# US 2016/0254372 A1 · Semiconductor device manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254372 A1
- Document ID: US20160254372A1
- Status: Published application
- Kind: A1
- Application number: 15/031,623
- Filed: 2013-12-13
- Published: 2016-09-01
- Earliest claimed: 2013-12-13
- Assignees: Mitsubishi Electric Corporation
- Applicants: Mitsubishi Electric Corporation
- Inventors: Yusuke KAWASE; Kazunori KANADA; Tadaharu MINATO
- Web page: https://patentgrep.com/patent/US20160254372A1

## CPC

- H10D 12/441: {Vertical IGBTs}
- H10D 12/032: {of vertical IGBTs}
- H10D 62/137: {Collector regions of BJTs}
- H10P 30/2044: {into semiconducting carbon, e.g. diamond or semiconducting diamond-like carbon}
- H10P 30/212: {Through-implantation}
- H10P 30/222: {characterised by the angle between the ion beam and the crystal planes or the main crystal surface (characterised by the angle between the ion beam and the mask H10P30/221)}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10D 62/834: further characterised by the dopants
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/21: {of electrically active species}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

According to the present invention, since the buffer layer is formed by multiple ion implantations of different acceleration energies and the non-diffusion region in which impurity do not diffuse is left between the buffer layer and the collector layer, the semiconductor device which can supply sufficient holes to the drift layer at the turn-off can be manufactured while the withstand voltage is ensured.

## Claims

### Claim 1

A semiconductor device manufacturing method comprising:
a first step in which, on a first main surface and a second main surface which is a surface opposite to the first main surface of a semiconductor substrate, a first conductivity-type impurity is implanted in the second main surface by using multiple ion implantations of different acceleration energies so as to form a first impurity region on the semiconductor substrate;
a second step in which a second conductivity-type impurity is implanted in the second main surface using the acceleration energy lower than the multiple ion implantations, and a second impurity region is formed so that a non-implantation region in which the impurity is not implanted is left between that and the first impurity region in the semiconductor substrate;
a heat treatment step in which heat treatment is applied to the semiconductor substrate so that a buffer layer is formed by the first conductivity-type impurity, a collector layer is formed by the second conductivity-type impurity, and a non-diffusion region in which the first conductivity-type impurity and the second conductivity-type impurity do not diffuse are left between the buffer layer and the collector layer; and
a step in which a collector electrode in contact with the collector layer is formed.

### Claim 2 (depends on 1)

The semiconductor device manufacturing method according to claim 1, wherein
the first conductivity-type impurity is implanted in the second main surface at the acceleration energy of 1 to 10 MeV; and
the second conductivity-type impurity is implanted in the second main surface at the acceleration energy of 5 to 100 KeV.

### Claim 3 (depends on 1)

The semiconductor device manufacturing method according to claim 1, wherein dosages of the multiple ion implantations are uniform.

### Claim 4 (depends on 1)

The semiconductor device manufacturing method according to claim 1, wherein the multiple ion implantations are performed so that the dosage of the first conductivity-type impurity becomes larger as going closer to the second main surface side.

### Claim 5 (depends on 1)

The semiconductor device manufacturing method according to claim 1, wherein in the first step, the first conductivity-type impurity is implanted perpendicularly to the second main surface.

### Claim 6 (depends on 1)

The semiconductor device manufacturing method according to claim 1, wherein the first conductivity-type impurity is phosphorous.

### Claim 7 (depends on 4)