about 1.5 hours.

### Claim 5 (depends on 1)

The method of claim 1 wherein forming the gate overlying the fin comprises forming a replacement metal gate overlying the fin; the method further comprising
forming a source and a drain electrically coupled to the silicon germanium layer in the fin.

### Claim 6 (depends on 5)

The method of claim 5 further comprising:
forming an interface insulating layer before forming the replacement metal gate, wherein the interface insulating layer is positioned between the fin and the replacement metal gate.

### Claim 7 (depends on 6)

The method of claim 6 further comprising:
forming a gate dielectric layer overlying the interface insulating layer such that the gate dielectric layer is positioned between the interface insulating layer and the replacement metal gate.

### Claim 8 (depends on 1)

The method of claim 1 further comprising:
forming a nanowire insulator from the silicon layer.

### Claim 9 (depends on 8)

The method of claim 8 wherein forming the nanowire insulator comprises oxidizing silicon in the silicon layer to form silicon dioxide.

### Claim 10 (depends on 1)

The method of claim 1 wherein condensing the stack comprises condensing the stack in an oxygen ambient.

### Claim 11 (depends on 1)

The method of claim 1 further comprising:
inducing a compressive strain on the silicon germanium layer.

### Claim 12

A method of fabricating a nanowire comprising:
epitaxially forming a stack over a substrate, wherein the stack comprises a silicon germanium layer and a silicon layer, and wherein the silicon germanium layer has a first silicon germanium layer volume;
condensing the stack to produce a second silicon germanium layer volume less than the first silicon germanium layer volume; and
forming a nanowire from the silicon germanium layer.

### Claim 13 (depends on 12)

The method of claim 12 wherein condensing the stack comprises changing a first germanium concentration before condensing the stack to a second germanium concentration after condensing the stack in the silicon germanium layer, wherein the first germanium concentration is from about 20 to about 50 weight percent germanium, and the second germanium concentration is from about 70 weight percent to about 90 weight percent germanium.

### Claim 14 (depends on 12)

The method of claim 12 wherein condensing the stack comprises:
migrating silicon from the silicon germanium layer into the silicon layer.

### Claim 15 (depends on 14)

The method of claim 14 wherein the silicon layer has a first silicon layer volume before condensing the stack, and wherein condensing the stack comprises:
producing a second silicon layer volume after condensing the stack that is larger than the first silicon layer volume.

### Claim 16 (depends on 12)

The method of claim 12 further comprising:
forming a fin, wherein the fin comprises the nanowire formed from the silicon germanium layer and the fin comprises the silicon layer, wherein the silicon layer comprises silicon dioxide after condensing the stack; and
forming a replacement metal gate overlying the fin.

### Claim 17 (depends on 16)

The method of claim 16 further comprising:
forming an interface insulating layer overlying the fin; and
forming a gate dielectric layer overlying the interface insulating layer such that the gate dielectric layer is positioned between the interface insulating layer and the replacement metal gate.

### Claim 18 (depends on 12)

The method of claim 12 wherein condensing the stack comprises condensing the stack at a temperature of from about 900 to about 1,100 degrees centigrade.

### Claim 19 (depends on 12)

The method of claim 12 further comprising:
inducing a compressive strain on the nanowire.

### Claim 20

An integrated circuit comprising:
a fin;
a gate overlying the fin;
a nanowire within the fin, wherein the nanowire comprises germanium with a germanium concentration of from about 70 weight percent to about 90 weight percent;
a nanowire insulator overlying the nanowire, wherein the nanowire insulator comprises silicon dioxide; and
a gate dielectric layer between the fin and the gate.