# US 2016/0254295 A1 · Semiconductor device and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254295 A1
- Document ID: US20160254295A1
- Status: Published application
- Kind: A1
- Application number: 15/151,541
- Filed: 2016-05-11
- Published: 2016-09-01
- Earliest claimed: 2012-12-03
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Applicants: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Shunpei YAMAZAKI
- Web page: https://patentgrep.com/patent/US20160254295A1

## CPC

- H10D 86/0229: {characterised by control of the annealing or irradiation parameters}
- G02F 1/133345: {Insulating layers (G02F1/1335, G02F1/1337, G02F1/135, G02F1/136 take precedence)}
- G02F 1/1341: Filling or closing of cells
- G02F 1/13439: {characterised by their electrical, optical, physical properties; materials therefor; method of making}
- G02F 1/136213: {Storage capacitors associated with the pixel electrode}
- G02F 1/136227: {Through-hole connection of the pixel electrode to the active element through an insulation layer}
- G02F 1/136286: {Wiring, e.g. gate line, drain line}
- G02F 1/1368: in which the switching element is a three-electrode device {(G02F1/136277 takes precedence)}
- H10D 30/6713: {characterised by the properties of the source or drain regions, e.g. compositions or sectional shapes}
- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- H10D 30/6757: {characterised by the structure of the channel, e.g. transverse or longitudinal shape or doping profile (TFTs having channel structures for preventing kink or snapback effects H10D30/6708; TFTs having lightly-doped source or drain extensions H10D30/6715)}
- H10D 62/80: characterised by the materials
- H10D 62/8271: {comprising only oxide semiconductor materials heterojunctions, e.g. IGZO/IZO}
- H10D 86/423: {comprising semiconductor materials not belonging to the Group IV, e.g. InGaZnO}
- H10D 86/60: wherein the TFTs are in active matrices
- H10D 99/00: Subject matter not provided for in other groups of this subclass
- H10D 62/875: {being semiconductor metal oxide, e.g. InGaZnO (Group II-VI materials H10D62/86; Group I-VI materials H10D62/871; Pb compounds or alloys H10D62/874)}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/662: {Laminate layers, e.g. stacks of alternating high-k metal oxides (adhesion layers or buffer layers H10P14/6508, H10P14/6548)}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

In a semiconductor device, a region where a channel is formed is protected. In a semiconductor device, a region protecting a region where a channel is formed is provided in a semiconductor layer. In a semiconductor device, a layer protecting a region where a channel is formed is provided. In a semiconductor device, a region and/or a layer protecting a region where a channel is formed have/has a low density of defect states. In a semiconductor device, a region where a channel is formed has a low density of defect states.

## Claims

### Claim 1

A method for manufacturing a semiconductor device comprising the steps of:
forming a gate electrode;
forming a gate insulating film over the gate electrode;
forming a first oxide semiconductor layer over the gate insulating film and forming a second oxide semiconductor layer over the first oxide semiconductor layer,
forming a conductive film over the second oxide semiconductor layer; and
partly etching the conductive film to expose a part of the second oxide semiconductor layer,
wherein the part of the second oxide semiconductor layer is etched so that a thickness of the part of the second oxide semiconductor layer is greater than or equal to 0 nm and less than 5 nm.

### Claim 2 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1,
wherein the second oxide semiconductor layer comprises a region having a larger energy gap than the energy gap of the first oxide semiconductor layer.

### Claim 3 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1,
wherein the second oxide semiconductor layer and the first oxide semiconductor layer comprise indium and an element M selected from aluminum, gallium, yttrium, zirconium, and tin, and
wherein the second oxide semiconductor layer comprises a region where a proportion of the element M is higher than a proportion of the element M in the first oxide semiconductor layer.

### Claim 4 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1,
wherein the second oxide semiconductor layer is formed by a sputtering method at a substrate temperature of higher than or equal to 100° C. and lower than 500° C.

### Claim 5 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1,
wherein a mixed region of the first oxide semiconductor layer and the second oxide semiconductor layer is formed between the first oxide semiconductor layer and the second oxide semiconductor layer.

### Claim 6

A method for manufacturing a semiconductor device comprising the steps of:
forming a conductive layer;
forming an insulating film over the conductive layer;
forming a first oxide semiconductor layer over the insulating film;
forming a second oxide semiconductor layer over the first oxide semiconductor layer;
forming a conductive film over the second oxide semiconductor layer; and
partly etching the conductive film to expose a part of the second oxide semiconductor layer,
wherein the part of the second oxide semiconductor layer is etched so that a thickness of the part of the second oxide semiconductor layer is greater than or equal to 0 nm and less than 5 nm.

### Claim 7 (depends on 6)

The method for manufacturing a semiconductor device according to claim 6,
wherein the second oxide semiconductor layer comprises a region having a larger energy gap than the energy gap of the first oxide semiconductor layer.

### Claim 8 (depends on 6)

The method for manufacturing a semiconductor device according to claim 6,
wherein the second oxide semiconductor layer and the first oxide semiconductor layer comprise indium and an element M selected from aluminum, gallium, yttrium, zirconium, and tin, and
wherein the second oxide semiconductor layer comprises a region where a proportion of the element M is higher than a proportion of the element M in the first oxide semiconductor layer.

### Claim 9 (depends on 6)

The method for manufacturing a semiconductor device according to claim 6,
wherein the second oxide semiconductor layer is formed by a sputtering method at a substrate temperature of higher than or equal to 100° C. and lower than 500° C.

### Claim 10 (depends on 6)

The method for manufacturing a semiconductor device according to claim 6,
wherein a mixed region of the first oxide semiconductor layer and the second oxide semiconductor layer is formed between the first oxide semiconductor layer and the second oxide semiconductor layer.