# US 2016/0254381 A1 · Modulating Germanium Percentage in MOS Devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254381 A1
- Document ID: US20160254381A1
- Status: Published application
- Kind: A1
- Application number: 15/152,260
- Filed: 2016-05-11
- Published: 2016-09-01
- Earliest claimed: 2013-08-09
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Tsz-Mei Kwok; Kun-Mu Li; Hsueh-Chang Sung; Chii-Horng Li; Tze-Liang Lee
- Web page: https://patentgrep.com/patent/US20160254381A1

## CPC

- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 30/0213: {providing different silicide thicknesses on gate electrodes and on source regions or drain regions}
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10D 30/0275: {forming single crystalline semiconductor source or drain regions resulting in recessed gates, e.g. forming raised source or drain regions}
- H10D 30/601: {having lightly-doped drain or source extensions, e.g. LDD IGFETs or DDD IGFETs (lightly doped source or drain extensions for TFTs H10D30/6715)}
- H10D 30/608: {having non-planar bodies, e.g. having recessed gate electrodes}
- H10D 62/021: {Forming source or drain recesses by etching e.g. recessing by etching and then refilling}
- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D 62/83: being Group IV materials, e.g. B-doped Si or undoped Ge
- H10D 62/834: further characterised by the dopants
- H10D 64/01: Manufacture or treatment
- H10D 64/0112: {using conductive layers comprising silicides}
- H10D 64/01125: {the silicides being formed by chemical reaction with the semiconductor after the contact hole formation}
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D 64/259: {Source or drain electrodes being self-aligned with the gate electrode and having bottom surfaces higher than the interface between the channel and the gate dielectric}
- H10D 64/62: Electrodes ohmically coupled to a semiconductor
- H10D 84/0133: {Manufacturing common source or drain regions between multiple IGFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/83: of only insulated-gate FETs [IGFET]
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/414: {of metal-silicide materials}
- H10P 50/642: {Chemical etching}
- H10D 30/0212: {using self-aligned silicidation}
- H10P 50/242: {of Group IV materials}
- H10P 50/644: {Anisotropic liquid etching (H10P50/61 takes precedence)}
- H10P 50/695: {characterised by the process involved to create the mask, e.g. lift-off masks or sidewalls or to modify the mask}
- H10W 20/033: {in openings in dielectrics}
- H10W 20/047: {by introducing additional elements therein}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

An integrated circuit structure includes a gate stack over a semiconductor substrate, and an opening extending into the semiconductor substrate, wherein the opening is adjacent to the gate stack. A first silicon germanium region is disposed in the opening, wherein the first silicon germanium region has a first germanium percentage. A second silicon germanium region is overlying the first silicon germanium region, wherein the second silicon germanium region has a second germanium percentage higher than the first germanium percentage. A metal silicide region is over and in contact with the second silicon germanium region.

## Claims

### Claim 1

An integrated circuit structure comprising:
a semiconductor substrate;
a recess in the semiconductor substrate;
a first silicon germanium region substantially filling the recess and having a topmost surface extending above a topmost surface of the substrate, wherein the first silicon germanium region has a first germanium percentage;
a second silicon germanium region on the topmost surface of the first silicon germanium region, wherein the second silicon germanium region has a second germanium percentage higher than the first germanium percentage; and
a metal silicide above and extending partly into the second silicon germanium region.

### Claim 2 (depends on 1)

The integrated circuit of claim 1, wherein the first germanium percentage is from about 30 percent to about 60 percent and wherein the second germanium percentage is from about 35 percent to about 80 percent.

### Claim 3 (depends on 1)

The integrated circuit of claim 1, wherein the first silicon germanium region further includes impurities at an impurity concentration of from about 5E18/cm3 to about 5E21/cm3.

### Claim 4 (depends on 3)

The integrated circuit of claim 3, wherein the impurities are boron.

### Claim 5 (depends on 1)

The integrated circuit of claim 1, wherein the metal silicide has a substantially cup shaped form.

### Claim 6 (depends on 1)

The integrated circuit of claim 1, wherein the germanium percentage in the first silicon germanium region is substantially uniform through the first silicon germanium region.

### Claim 7 (depends on 1)

The integrated circuit of claim 1, wherein the germanium percentage in the first silicon germanium region gradually and continuously changes through the first silicon germanium region.

### Claim 8

An integrated circuit structure comprising:
a semiconductor substrate;
a gate stack over the semiconductor substrate; and
a source region adjacent a first side of the gate stack, the source region including:
a first silicon germanium region having a first germanium percentage, the first silicon germanium region extending into the semiconductor substrate and having a topmost surface extending to at least a topmost surface of the semiconductor substrate;
a second silicon germanium region on the first silicon germanium region, the second silicon germanium region having a second germanium percentage higher than the first germanium percentage; and
a metal silicide above and extending partly into the second silicon germanium region.

### Claim 9 (depends on 8)

The integrated circuit of claim 8, further comprising:
a drain region adjacent a second side of the gate stack, the drain region including:
a third silicon germanium region having a third germanium percentage equal to the first germanium percentage; and
a fourth silicon germanium region having a fourth germanium percentage equal to the second germanium percentage; and
a second metal silicide above and extending partly into the fourth silicon germanium region.

### Claim 10 (depends on 8)

The integrated circuit of claim 8, further comprising:
a cap layer formed atop the second silicon germanium region, wherein the metal silicide extends through an opening in the cap layer.

### Claim 11 (depends on 8)

The integrated circuit of claim 8, further including a cap layer on the second silicon germanium region, wherein the cap layer is substantially free of germanium.

### Claim 12 (depends on 11)

The integrated circuit of claim 11, wherein the cap layer has an annular shape surrounding the metal silicide when viewed from a top down perspective.

### Claim 13 (depends on 8)

The integrated circuit of claim 8, wherein the first germanium percentage is from about 30 percent to about 60 percent and wherein the second germanium percentage is from about 35 percent to about 80 percent.

### Claim 14 (depends on 8)

The integrated circuit of claim 8, wherein the first silicon germanium region further includes impurities at an impurity concentration of from about 5E18/cm3 to about 5E21/cm3.

### Claim 15 (depends on 14)

The integrated circuit of claim 14, wherein the impurities are boron.

### Claim 16 (depends on 8)

The integrated circuit of claim 8, wherein the first silicon germanium region fills a hole in the semiconductor substrate and wherein sidewalls of the hole comprises facets along planes of the semiconductor crystal structure.

### Claim 17 (depends on 8)

The integrated circuit of claim 8, wherein the second silicon germanium region abuts a gate spacer of the gate stack.

### Claim 18

A method of forming an integrated circuit comprising:
forming a dummy gate stack;
etching a source recess and a drain recess adjacent respective sides of the dummy gate stack;
epitaxially growing a first silicon germanium layer in the source recess and in the drain recess, the first silicon germanium layer having a first germanium percentage;
epitaxially growing a second silicon germanium layer on the first silicon germanium layer in the source recess and the drain recess, the second silicon germanium layer having a second germanium percentage higher than the first germanium percentage;
forming a cap layer over the second silicon germanium layer; and
forming a metal over a portion of the cap layer; and
siliciding the cap layer and a portion of the second silicon germanium layer to form a silicide region over the source recess and over the drain recess, respectively.

### Claim 19 (depends on 18)

The method of claim 18, further comprising removing the dummy gate stack and forming in its place an operative gate stack.

### Claim 20 (depends on 18)

The method of claim 18, further comprising forming a source contact plug contacting the silicide region over the source recess and forming a drain contact plug contacting the silicide region over the drain recess.