# US 2016/0254374 A1 · Semiconductor device and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254374 A1
- Document ID: US20160254374A1
- Status: Published application
- Kind: A1
- Application number: 15/006,164
- Filed: 2016-01-26
- Published: 2016-09-01
- Earliest claimed: 2015-02-27
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Applicants: Toyota Jidosha Kabushiki Kaisha
- Inventors: Satoru KAMEYAMA; Shinya IWASAKI
- Web page: https://patentgrep.com/patent/US20160254374A1

## CPC

- H10D 12/481: {having gate structures on slanted surfaces, on vertical surfaces, or in grooves, e.g. trench gate IGBTs}
- H10D 8/00: Diodes (variable-capacitance diodes H10D1/64; gated diodes H10D12/00)
- H10D 8/01: Manufacture or treatment
- H10D 12/038: {having a recessed gate, e.g. trench-gate IGBTs}
- H10D 62/128: {Anode regions of diodes}
- H10D 62/133: {Emitter regions of BJTs}
- H10D 62/137: {Collector regions of BJTs}
- H10D 62/142: {Anode regions of thyristors or collector regions of gated bipolar-mode devices}
- H10D 62/393: {Body regions of DMOS transistors or IGBTs (cell layout of DMOS H10D62/127)}
- H10D 62/53: the imperfections being within the semiconductor body
- H10D 84/811: {Combinations of field-effect devices and one or more diodes, capacitors or resistors}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/208: {of electrically inactive species}
- H10P 34/40: with high-energy radiation
- H10D 8/422: {PN diodes having the PN junctions in mesas}
- H10D 64/117: {Recessed field plates, e.g. trench field plates or buried field plates}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor device includes a semiconductor substrate that includes an IGBT region. A first lifetime control layer extending along a planar direction of the semiconductor substrate is provided in a range in a drift region that is closer to the rear surface than an intermediate portion of the semiconductor substrate in a thickness direction. A crystal defect density in the first lifetime control layer is higher than any of a crystal defect density in a region adjacent to the first lifetime control layer on the rear surface side and a crystal defect density in a region adjacent to the first lifetime control layer on a front surface side. A crystal defect density in a region between the first lifetime control layer and the rear surface is lower than a crystal defect density in a region between the first lifetime control layer and the front surface.

## Claims

### Claim 1

A semiconductor device, comprising a semiconductor substrate that includes an IGBT region,
wherein
the semiconductor substrate includes a front surface and a rear surface,
the IGBT region comprises:
an emitter region being of n-type and exposed on the front surface;
a body region being of p-type and in contact with the emitter region;
a drift region being of n-type, located on a rear surface side with respect to the body region, and separated from the emitter region by the body region; and
a collector region being of p-type, located on the rear surface side with respect to the drift region, separated from the body region by the drift region, and exposed on the rear surface,
a gate electrode is located so as to face, via a gate insulating film, a part of the body region in a range separating the emitter region from the drift region,
a first lifetime control layer extending along a planar direction of the semiconductor substrate is provided in a range in the drift region that is closer to the rear surface than an intermediate portion of the semiconductor substrate in a thickness direction of the semiconductor substrate,
a crystal defect density in the first lifetime control layer is higher than any of a crystal defect density in a region adjacent to the first lifetime control layer on the rear surface side and a crystal defect density in a region adjacent to the first lifetime control layer on a front surface side, and
a crystal defect density in a region between the first lifetime control layer and the rear surface is lower than a crystal defect density in a region between the first lifetime control layer and the front surface.

### Claim 2 (depends on 1)

The semiconductor device of claim 1, wherein
a second lifetime control layer extending along the planar direction of the semiconductor substrate is provided in a range in the drift region that is closer to the front surface than the first lifetime control layer, and
a crystal defect density in the second first lifetime control layer is higher than any of a crystal defect density in a region adjacent to the second lifetime control layer on the rear surface side and a crystal defect density in a region adjacent to the second lifetime control layer on the front surface side.

### Claim 3 (depends on 1)

The semiconductor device of claim 1, wherein
the drift region comprises:
a low density drift region; and
a buffer region located between the low density drift region and the collector region and including an n-type impurity density ten or more times higher than an n-type impurity density in the low density drift region, and
the first lifetime control layer is provided in the low density drift region.

### Claim 4 (depends on 1)

The semiconductor device of claim 1, wherein
the semiconductor substrate comprises a diode region, and
the diode region comprises an anode region being of p-type and exposed on the front surface,
the drift region is in contact with the anode region and exposed on the rear surface in the diode region, and
the first lifetime control layer is distributed across the IGBT region and the diode region.

### Claim 5

A method for manufacturing a semiconductor device, the method comprising:
implanting charged particles into a semiconductor substrate comprising an n-type drift region so as to form a first lifetime control layer in the n-type drift region, wherein the semiconductor substrate includes a front surface and a rear surface, the charged particles are implanted from a front surface side, and a crystal defect density is increased in the first lifetime control layer;
forming an emitter region, a body region, and a gate electrode in a range closer to the front surface than the first lifetime control layer; and
forming a collector region in a range closer to the rear surface than the first lifetime control layer,
wherein
the emitter region is of n-type and exposed on the front surface,
the body region is of p-type, is in contact with the emitter region, and separates the emitter region from the n-type drift region,
the gate electrode faces, via a gate insulating film, a part of the body region in a range separating the emitter region from the n-type drift region,
the collector region is of p-type, located on a rear surface side with respect to the n-type drift region, separated from the body region by the n-type drift region, and exposed on the rear surface, and
the first lifetime control layer is located in a range closer to the rear surface than an intermediate portion of the semiconductor substrate in a thickness direction of the semiconductor substrate.

### Claim 6 (depends on 5)

The method of claim 5, further comprising polishing the rear surface so as to thin the semiconductor substrate after the formation of the first lifetime control layer so that a semiconductor layer remains in the range closer to the rear surface than the first lifetime control layer,
wherein the collector region is formed in the semiconductor layer remaining in the range closer to the rear surface than the first lifetime control layer in the formation of the collector region.

### Claim 7 (depends on 5)

The method of claim 5, further comprising implanting charged particles into the semiconductor substrate from the front surface side so as to form a second lifetime control layer in which a crystal defect density is increased, the second lifetime control layer being formed in a range in the n-type drift region that is closer to the front surface than the first lifetime control layer.

### Claim 8 (depends on 5)

The method of claim 5, further comprising forming a buffer region in a range in the n-type drift region that is closer to the rear surface than the first lifetime control layer, wherein the buffer region includes an n-type impurity density ten or more times higher than an n-type impurity density in the original n-type drift region.

### Claim 9 (depends on 5)

The method of claim 5, further comprising forming an anode region being of p-type in a range in the semiconductor substrate that is closer to the front surface than the first lifetime control layer so that the anode region is exposed on the front surface, the n-type drift region is in contact with the anode region, and the n-type drift region is exposed on the rear surface at a position on the rear surface side with respect to the anode region.