# US 2016/0254363 A1 · Gallium nitride power devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254363 A1
- Document ID: US20160254363A1
- Status: Published application
- Kind: A1
- Application number: 15/149,467
- Filed: 2016-05-09
- Published: 2016-09-01
- Earliest claimed: 2007-09-17
- Assignees: Transphorm Inc.
- Applicants: Transphorm Inc.
- Inventors: Chang Soo Suh; Umesh Mishra
- Web page: https://patentgrep.com/patent/US20160254363A1

## CPC

- H10D 30/015: {of FETs having heterojunction interface channels or heterojunction gate electrodes, e.g. HEMT}
- H10D 30/47: having two-dimensional [2D] charge carrier gas channels, e.g. nanoribbon FETs or high electron mobility transistors [HEMT]
- H10D 30/472: {having lower bandgap active layer formed on top of wider bandgap layer, e.g. inverted HEMT}
- H10D 30/4732: {using Group III-V semiconductor material}
- H10D 30/4755: {having wide bandgap charge-carrier supplying layers, e.g. modulation doped HEMTs such as n-AlGaAs/GaAs HEMTs}
- H10D 62/343: {Gate regions of field-effect devices having PN junction gates}
- H10D 62/357: {of FETs}
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10D 64/111: {Field plates}
- H10D 64/256: {for lateral devices wherein the source or drain electrodes are recessed in semiconductor bodies (source or drain electrodes of TFTs H10D30/673)}
- H10D 64/602: {Heterojunction gate electrodes for FETs}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Enhancement mode III-nitride devices are described. The 2DEG is depleted in the gate region so that the device is unable to conduct current when no bias is applied at the gate. Both gallium face and nitride face devices formed as enhancement mode devices.

## Claims

### Claim 1

A method of forming a III-nitride device, comprising:
forming a GaN material on a substrate;
forming a passivation layer over the GaN material, wherein the substrate, the GaN material, and the passivation layer are part of a structure having a first side adjacent the substrate and a second side opposite the substrate;
attaching a carrier wafer to the second side of the structure via a bonding layer provided therebetween; and
after attaching the carrier wafer to the second side of the structure, removing the substrate to expose a surface of the GaN material.

### Claim 2 (depends on 1)

The method of claim 1, wherein the GaN material comprises a GaN channel layer and an AlxGaN layer.

### Claim 3 (depends on 2)

The method of claim 2, wherein the AlxGaN layer has a thickness of less than 500 Angstroms.

### Claim 4 (depends on 2)

The method of claim 2, wherein the channel layer has a thickness of less than 300 Angstroms.

### Claim 5 (depends on 2)

The method of claim 2, wherein the GaN material further comprises a buffer layer between the substrate and the channel layer.

### Claim 6 (depends on 5)

The method of claim 5, wherein the buffer layer further comprises a sacrificial layer and an etch stop layer.

### Claim 7 (depends on 6)

The method of claim 6, wherein after removing the substrate, the sacrificial layer is selectively removed to expose a planar GaN surface.

### Claim 8 (depends on 1)

The method of claim 1, wherein the exposed planar GaN surface is an N-face of the GaN material.

### Claim 9 (depends on 1)

The method of claim 1, wherein III-nitride device is an enhancement mode transistor device.

### Claim 10 (depends on 1)

The method of claim 1, wherein the III-nitride device is configured to block at least 600V.

### Claim 11

A method of forming a III-nitride device, comprising:
providing, on a substrate, a structure comprising a GaN material and a passivation layer formed on the GaN material, the GaN material contacting the substrate;
attaching a carrier wafer to a side of the structure opposite the substrate, wherein a bonding layer attaches the carrier wafer to the structure; and
after attaching the carrier wafer to the structure, removing the substrate to expose a surface of the GaN material.

### Claim 12 (depends on 11)

The method of claim 11, wherein the GaN material comprises a GaN channel layer and an AlxGaN layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the AlxGaN layer has a thickness of less than 500 Angstroms.

### Claim 14 (depends on 12)

The method of claim 12, wherein the channel layer has a thickness of less than 300 Angstroms.

### Claim 15 (depends on 12)

The method of claim 12, wherein the GaN material further comprises a buffer layer between the substrate and the channel layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein the buffer layer further comprises a sacrificial layer and an etch stop layer.

### Claim 17 (depends on 16)

The method of claim 16, wherein after removing the substrate, the sacrificial layer is selectively removed to expose a planar GaN surface.

### Claim 18 (depends on 11)

The method of claim 11, wherein the exposed planar GaN surface is an N-face GaN material.

### Claim 19 (depends on 11)

The method of claim 11, wherein the III-nitride device is an enhancement mode transistor device.

### Claim 20 (depends on 10)

The method of claim 10, wherein the III-nitride device is configured to block at least 600V.